STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Four Equal Spans » Wide Flange Steel I Beam » W14 × 605
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in four equal spans, we compute the displacement at the middle of the first and fourth spans, and the maximum normal stress stress_max occuring at the second and fourth supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 10800 in4) for the W14 × 605 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 1.62 × 10-6 6.78
700 1.88 × 10-6 7.84
800 2.14 × 10-6 8.96
900 2.41 × 10-6 10.1
1000 2.68 × 10-6 11.2
2000 5.36 × 10-6 22.4
3000 8.04 × 10-6 33.6
4000 1.07 × 10-5 44.8
5000 1.34 × 10-5 56.0
6000 1.61 × 10-5 67.2
7000 1.88 × 10-5 78.4
8000 2.14 × 10-5 89.6
9000 2.41 × 10-5 101
1.00 × 104 2.68 × 10-5 112
2.00 × 104 5.36 × 10-5 224
3.00 × 104 8.04 × 10-5 336
4.00 × 104 1.07 × 10-4 448
5.00 × 104 1.34 × 10-4 560
6.00 × 104 1.61 × 10-4 672
7.00 × 104 1.88 × 10-4 784
8.00 × 104 2.14 × 10-4 896
9.00 × 104 2.41 × 10-4 1010
1.00 × 105 2.68 × 10-4 1120
2.00 × 105 5.36 × 10-4 2240
3.00 × 105 8.04 × 10-4 3360
4.00 × 105 0.00107 4480
5.00 × 105 0.00134 5600
6.00 × 105 0.00161 6720
7.00 × 105 0.00188 7840
8.00 × 105 0.00214 8960
9.00 × 105 0.00241 1.01 × 104
1.00 × 106 0.00268 1.12 × 104
2.00 × 106 0.00536 2.24 × 104
3.00 × 106 0.00804 3.36 × 104
4.00 × 106 0.0107 4.48 × 104
5.00 × 106 0.0134 5.60 × 104
6.00 × 106 0.0161 6.72 × 104
7.00 × 106 0.0188 7.84 × 104
8.00 × 106 0.0214 8.96 × 104
9.00 × 106 0.0241 1.01 × 105
1.00 × 107 0.0268 1.12 × 105
2.00 × 107 0.0536 2.24 × 105
2.65 × 107 0.0711 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 1.25 × 10-5 18.8
700 1.45 × 10-5 21.8
800 1.65 × 10-5 24.9
900 1.86 × 10-5 28.0
1000 2.07 × 10-5 31.1
2000 4.14 × 10-5 62.2
3000 6.21 × 10-5 93.4
4000 8.27 × 10-5 124
5000 1.03 × 10-4 156
6000 1.24 × 10-4 187
7000 1.45 × 10-4 218
8000 1.65 × 10-4 249
9000 1.86 × 10-4 280
1.00 × 104 2.07 × 10-4 311
2.00 × 104 4.14 × 10-4 622
3.00 × 104 6.21 × 10-4 934
4.00 × 104 8.27 × 10-4 1240
5.00 × 104 0.00103 1560
6.00 × 104 0.00124 1870
7.00 × 104 0.00145 2180
8.00 × 104 0.00165 2490
9.00 × 104 0.00186 2800
1.00 × 105 0.00207 3110
2.00 × 105 0.00414 6220
3.00 × 105 0.00621 9340
4.00 × 105 0.00827 1.24 × 104
5.00 × 105 0.0103 1.56 × 104
6.00 × 105 0.0124 1.87 × 104
7.00 × 105 0.0145 2.18 × 104
8.00 × 105 0.0165 2.49 × 104
9.00 × 105 0.0186 2.80 × 104
1.00 × 106 0.0207 3.11 × 104
2.00 × 106 0.0414 6.22 × 104
3.00 × 106 0.0621 9.34 × 104
4.00 × 106 0.0827 1.24 × 105
5.00 × 106 0.103 1.56 × 105
6.00 × 106 0.124 1.87 × 105
7.00 × 106 0.145 2.18 × 105
8.00 × 106 0.165 2.49 × 105
9.00 × 106 0.186 2.80 × 105
9.55 × 106 0.197 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 2.00 × 10-4 75.3
700 2.32 × 10-4 87.1
800 2.65 × 10-4 99.6
900 2.98 × 10-4 112
1000 3.31 × 10-4 124
2000 6.62 × 10-4 249
3000 9.93 × 10-4 373
4000 0.00132 498
5000 0.00165 622
6000 0.00199 747
7000 0.00232 871
8000 0.00265 996
9000 0.00298 1120
1.00 × 104 0.00331 1240
2.00 × 104 0.00662 2490
3.00 × 104 0.00993 3730
4.00 × 104 0.0132 4980
5.00 × 104 0.0165 6220
6.00 × 104 0.0199 7470
7.00 × 104 0.0232 8710
8.00 × 104 0.0265 9960
9.00 × 104 0.0298 1.12 × 104
