Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Chemical Engineering

The industry gateway for chemical engineering and plant operations.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Four Equal Spans » Wide Flange Steel I Beam » W14 × 145
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in four equal spans, we compute the displacement at the middle of the first and fourth spans, and the maximum normal stress stress_max occuring at the second and fourth supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1710 in4) for the W14 × 145 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 2.45 × 10-6 7.25
200 3.39 × 10-6 10.0
300 5.08 × 10-6 15.0
400 6.77 × 10-6 20.0
500 8.47 × 10-6 25.0
600 1.02 × 10-5 30.0
700 1.19 × 10-5 35.0
800 1.35 × 10-5 40.0
900 1.52 × 10-5 45.0
1000 1.69 × 10-5 50.0
2000 3.39 × 10-5 100
3000 5.08 × 10-5 150
4000 6.77 × 10-5 200
5000 8.47 × 10-5 250
6000 1.02 × 10-4 300
7000 1.19 × 10-4 350
8000 1.35 × 10-4 400
9000 1.52 × 10-4 450
1.00 × 104 1.69 × 10-4 500
2.00 × 104 3.39 × 10-4 1000
3.00 × 104 5.08 × 10-4 1500
4.00 × 104 6.77 × 10-4 2000
5.00 × 104 8.47 × 10-4 2500
6.00 × 104 0.00102 3000
7.00 × 104 0.00119 3500
8.00 × 104 0.00135 4000
9.00 × 104 0.00152 4500
1.00 × 105 0.00169 5000
2.00 × 105 0.00339 10000
3.00 × 105 0.00508 1.50 × 104
4.00 × 105 0.00677 2.00 × 104
5.00 × 105 0.00847 2.50 × 104
6.00 × 105 0.0102 3.00 × 104
7.00 × 105 0.0119 3.50 × 104
8.00 × 105 0.0135 4.00 × 104
9.00 × 105 0.0152 4.50 × 104
1.00 × 106 0.0169 5.00 × 104
2.00 × 106 0.0339 1.00 × 105
3.00 × 106 0.0508 1.50 × 105
4.00 × 106 0.0677 2.00 × 105
5.00 × 106 0.0847 2.50 × 105
5.94 × 106 0.101 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 1.89 × 10-5 20.1
200 2.61 × 10-5 27.8
300 3.92 × 10-5 41.7
400 5.23 × 10-5 55.5
500 6.53 × 10-5 69.4
600 7.84 × 10-5 83.3
700 9.14 × 10-5 97.2
800 1.05 × 10-4 111
900 1.18 × 10-4 125
1000 1.31 × 10-4 139
2000 2.61 × 10-4 278
3000 3.92 × 10-4 417
4000 5.23 × 10-4 555
5000 6.53 × 10-4 694
6000 7.84 × 10-4 833
7000 9.14 × 10-4 972
8000 0.00105 1110
9000 0.00118 1250
1.00 × 104 0.00131 1390
2.00 × 104 0.00261 2780
3.00 × 104 0.00392 4170
4.00 × 104 0.00523 5550
5.00 × 104 0.00653 6940
6.00 × 104 0.00784 8330
7.00 × 104 0.00914 9720
8.00 × 104 0.0105 1.11 × 104
9.00 × 104 0.0118 1.25 × 104
1.00 × 105 0.0131 1.39 × 104
2.00 × 105 0.0261 2.78 × 104
3.00 × 105 0.0392 4.17 × 104
4.00 × 105 0.0523 5.55 × 104
5.00 × 105 0.0653 6.94 × 104
6.00 × 105 0.0784 8.33 × 104
7.00 × 105 0.0914 9.72 × 104
8.00 × 105 0.105 1.11 × 105
9.00 × 105 0.118 1.25 × 105
1.00 × 106 0.131 1.39 × 105
2.00 × 106 0.261 2.78 × 105
2.14 × 106 0.279 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 3.03 × 10-4 80.5
200 4.18 × 10-4 111
300 6.27 × 10-4 167
400 8.36 × 10-4 222
