Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Offshore

International news and technology for marine/offshore operations around the world.

Reinforced Plastics

Informed and impartial coverage on the global composites industry.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » S Section Steel I Beam » S24 × 106
S Section Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 2940 in4) for the S24 × 106 S Section Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.16 × 10-6 5.96
200 4.07 × 10-6 11.3
300 6.11 × 10-6 16.9
400 8.14 × 10-6 22.5
500 1.02 × 10-5 28.1
600 1.22 × 10-5 33.8
700 1.42 × 10-5 39.4
800 1.63 × 10-5 45.0
900 1.83 × 10-5 50.6
1000 2.04 × 10-5 56.3
2000 4.07 × 10-5 113
3000 6.11 × 10-5 169
4000 8.14 × 10-5 225
5000 1.02 × 10-4 281
6000 1.22 × 10-4 338
7000 1.42 × 10-4 394
8000 1.63 × 10-4 450
9000 1.83 × 10-4 506
1.00 × 104 2.04 × 10-4 563
2.00 × 104 4.07 × 10-4 1130
3.00 × 104 6.11 × 10-4 1690
4.00 × 104 8.14 × 10-4 2250
5.00 × 104 0.00102 2810
6.00 × 104 0.00122 3380
7.00 × 104 0.00142 3940
8.00 × 104 0.00163 4500
9.00 × 104 0.00183 5060
1.00 × 105 0.00204 5630
2.00 × 105 0.00407 1.13 × 104
3.00 × 105 0.00611 1.69 × 104
4.00 × 105 0.00814 2.25 × 104
5.00 × 105 0.0102 2.81 × 104
6.00 × 105 0.0122 3.38 × 104
7.00 × 105 0.0142 3.94 × 104
8.00 × 105 0.0163 4.50 × 104
9.00 × 105 0.0183 5.06 × 104
1.00 × 106 0.0204 5.63 × 104
2.00 × 106 0.0407 1.13 × 105
3.00 × 106 0.0611 1.69 × 105
4.00 × 106 0.0814 2.25 × 105
5.00 × 106 0.102 2.81 × 105
5.28 × 106 0.107 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.66 × 10-5 16.6
200 3.14 × 10-5 31.3
300 4.71 × 10-5 46.9
400 6.28 × 10-5 62.5
500 7.85 × 10-5 78.1
600 9.42 × 10-5 93.8
700 1.10 × 10-4 109
800 1.26 × 10-4 125
900 1.41 × 10-4 141
1000 1.57 × 10-4 156
2000 3.14 × 10-4 313
3000 4.71 × 10-4 469
4000 6.28 × 10-4 625
5000 7.85 × 10-4 781
6000 9.42 × 10-4 938
7000 0.00110 1090
8000 0.00126 1250
9000 0.00141 1410
1.00 × 104 0.00157 1560
2.00 × 104 0.00314 3130
3.00 × 104 0.00471 4690
4.00 × 104 0.00628 6250
5.00 × 104 0.00785 7810
6.00 × 104 0.00942 9380
7.00 × 104 0.0110 1.09 × 104
8.00 × 104 0.0126 1.25 × 104
9.00 × 104 0.0141 1.41 × 104
1.00 × 105 0.0157 1.56 × 104
2.00 × 105 0.0314 3.13 × 104
3.00 × 105 0.0471 4.69 × 104
4.00 × 105 0.0628 6.25 × 104
5.00 × 105 0.0785 7.81 × 104
6.00 × 105 0.0942 9.38 × 104
7.00 × 105 0.110 1.09 × 105
8.00 × 105 0.126 1.25 × 105
9.00 × 105 0.141 1.41 × 105
1.00 × 106 0.157 1.56 × 105
1.90 × 106 0.299 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.66 × 10-4 66.3
200 5.03 × 10-4 125
300 7.54 × 10-4 188
400 0.00101 250
500 0.00126 313
600 0.00151 375
700 0.00176 438
