Glossary » Beams » Simply Supported » Uniformly Distributed Load » Four Equal Spans » Wide Flange Steel I Beam » W14 × 68
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in four equal spans, we compute the displacement at the middle of the first and fourth spans, and the maximum normal stress stress_max occuring at the second and fourth supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 723 in4) for the W14 × 68 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 2.72 × 10-6 7.64
70.0 2.80 × 10-6 7.86
80.0 3.20 × 10-6 8.98
90.0 3.60 × 10-6 10.1
100 4.00 × 10-6 11.2
200 8.01 × 10-6 22.5
300 1.20 × 10-5 33.7
400 1.60 × 10-5 44.9
500 2.00 × 10-5 56.2
600 2.40 × 10-5 67.4
700 2.80 × 10-5 78.6
800 3.20 × 10-5 89.8
900 3.60 × 10-5 101
1000 4.00 × 10-5 112
2000 8.01 × 10-5 225
3000 1.20 × 10-4 337
4000 1.60 × 10-4 449
5000 2.00 × 10-4 562
6000 2.40 × 10-4 674
7000 2.80 × 10-4 786
8000 3.20 × 10-4 898
9000 3.60 × 10-4 1010
1.00 × 104 4.00 × 10-4 1120
2.00 × 104 8.01 × 10-4 2250
3.00 × 104 0.00120 3370
4.00 × 104 0.00160 4490
5.00 × 104 0.00200 5620
6.00 × 104 0.00240 6740
7.00 × 104 0.00280 7860
8.00 × 104 0.00320 8980
9.00 × 104 0.00360 1.01 × 104
1.00 × 105 0.00400 1.12 × 104
2.00 × 105 0.00801 2.25 × 104
3.00 × 105 0.0120 3.37 × 104
4.00 × 105 0.0160 4.49 × 104
5.00 × 105 0.0200 5.62 × 104
6.00 × 105 0.0240 6.74 × 104
7.00 × 105 0.0280 7.86 × 104
8.00 × 105 0.0320 8.98 × 104
9.00 × 105 0.0360 1.01 × 105
1.00 × 106 0.0400 1.12 × 105
2.00 × 106 0.0801 2.25 × 105
2.64 × 106 0.106 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 2.10 × 10-5 21.2
70.0 2.16 × 10-5 21.8
80.0 2.47 × 10-5 25.0
90.0 2.78 × 10-5 28.1
100 3.09 × 10-5 31.2
200 6.18 × 10-5 62.4
300 9.27 × 10-5 93.6
400 1.24 × 10-4 125
500 1.54 × 10-4 156
600 1.85 × 10-4 187
700 2.16 × 10-4 218
800 2.47 × 10-4 250
900 2.78 × 10-4 281
1000 3.09 × 10-4 312
2000 6.18 × 10-4 624
3000 9.27 × 10-4 936
4000 0.00124 1250
5000 0.00154 1560
6000 0.00185 1870
7000 0.00216 2180
8000 0.00247 2500
9000 0.00278 2810
1.00 × 104 0.00309 3120
2.00 × 104 0.00618 6240
3.00 × 104 0.00927 9360
4.00 × 104 0.0124 1.25 × 104
5.00 × 104 0.0154 1.56 × 104
6.00 × 104 0.0185 1.87 × 104
7.00 × 104 0.0216 2.18 × 104
8.00 × 104 0.0247 2.50 × 104
9.00 × 104 0.0278 2.81 × 104
1.00 × 105 0.0309 3.12 × 104
2.00 × 105 0.0618 6.24 × 104
3.00 × 105 0.0927 9.36 × 104
4.00 × 105 0.124 1.25 × 105
5.00 × 105 0.154 1.56 × 105
6.00 × 105 0.185 1.87 × 105
7.00 × 105 0.216 2.18 × 105
8.00 × 105 0.247 2.50 × 105
9.00 × 105 0.278 2.81 × 105
9.52 × 105 0.294 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 3.36 × 10-4 84.9
70.0 3.46 × 10-4 87.4
80.0 3.95 × 10-4 99.8
90.0 4.45 × 10-4 112
100 4.94 × 10-4 125
200 9.89 × 10-4 250
300 0.00148 374
400 0.00198 499