500 0.00105 278
600 0.00125 333
700 0.00146 389
800 0.00167 444
900 0.00188 500
1000 0.00209 555
2000 0.00418 1110
3000 0.00627 1670
4000 0.00836 2220
5000 0.0105 2780
6000 0.0125 3330
7000 0.0146 3890
8000 0.0167 4440
9000 0.0188 5000
1.00 × 104 0.0209 5550
2.00 × 104 0.0418 1.11 × 104
3.00 × 104 0.0627 1.67 × 104
4.00 × 104 0.0836 2.22 × 104
5.00 × 104 0.105 2.78 × 104
6.00 × 104 0.125 3.33 × 104
7.00 × 104 0.146 3.89 × 104
8.00 × 104 0.167 4.44 × 104
9.00 × 104 0.188 5.00 × 104
1.00 × 105 0.209 5.55 × 104
2.00 × 105 0.418 1.11 × 105
3.00 × 105 0.627 1.67 × 105
4.00 × 105 0.836 2.22 × 105
5.00 × 105 1.05 2.78 × 105
5.35 × 105 1.12 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.00153 181
200 0.00212 250
300 0.00317 375
400 0.00423 500
500 0.00529 625
600 0.00635 750
700 0.00741 875
800 0.00847 1000
900 0.00952 1120
1000 0.0106 1250
2000 0.0212 2500
3000 0.0317 3750
4000 0.0423 5000
5000 0.0529 6250
6000 0.0635 7500
7000 0.0741 8750
8000 0.0847 10000
9000 0.0952 1.12 × 104
1.00 × 104 0.106 1.25 × 104
2.00 × 104 0.212 2.50 × 104
3.00 × 104 0.317 3.75 × 104
4.00 × 104 0.423 5.00 × 104
5.00 × 104 0.529 6.25 × 104
6.00 × 104 0.635 7.50 × 104
7.00 × 104 0.741 8.75 × 104
8.00 × 104 0.847 1.00 × 105
9.00 × 104 0.952 1.12 × 105
1.00 × 105 1.06 1.25 × 105
2.00 × 105 2.12 2.50 × 105
2.38 × 105 2.52 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.00485 322
200 0.00669 444
300 0.0100 667
400 0.0134 889
500 0.0167 1110
600 0.0201 1330
700 0.0234 1560
800 0.0268 1780
900 0.0301 2000
1000 0.0334 2220
2000 0.0669 4440
3000 0.100 6670
4000 0.134 8890
5000 0.167 1.11 × 104
6000 0.201 1.33 × 104
7000 0.234 1.56 × 104
8000 0.268 1.78 × 104
9000 0.301 2.00 × 104
1.00 × 104 0.334 2.22 × 104
2.00 × 104 0.669 4.44 × 104
3.00 × 104 1.00 6.67 × 104
4.00 × 104 1.34 8.89 × 104
5.00 × 104 1.67 1.11 × 105
6.00 × 104 2.01 1.33 × 105
7.00 × 104 2.34 1.56 × 105
8.00 × 104 2.68 1.78 × 105
9.00 × 104 3.01 2.00 × 105
1.00 × 105 3.34 2.22 × 105
1.34 × 105 4.47 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.0118 503
200 0.0163 694
300 0.0245 1040
400 0.0327 1390
500 0.0408 1740
600 0.0490 2080
700 0.0572 2430
800 0.0653 2780
900 0.0735 3120
1000 0.0816 3470
2000 0.163 6940
3000 0.245 1.04 × 104
4000 0.327 1.39 × 104
5000 0.408 1.74 × 104
6000 0.490 2.08 × 104
7000 0.572 2.43 × 104
8000 0.653 2.78 × 104
9000 0.735 3.12 × 104
1.00 × 104 0.816 3.47 × 104
2.00 × 104 1.63 6.94 × 104
3.00 × 104 2.45 1.04 × 105
4.00 × 104 3.27 1.39 × 105
5.00 × 104 4.08 1.74 × 105
6.00 × 104 4.90 2.08 × 105
7.00 × 104 5.72 2.43 × 105
8.00 × 104 6.53 2.78 × 105
8.56 × 104 6.99 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.0245 725
200 0.0339 1000
300 0.0508 1500
400 0.0677 2000
500 0.0847 2500
600 0.102 3000
700 0.119 3500
800 0.135 4000