1.00 × 105 0.0331 1.24 × 104
2.00 × 105 0.0662 2.49 × 104
3.00 × 105 0.0993 3.73 × 104
4.00 × 105 0.132 4.98 × 104
5.00 × 105 0.165 6.22 × 104
6.00 × 105 0.199 7.47 × 104
7.00 × 105 0.232 8.71 × 104
8.00 × 105 0.265 9.96 × 104
9.00 × 105 0.298 1.12 × 105
1.00 × 106 0.331 1.24 × 105
2.00 × 106 0.662 2.49 × 105
2.39 × 106 0.790 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.00101 169
700 0.00117 196
800 0.00134 224
900 0.00151 252
1000 0.00168 280
2000 0.00335 560
3000 0.00503 840
4000 0.00670 1120
5000 0.00838 1400
6000 0.0101 1680
7000 0.0117 1960
8000 0.0134 2240
9000 0.0151 2520
1.00 × 104 0.0168 2800
2.00 × 104 0.0335 5600
3.00 × 104 0.0503 8400
4.00 × 104 0.0670 1.12 × 104
5.00 × 104 0.0838 1.40 × 104
6.00 × 104 0.101 1.68 × 104
7.00 × 104 0.117 1.96 × 104
8.00 × 104 0.134 2.24 × 104
9.00 × 104 0.151 2.52 × 104
1.00 × 105 0.168 2.80 × 104
2.00 × 105 0.335 5.60 × 104
3.00 × 105 0.503 8.40 × 104
4.00 × 105 0.670 1.12 × 105
5.00 × 105 0.838 1.40 × 105
6.00 × 105 1.01 1.68 × 105
7.00 × 105 1.17 1.96 × 105
8.00 × 105 1.34 2.24 × 105
9.00 × 105 1.51 2.52 × 105
1.00 × 106 1.68 2.80 × 105
1.06 × 106 1.78 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.00320 301
700 0.00371 349
800 0.00424 398
900 0.00477 448
1000 0.00530 498
2000 0.0106 996
3000 0.0159 1490
4000 0.0212 1990
5000 0.0265 2490
6000 0.0318 2990
7000 0.0371 3490
8000 0.0424 3980
9000 0.0477 4480
1.00 × 104 0.0530 4980
2.00 × 104 0.106 9960
3.00 × 104 0.159 1.49 × 104
4.00 × 104 0.212 1.99 × 104
5.00 × 104 0.265 2.49 × 104
6.00 × 104 0.318 2.99 × 104
7.00 × 104 0.371 3.49 × 104
8.00 × 104 0.424 3.98 × 104
9.00 × 104 0.477 4.48 × 104
1.00 × 105 0.530 4.98 × 104
2.00 × 105 1.06 9.96 × 104
3.00 × 105 1.59 1.49 × 105
4.00 × 105 2.12 1.99 × 105
5.00 × 105 2.65 2.49 × 105
5.97 × 105 3.16 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.00782 471
700 0.00905 545
800 0.0103 622
900 0.0116 700
1000 0.0129 778
2000 0.0259 1560
3000 0.0388 2330
4000 0.0517 3110
5000 0.0646 3890
6000 0.0776 4670
7000 0.0905 5450
8000 0.103 6220
9000 0.116 7000
1.00 × 104 0.129 7780
2.00 × 104 0.259 1.56 × 104
3.00 × 104 0.388 2.33 × 104
4.00 × 104 0.517 3.11 × 104
5.00 × 104 0.646 3.89 × 104
6.00 × 104 0.776 4.67 × 104
7.00 × 104 0.905 5.45 × 104
8.00 × 104 1.03 6.22 × 104
9.00 × 104 1.16 7.00 × 104
1.00 × 105 1.29 7.78 × 104
2.00 × 105 2.59 1.56 × 105
3.00 × 105 3.88 2.33 × 105
3.82 × 105 4.94 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.0162 678
700 0.0188 784
800 0.0214 896
900 0.0241 1010
1000 0.0268 1120
2000 0.0536 2240
3000 0.0804 3360
4000 0.107 4480
5000 0.134 5600
6000 0.161 6720
7000 0.188 7840
8000 0.214 8960
9000 0.241 1.01 × 104
1.00 × 104 0.268 1.12 × 104
2.00 × 104 0.536 2.24 × 104
3.00 × 104 0.804 3.36 × 104
4.00 × 104 1.07 4.48 × 104
5.00 × 104 1.34 5.60 × 104
6.00 × 104 1.61 6.72 × 104
7.00 × 104 1.88 7.84 × 104
8.00 × 104 2.14 8.96 × 104
9.00 × 104 2.41 1.01 × 105
1.00 × 105 2.68 1.12 × 105
2.00 × 105 5.36 2.24 × 105
2.65 × 105 7.11 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.0513 1200
700 0.0593 1390
800 0.0678 1590
900 0.0763 1790
1000 0.0847 1990
2000 0.169 3980
3000 0.254 5970
4000 0.339 7970