500 0.00247 624
600 0.00297 749
700 0.00346 874
800 0.00395 998
900 0.00445 1120
1000 0.00494 1250
2000 0.00989 2500
3000 0.0148 3740
4000 0.0198 4990
5000 0.0247 6240
6000 0.0297 7490
7000 0.0346 8740
8000 0.0395 9980
9000 0.0445 1.12 × 104
1.00 × 104 0.0494 1.25 × 104
2.00 × 104 0.0989 2.50 × 104
3.00 × 104 0.148 3.74 × 104
4.00 × 104 0.198 4.99 × 104
5.00 × 104 0.247 6.24 × 104
6.00 × 104 0.297 7.49 × 104
7.00 × 104 0.346 8.74 × 104
8.00 × 104 0.395 9.98 × 104
9.00 × 104 0.445 1.12 × 105
1.00 × 105 0.494 1.25 × 105
2.00 × 105 0.989 2.50 × 105
2.38 × 105 1.18 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.00170 191
70.0 0.00175 197
80.0 0.00200 225
90.0 0.00225 253
100 0.00250 281
200 0.00501 562
300 0.00751 842
400 0.0100 1120
500 0.0125 1400
600 0.0150 1680
700 0.0175 1970
800 0.0200 2250
900 0.0225 2530
1000 0.0250 2810
2000 0.0501 5620
3000 0.0751 8420
4000 0.100 1.12 × 104
5000 0.125 1.40 × 104
6000 0.150 1.68 × 104
7000 0.175 1.97 × 104
8000 0.200 2.25 × 104
9000 0.225 2.53 × 104
1.00 × 104 0.250 2.81 × 104
2.00 × 104 0.501 5.62 × 104
3.00 × 104 0.751 8.42 × 104
4.00 × 104 1.00 1.12 × 105
5.00 × 104 1.25 1.40 × 105
6.00 × 104 1.50 1.68 × 105
7.00 × 104 1.75 1.97 × 105
8.00 × 104 2.00 2.25 × 105
9.00 × 104 2.25 2.53 × 105
1.00 × 105 2.50 2.81 × 105
1.06 × 105 2.65 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.00538 339
70.0 0.00554 349
80.0 0.00633 399
90.0 0.00712 449
100 0.00791 499
200 0.0158 998
300 0.0237 1500
400 0.0316 2000
500 0.0395 2500
600 0.0475 2990
700 0.0554 3490
800 0.0633 3990
900 0.0712 4490
1000 0.0791 4990
2000 0.158 9980
3000 0.237 1.50 × 104
4000 0.316 2.00 × 104
5000 0.395 2.50 × 104
6000 0.475 2.99 × 104
7000 0.554 3.49 × 104
8000 0.633 3.99 × 104
9000 0.712 4.49 × 104
1.00 × 104 0.791 4.99 × 104
2.00 × 104 1.58 9.98 × 104
3.00 × 104 2.37 1.50 × 105
4.00 × 104 3.16 2.00 × 105
5.00 × 104 3.95 2.50 × 105
5.95 × 104 4.71 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.0131 530
70.0 0.0135 546
80.0 0.0154 624
90.0 0.0174 702
100 0.0193 780
200 0.0386 1560
300 0.0579 2340
400 0.0772 3120
500 0.0966 3900
600 0.116 4680
700 0.135 5460
800 0.154 6240
900 0.174 7020
1000 0.193 7800
2000 0.386 1.56 × 104
3000 0.579 2.34 × 104
4000 0.772 3.12 × 104
5000 0.966 3.90 × 104
6000 1.16 4.68 × 104
7000 1.35 5.46 × 104
8000 1.54 6.24 × 104
9000 1.74 7.02 × 104
1.00 × 104 1.93 7.80 × 104
2.00 × 104 3.86 1.56 × 105
3.00 × 104 5.79 2.34 × 105
3.81 × 104 7.35 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.0272 764
70.0 0.0280 786
80.0 0.0320 898
90.0 0.0360 1010
100 0.0400 1120
200 0.0801 2250
300 0.120 3370
400 0.160 4490
500 0.200 5620
600 0.240 6740
700 0.280 7860
800 0.320 8980
900 0.360 1.01 × 104
1000 0.400 1.12 × 104
2000 0.801 2.25 × 104