900 0.152 4500
1000 0.169 5000
2000 0.339 10000
3000 0.508 1.50 × 104
4000 0.677 2.00 × 104
5000 0.847 2.50 × 104
6000 1.02 3.00 × 104
7000 1.19 3.50 × 104
8000 1.35 4.00 × 104
9000 1.52 4.50 × 104
1.00 × 104 1.69 5.00 × 104
2.00 × 104 3.39 1.00 × 105
3.00 × 104 5.08 1.50 × 105
4.00 × 104 6.77 2.00 × 105
5.00 × 104 8.47 2.50 × 105
5.94 × 104 10.1 2.97 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.0776 1290
200 0.107 1780
300 0.161 2670
400 0.214 3550
500 0.268 4440
600 0.321 5330
700 0.375 6220
800 0.428 7110
900 0.482 8000
1000 0.535 8890
2000 1.07 1.78 × 104
3000 1.61 2.67 × 104
4000 2.14 3.55 × 104
5000 2.68 4.44 × 104
6000 3.21 5.33 × 104
7000 3.75 6.22 × 104
8000 4.28 7.11 × 104
9000 4.82 8.00 × 104
1.00 × 104 5.35 8.89 × 104
2.00 × 104 10.7 1.78 × 105
2.76 × 104 14.8 2.45 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.189 2010
200 0.261 2780
300 0.392 4170
400 0.523 5550
500 0.653 6940
600 0.784 8330
700 0.914 9720
800 1.05 1.11 × 104
900 1.18 1.25 × 104
1000 1.31 1.39 × 104
2000 2.61 2.78 × 104
3000 3.92 4.17 × 104
4000 5.23 5.55 × 104
5000 6.53 6.94 × 104
6000 7.84 8.33 × 104
7000 9.14 9.72 × 104
8000 10.5 1.11 × 105
9000 11.8 1.25 × 105
1.00 × 104 13.1 1.39 × 105
1.13 × 104 14.8 1.57 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.393 2900
200 0.542 4000
300 0.813 6000
400 1.08 8000
500 1.35 10000
600 1.63 1.20 × 104
700 1.90 1.40 × 104
800 2.17 1.60 × 104
900 2.44 1.80 × 104
1000 2.71 2.00 × 104
2000 5.42 4.00 × 104
3000 8.13 6.00 × 104
4000 10.8 8.00 × 104
5000 13.5 1.00 × 105
5460 14.8 1.09 × 105
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 0.728 3950
200 1.00 5440
300 1.51 8160
400 2.01 1.09 × 104
500 2.51 1.36 × 104
600 3.01 1.63 × 104
700 3.51 1.91 × 104
800 4.01 2.18 × 104
900 4.52 2.45 × 104
1000 5.02 2.72 × 104
2000 10.0 5.44 × 104
2950 14.8 8.02 × 104
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 1.24 5150
200 1.71 7110
300 2.57 1.07 × 104
400 3.42 1.42 × 104
500 4.28 1.78 × 104
600 5.14 2.13 × 104
700 5.99 2.49 × 104
800 6.85 2.84 × 104
900 7.71 3.20 × 104
1000 8.56 3.55 × 104
1730 14.8 6.14 × 104
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 1.99 6520
200 2.74 9000
300 4.11 1.35 × 104
400 5.49 1.80 × 104
500 6.86 2.25 × 104
600 8.23 2.70 × 104
700 9.60 3.15 × 104
800 11.0 3.60 × 104
900 12.3 4.05 × 104
1000 13.7 4.50 × 104
1080 14.8 4.85 × 104
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 3.03 8050
200 4.18 1.11 × 104
300 6.27 1.67 × 104
400 8.36 2.22 × 104
500 10.5 2.78 × 104
600 12.5 3.33 × 104
700 14.6 3.89 × 104
707 14.8 3.93 × 104
Steel I Beam: W14 × 145 (Wide Flange 14 inch tall × 145 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
145 7.40 1.26 × 104
200 10.2 1.74 × 104
290 14.8 2.51 × 104
Additional Information