For a simply supported beam in a single span, the maximum displacement
and the maximum normal stress
occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 255.57 in4) for the 12.00 × 11.672 Aluminum I Beam and the typical Young's modulus (E = 1.015 × 107 psi) of aluminum alloys. Note that the typical yielding stress
of aluminum alloys can range from 4061 to 7.614 × 104 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
and the maximum normal stress
occur at the center of the beam.
of aluminum alloys can range from 4061 to 7.614 × 104 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
|
|
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Additional Information
Related Glossary Pages
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W10 × 54
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Two Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span: Wide Flange Steel I Beam: W14 × 500
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Two Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans: Wide Flange Steel I Beam: W12 × 79
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W18 × 65
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Two Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span: Wide Flange Steel I Beam: W14 × 500
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Two Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans: Wide Flange Steel I Beam: W12 × 79
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W18 × 65
Related Pages
Steel S Section I-Beams
Database of standard S Section I-beams with geometric properties.
Centroid, Area, Moments of Inertia, Polar Moments of Inertia ...
Aluminum Channels. Common Beams. Square I-Beam · Tapered I-Beam · Uneven I-Beam · General Shape · Square Channel · Tapered Channel · Square L Beam ...
eFunda: Glossary: Materials: Alloys: Aluminum Alloy: 413.0
It is composed of (in weight percentage) 86.00% Aluminum (Al), 12.00% Silicon (Si), and 2.0% Iron (Fe). It is usually used in die casting. ...
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the maximum displacement and stress of a clamped (fixed) rectangular plate under a uniformly distributed load. ...
eFunda: Plate Calculator -- Clamped circular plate with uniformly ...
This calculator computes the displacement of a clamped circular plate under a uniformly distributed load.
eFunda: Theory of Diaphragm Pressure Gages
Clamped circular plate with uniformly distributed load. where is the bending rigidity of the plate, and h and n are the thickness and Poisson's ratio of the ...
Simply Supported Beam Loading Options
Simply Supported beams under different loading conditions, such as center load, intermediate load, uniformly distributed load, and two equi-distant load.
Engineering Fundamentals: Standard Beams
Database of geometric properties for standard steel and aluminum beams.
Materials: Metal Alloys: Properties
Element, Weight %. Al, 86.00. Si, 12.00. Fe, 2.0. Mechanical Properties. Properties, Conditions. T (°C), Treatment. Density (×1000 kg/m3), 2.6-2.8 · 25 ...