3000 1.20 3.37 × 104
4000 1.60 4.49 × 104
5000 2.00 5.62 × 104
6000 2.40 6.74 × 104
7000 2.80 7.86 × 104
8000 3.20 8.98 × 104
9000 3.60 1.01 × 105
1.00 × 104 4.00 1.12 × 105
2.00 × 104 8.01 2.25 × 105
2.64 × 104 10.6 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.0861 1360
70.0 0.0886 1400
80.0 0.101 1600
90.0 0.114 1800
100 0.127 2000
200 0.253 3990
300 0.380 5990
400 0.506 7990
500 0.633 9980
600 0.759 1.20 × 104
700 0.886 1.40 × 104
800 1.01 1.60 × 104
900 1.14 1.80 × 104
1000 1.27 2.00 × 104
2000 2.53 3.99 × 104
3000 3.80 5.99 × 104
4000 5.06 7.99 × 104
5000 6.33 9.98 × 104
6000 7.59 1.20 × 105
7000 8.86 1.40 × 105
8000 10.1 1.60 × 105
9000 11.4 1.80 × 105
1.00 × 104 12.7 2.00 × 105
1.49 × 104 18.8 2.97 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.210 2120
70.0 0.216 2180
80.0 0.247 2500
90.0 0.278 2810
100 0.309 3120
200 0.618 6240
300 0.927 9360
400 1.24 1.25 × 104
500 1.54 1.56 × 104
600 1.85 1.87 × 104
700 2.16 2.18 × 104
800 2.47 2.50 × 104
900 2.78 2.81 × 104
1000 3.09 3.12 × 104
2000 6.18 6.24 × 104
3000 9.27 9.36 × 104
4000 12.4 1.25 × 105
4540 14.0 1.42 × 105
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.436 3050
70.0 0.448 3140
80.0 0.513 3590
90.0 0.577 4040
100 0.641 4490
200 1.28 8980
300 1.92 1.35 × 104
400 2.56 1.80 × 104
500 3.20 2.25 × 104
600 3.84 2.70 × 104
700 4.48 3.14 × 104
800 5.13 3.59 × 104
900 5.77 4.04 × 104
1000 6.41 4.49 × 104
2000 12.8 8.98 × 104
2190 14.0 9.84 × 104
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 0.807 4160
70.0 0.831 4280
80.0 0.950 4890
90.0 1.07 5500
100 1.19 6110
200 2.37 1.22 × 104
300 3.56 1.83 × 104
400 4.75 2.45 × 104
500 5.93 3.06 × 104
600 7.12 3.67 × 104
700 8.31 4.28 × 104
800 9.50 4.89 × 104
900 10.7 5.50 × 104
1000 11.9 6.11 × 104
1180 14.0 7.23 × 104
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 1.38 5430
70.0 1.42 5590
80.0 1.62 6390
90.0 1.82 7190
100 2.02 7990
200 4.05 1.60 × 104
300 6.07 2.40 × 104
400 8.10 3.19 × 104
500 10.1 3.99 × 104
600 12.1 4.79 × 104
693 14.0 5.54 × 104
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 2.21 6870
70.0 2.27 7080
80.0 2.59 8090
90.0 2.92 9100
100 3.24 1.01 × 104
200 6.49 2.02 × 104
300 9.73 3.03 × 104
400 13.0 4.04 × 104
433 14.0 4.38 × 104
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 3.36 8490
70.0 3.46 8740
80.0 3.95 9980
90.0 4.45 1.12 × 104
100 4.94 1.25 × 104
200 9.89 2.50 × 104
284 14.0 3.54 × 104
Steel I Beam: W14 × 68 (Wide Flange 14 inch tall × 68 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
68.0 8.21 1.33 × 104
70.0 8.45 1.36 × 104
80.0 9.66 1.56 × 104
90.0 10.9 1.75 × 104
100 12.1 1.95 × 104
116 14.0 2.27 × 104
Additional Information
Related Pages
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!