5000 0.424 9960
6000 0.508 1.19 × 104
7000 0.593 1.39 × 104
8000 0.678 1.59 × 104
9000 0.763 1.79 × 104
1.00 × 104 0.847 1.99 × 104
2.00 × 104 1.69 3.98 × 104
3.00 × 104 2.54 5.97 × 104
4.00 × 104 3.39 7.97 × 104
5.00 × 104 4.24 9.96 × 104
6.00 × 104 5.08 1.19 × 105
7.00 × 104 5.93 1.39 × 105
8.00 × 104 6.78 1.59 × 105
9.00 × 104 7.63 1.79 × 105
1.00 × 105 8.47 1.99 × 105
1.49 × 105 12.6 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.125 1880
700 0.145 2180
800 0.165 2490
900 0.186 2800
1000 0.207 3110
2000 0.414 6220
3000 0.621 9340
4000 0.827 1.24 × 104
5000 1.03 1.56 × 104
6000 1.24 1.87 × 104
7000 1.45 2.18 × 104
8000 1.65 2.49 × 104
9000 1.86 2.80 × 104
1.00 × 104 2.07 3.11 × 104
2.00 × 104 4.14 6.22 × 104
3.00 × 104 6.21 9.34 × 104
4.00 × 104 8.27 1.24 × 105
5.00 × 104 10.3 1.56 × 105
6.00 × 104 12.4 1.87 × 105
7.00 × 104 14.5 2.18 × 105
8.00 × 104 16.5 2.49 × 105
9.00 × 104 18.6 2.80 × 105
9.55 × 104 19.7 2.97 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.259 2710
700 0.300 3140
800 0.343 3580
900 0.386 4030
1000 0.429 4480
2000 0.858 8960
3000 1.29 1.34 × 104
4000 1.72 1.79 × 104
5000 2.14 2.24 × 104
6000 2.57 2.69 × 104
7000 3.00 3.14 × 104
8000 3.43 3.58 × 104
9000 3.86 4.03 × 104
1.00 × 104 4.29 4.48 × 104
2.00 × 104 8.58 8.96 × 104
3.00 × 104 12.9 1.34 × 105
4.00 × 104 17.2 1.79 × 105
4.88 × 104 20.9 2.19 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.481 3690
700 0.556 4270
800 0.636 4880
900 0.715 5490
1000 0.795 6100
2000 1.59 1.22 × 104
3000 2.38 1.83 × 104
4000 3.18 2.44 × 104
5000 3.97 3.05 × 104
6000 4.77 3.66 × 104
7000 5.56 4.27 × 104
8000 6.36 4.88 × 104
9000 7.15 5.49 × 104
1.00 × 104 7.95 6.10 × 104
2.00 × 104 15.9 1.22 × 105
2.63 × 104 20.9 1.61 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 0.820 4820
700 0.949 5580
800 1.08 6370
900 1.22 7170
1000 1.36 7970
2000 2.71 1.59 × 104
3000 4.07 2.39 × 104
4000 5.42 3.19 × 104
5000 6.78 3.98 × 104
6000 8.13 4.78 × 104
7000 9.49 5.58 × 104
8000 10.8 6.37 × 104
9000 12.2 7.17 × 104
1.00 × 104 13.6 7.97 × 104
1.54 × 104 20.9 1.23 × 105
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 1.31 6100
700 1.52 7060
800 1.74 8070
900 1.95 9070
1000 2.17 1.01 × 104
2000 4.34 2.02 × 104
3000 6.51 3.02 × 104
4000 8.69 4.03 × 104
5000 10.9 5.04 × 104
6000 13.0 6.05 × 104
7000 15.2 7.06 × 104
8000 17.4 8.07 × 104
9000 19.5 9.07 × 104
9630 20.9 9.71 × 104
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 2.00 7530
700 2.32 8710
800 2.65 9960
900 2.98 1.12 × 104
1000 3.31 1.24 × 104
2000 6.62 2.49 × 104
3000 9.93 3.73 × 104
4000 13.2 4.98 × 104
5000 16.5 6.22 × 104
6000 19.9 7.47 × 104
6320 20.9 7.87 × 104
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 4.89 1.18 × 104
700 5.66 1.36 × 104
800 6.46 1.56 × 104
900 7.27 1.75 × 104
1000 8.08 1.94 × 104
2000 16.2 3.89 × 104
2590 20.9 5.04 × 104
Steel I Beam: W14 × 605 (Wide Flange 14 inch tall × 605 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
605 10.1 1.69 × 104
700 11.7 1.96 × 104
800 13.4 2.24 × 104
900 15.1 2.52 × 104
1000 16.8 2.80 × 104
1250 20.9 3.50 × 104
Additional Information
Related Pages
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!