800 0.00201 500
900 0.00226 563
1000 0.00251 625
2000 0.00503 1250
3000 0.00754 1880
4000 0.0101 2500
5000 0.0126 3130
6000 0.0151 3750
7000 0.0176 4380
8000 0.0201 5000
9000 0.0226 5630
1.00 × 104 0.0251 6250
2.00 × 104 0.0503 1.25 × 104
3.00 × 104 0.0754 1.88 × 104
4.00 × 104 0.101 2.50 × 104
5.00 × 104 0.126 3.13 × 104
6.00 × 104 0.151 3.75 × 104
7.00 × 104 0.176 4.38 × 104
8.00 × 104 0.201 5.00 × 104
9.00 × 104 0.226 5.63 × 104
1.00 × 105 0.251 6.25 × 104
2.00 × 105 0.503 1.25 × 105
3.00 × 105 0.754 1.88 × 105
4.00 × 105 1.01 2.50 × 105
4.75 × 105 1.19 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00135 149
200 0.00254 281
300 0.00382 422
400 0.00509 563
500 0.00636 703
600 0.00763 844
700 0.00890 984
800 0.0102 1130
900 0.0114 1270
1000 0.0127 1410
2000 0.0254 2810
3000 0.0382 4220
4000 0.0509 5630
5000 0.0636 7030
6000 0.0763 8440
7000 0.0890 9840
8000 0.102 1.13 × 104
9000 0.114 1.27 × 104
1.00 × 104 0.127 1.41 × 104
2.00 × 104 0.254 2.81 × 104
3.00 × 104 0.382 4.22 × 104
4.00 × 104 0.509 5.63 × 104
5.00 × 104 0.636 7.03 × 104
6.00 × 104 0.763 8.44 × 104
7.00 × 104 0.890 9.84 × 104
8.00 × 104 1.02 1.13 × 105
9.00 × 104 1.14 1.27 × 105
1.00 × 105 1.27 1.41 × 105
2.00 × 105 2.54 2.81 × 105
2.11 × 105 2.69 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00426 265
200 0.00804 500
300 0.0121 750
400 0.0161 1000
500 0.0201 1250
600 0.0241 1500
700 0.0281 1750
800 0.0322 2000
900 0.0362 2250
1000 0.0402 2500
2000 0.0804 5000
3000 0.121 7500
4000 0.161 1.00 × 104
5000 0.201 1.25 × 104
6000 0.241 1.50 × 104
7000 0.281 1.75 × 104
8000 0.322 2.00 × 104
9000 0.362 2.25 × 104
1.00 × 104 0.402 2.50 × 104
2.00 × 104 0.804 5.00 × 104
3.00 × 104 1.21 7.50 × 104
4.00 × 104 1.61 1.00 × 105
5.00 × 104 2.01 1.25 × 105
6.00 × 104 2.41 1.50 × 105
7.00 × 104 2.81 1.75 × 105
8.00 × 104 3.22 2.00 × 105
9.00 × 104 3.62 2.25 × 105
1.00 × 105 4.02 2.50 × 105
1.19 × 105 4.78 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0104 414
200 0.0196 781
300 0.0294 1170
400 0.0393 1560
500 0.0491 1950
600 0.0589 2340
700 0.0687 2730
800 0.0785 3130
900 0.0883 3520
1000 0.0982 3910
2000 0.196 7810
3000 0.294 1.17 × 104
4000 0.393 1.56 × 104
5000 0.491 1.95 × 104
6000 0.589 2.34 × 104
7000 0.687 2.73 × 104
8000 0.785 3.13 × 104
9000 0.883 3.52 × 104
1.00 × 104 0.982 3.91 × 104
2.00 × 104 1.96 7.81 × 104
3.00 × 104 2.94 1.17 × 105
4.00 × 104 3.93 1.56 × 105
5.00 × 104 4.91 1.95 × 105
6.00 × 104 5.89 2.34 × 105
7.00 × 104 6.87 2.73 × 105
7.60 × 104 7.46 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0216 596
200 0.0407 1130
300 0.0611 1690
400 0.0814 2250
500 0.102 2810
600 0.122 3380
