Glossary » Design » Oring » Chemical » Propyl Acetate

Common O-Ring materials that are SUITABLE for dynamic and static seal in the environment containing Propyl Acetate include

  • Chemraz: Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE.

The O-Ring materials below are USUALLY SUITABLE for static seal in the environment containing Propyl Acetate.

  • Butyl: Butyl (IIR) is a synthetic rubber, a copolymer of isobutylene and isoprene.
  • Ethylene-Propylene: Ethylene-propylene (EP) is a copolymer of ethylene and propylene.
  • Polysulfide: Polysulfide was one of the first commercial synthetic elastomers.

O-Ring materials that are NOT SUITABLE for using in the environment containing Propyl Acetate include

  • Buna-N (Nitrile): Buna-N, also known as Nitrile rubber, is a synthetic rubber copolymer of acrylonitrile (ACN) and butadiene.
  • Epichlorohydrin: Epichlorohydrin (ECO) has properties similar to nitrile rubber but with better heat and oil resistance as well as better low temperature flexibility.
  • Fluorocarbon: Fluorocarbon elastomer (FKM) material is also known by its tradename VITON or Fluorel.
  • Fluorosilicone: Fluorosilicone combines excellent low-temperature performance of silicone with improved chemical resistance.
  • Hypalon: Hypalon is the traenme of a clasof Chlorosulfonated Polyethylene (CSM).
  • Natural Rubber: Natural rubber is a product coagulated from the latex of the rubber tree, hevea brasiliensis.
  • Neoprene: Neoprene is a homopolymer of chlorobutadiene (CR).
  • Hydrogenated Nitrile: Hydrogenated Nitrile Butadiene Rubber (HNBR) is also known as Highly Saturated Nitrile (HSN).
  • Polyacrylate: Polyacrylate (ACM) is a class of copolymer of ethyl and acrylates.
  • Millable Polyurethane: Millable Polyurethane rubber is made from both polyester and polyether polyols.
  • Silicone: Silicone is a semi-organic elastomer with outstanding resistance to extremes of temperature.
  • Styrene Butadiene: Styrene-Butadiene rubber (SBR) has properties similar to those of natural rubber.
  • Virgin Teflon: Because Teflon is a hard plastic rather than a stretchy elastomer, it is uncommon to see an o-ring that is made entirely of Teflon.
Additional Information

There is not enough data to determine whether the following common O-Ring materials are suitable for using in the environment containing Propyl Acetate or not.

  • Aflas: Aflas is the tradename for a unique fluoroelastomer based upon an alternating copolymer of tetrafluoroethylene and propylene ("TFE/P").
  • Kalrez: Kalrez is the tradename for a perfluoroelastomeric material.
  • Cast Polyurethane: Cast Polyurethane exhibits outstanding tensile strength and abrasion resistance in comparison with other elastomers.
  • Vamac: Vamac is the tradename of a class of Ethylene Acrylic elastomer (AEM).
Related Pages
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.