Glossary » Design » Oring » Chemical » Vinegar

Common O-Ring materials that are SUITABLE for dynamic and static seal in the environment containing Vinegar include

  • Butyl: Butyl (IIR) is a synthetic rubber, a copolymer of isobutylene and isoprene.
  • Ethylene-Propylene: Ethylene-propylene (EP) is a copolymer of ethylene and propylene.
  • Fluorocarbon: Fluorocarbon elastomer (FKM) material is also known by its tradename VITON or Fluorel.
  • Hypalon: Hypalon is the traenme of a clasof Chlorosulfonated Polyethylene (CSM).
  • Kalrez: Kalrez is the tradename for a perfluoroelastomeric material.
  • Silicone: Silicone is a semi-organic elastomer with outstanding resistance to extremes of temperature.
  • Virgin Teflon: Because Teflon is a hard plastic rather than a stretchy elastomer, it is uncommon to see an o-ring that is made entirely of Teflon.

The O-Ring materials below are USUALLY SUITABLE for static seal in the environment containing Vinegar.

  • Buna-N (Nitrile): Buna-N, also known as Nitrile rubber, is a synthetic rubber copolymer of acrylonitrile (ACN) and butadiene.
  • Natural Rubber: Natural rubber is a product coagulated from the latex of the rubber tree, hevea brasiliensis.
  • Neoprene: Neoprene is a homopolymer of chlorobutadiene (CR).
  • Polysulfide: Polysulfide was one of the first commercial synthetic elastomers.
  • Styrene Butadiene: Styrene-Butadiene rubber (SBR) has properties similar to those of natural rubber.
  • Vamac: Vamac is the tradename of a class of Ethylene Acrylic elastomer (AEM).

The following O-Ring materials are SOMETIMES OK for static seal but not for dynamic seal in the environment containing Vinegar.

  • Fluorosilicone: Fluorosilicone combines excellent low-temperature performance of silicone with improved chemical resistance.

O-Ring materials that are NOT SUITABLE for using in the environment containing Vinegar include

  • Polyacrylate: Polyacrylate (ACM) is a class of copolymer of ethyl and acrylates.
Additional Information

There is not enough data to determine whether the following common O-Ring materials are suitable for using in the environment containing Vinegar or not.

  • Aflas: Aflas is the tradename for a unique fluoroelastomer based upon an alternating copolymer of tetrafluoroethylene and propylene ("TFE/P").
  • Chemraz: Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE.
  • Epichlorohydrin: Epichlorohydrin (ECO) has properties similar to nitrile rubber but with better heat and oil resistance as well as better low temperature flexibility.
  • Hydrogenated Nitrile: Hydrogenated Nitrile Butadiene Rubber (HNBR) is also known as Highly Saturated Nitrile (HSN).
  • Cast Polyurethane: Cast Polyurethane exhibits outstanding tensile strength and abrasion resistance in comparison with other elastomers.
  • Millable Polyurethane: Millable Polyurethane rubber is made from both polyester and polyether polyols.
Related Pages
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.