Glossary » Design » Oring » Chemical » Freon TF

Common O-Ring materials that are SUITABLE for dynamic and static seal in the environment containing Freon TF include

  • Buna-N (Nitrile): Buna-N, also known as Nitrile rubber, is a synthetic rubber copolymer of acrylonitrile (ACN) and butadiene.
  • Epichlorohydrin: Epichlorohydrin (ECO) has properties similar to nitrile rubber but with better heat and oil resistance as well as better low temperature flexibility.
  • Hypalon: Hypalon is the traenme of a clasof Chlorosulfonated Polyethylene (CSM).
  • Neoprene: Neoprene is a homopolymer of chlorobutadiene (CR).
  • Hydrogenated Nitrile: Hydrogenated Nitrile Butadiene Rubber (HNBR) is also known as Highly Saturated Nitrile (HSN).
  • Polysulfide: Polysulfide was one of the first commercial synthetic elastomers.
  • Virgin Teflon: Because Teflon is a hard plastic rather than a stretchy elastomer, it is uncommon to see an o-ring that is made entirely of Teflon.

The O-Ring materials below are USUALLY SUITABLE for static seal in the environment containing Freon TF.

  • Fluorocarbon: Fluorocarbon elastomer (FKM) material is also known by its tradename VITON or Fluorel.
  • Styrene Butadiene: Styrene-Butadiene rubber (SBR) has properties similar to those of natural rubber.

The following O-Ring materials are SOMETIMES OK for static seal but not for dynamic seal in the environment containing Freon TF.

  • Butyl: Butyl (IIR) is a synthetic rubber, a copolymer of isobutylene and isoprene.
  • Vamac: Vamac is the tradename of a class of Ethylene Acrylic elastomer (AEM).

O-Ring materials that are NOT SUITABLE for using in the environment containing Freon TF include

  • Aflas: Aflas is the tradename for a unique fluoroelastomer based upon an alternating copolymer of tetrafluoroethylene and propylene ("TFE/P").
  • Ethylene-Propylene: Ethylene-propylene (EP) is a copolymer of ethylene and propylene.
  • Fluorosilicone: Fluorosilicone combines excellent low-temperature performance of silicone with improved chemical resistance.
  • Kalrez: Kalrez is the tradename for a perfluoroelastomeric material.
  • Natural Rubber: Natural rubber is a product coagulated from the latex of the rubber tree, hevea brasiliensis.
  • Silicone: Silicone is a semi-organic elastomer with outstanding resistance to extremes of temperature.
Additional Information

There is not enough data to determine whether the following common O-Ring materials are suitable for using in the environment containing Freon TF or not.

  • Chemraz: Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE.
  • Polyacrylate: Polyacrylate (ACM) is a class of copolymer of ethyl and acrylates.
  • Cast Polyurethane: Cast Polyurethane exhibits outstanding tensile strength and abrasion resistance in comparison with other elastomers.
  • Millable Polyurethane: Millable Polyurethane rubber is made from both polyester and polyether polyols.
Related Pages
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.