700 0.142 3940
800 0.163 4500
900 0.183 5060
1000 0.204 5630
2000 0.407 1.13 × 104
3000 0.611 1.69 × 104
4000 0.814 2.25 × 104
5000 1.02 2.81 × 104
6000 1.22 3.38 × 104
7000 1.42 3.94 × 104
8000 1.63 4.50 × 104
9000 1.83 5.06 × 104
1.00 × 104 2.04 5.63 × 104
2.00 × 104 4.07 1.13 × 105
3.00 × 104 6.11 1.69 × 105
4.00 × 104 8.14 2.25 × 105
5.00 × 104 10.2 2.81 × 105
5.28 × 104 10.7 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0682 1060
200 0.129 2000
300 0.193 3000
400 0.257 4000
500 0.322 5000
600 0.386 6000
700 0.450 7000
800 0.515 8000
900 0.579 9000
1000 0.643 1.00 × 104
2000 1.29 2.00 × 104
3000 1.93 3.00 × 104
4000 2.57 4.00 × 104
5000 3.22 5.00 × 104
6000 3.86 6.00 × 104
7000 4.50 7.00 × 104
8000 5.15 8.00 × 104
9000 5.79 9.00 × 104
1.00 × 104 6.43 1.00 × 105
2.00 × 104 12.9 2.00 × 105
2.97 × 104 19.1 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.166 1660
200 0.314 3130
300 0.471 4690
400 0.628 6250
500 0.785 7810
600 0.942 9380
700 1.10 1.09 × 104
800 1.26 1.25 × 104
900 1.41 1.41 × 104
1000 1.57 1.56 × 104
2000 3.14 3.13 × 104
3000 4.71 4.69 × 104
4000 6.28 6.25 × 104
5000 7.85 7.81 × 104
6000 9.42 9.38 × 104
7000 11.0 1.09 × 105
8000 12.6 1.25 × 105
9000 14.1 1.41 × 105
1.00 × 104 15.7 1.56 × 105
1.90 × 104 29.9 2.97 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.345 2390
200 0.651 4500
300 0.977 6750
400 1.30 9000
500 1.63 1.13 × 104
600 1.95 1.35 × 104
700 2.28 1.58 × 104
800 2.61 1.80 × 104
900 2.93 2.03 × 104
1000 3.26 2.25 × 104
2000 6.51 4.50 × 104
3000 9.77 6.75 × 104
4000 13.0 9.00 × 104
5000 16.3 1.13 × 105
6000 19.5 1.35 × 105
7000 22.8 1.58 × 105
7520 24.5 1.69 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.639 3250
200 1.21 6130
300 1.81 9190
400 2.41 1.23 × 104
500 3.02 1.53 × 104
600 3.62 1.84 × 104
700 4.22 2.14 × 104
800 4.83 2.45 × 104
900 5.43 2.76 × 104
1000 6.03 3.06 × 104
2000 12.1 6.13 × 104
3000 18.1 9.19 × 104
4000 24.1 1.23 × 105
4060 24.5 1.24 × 105
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.09 4240
200 2.06 8000
300 3.09 1.20 × 104
400 4.12 1.60 × 104
500 5.15 2.00 × 104
600 6.18 2.40 × 104
700 7.20 2.80 × 104
800 8.23 3.20 × 104
900 9.26 3.60 × 104
1000 10.3 4.00 × 104
2000 20.6 8.00 × 104
2380 24.5 9.52 × 104
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.75 5370
200 3.30 1.01 × 104
300 4.95 1.52 × 104
400 6.59 2.03 × 104
500 8.24 2.53 × 104
600 9.89 3.04 × 104
700 11.5 3.54 × 104
800 13.2 4.05 × 104
900 14.8 4.56 × 104
1000 16.5 5.06 × 104
1490 24.5 7.52 × 104
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.66 6630
200 5.03 1.25 × 104
300 7.54 1.88 × 104
400 10.1 2.50 × 104
500 12.6 3.13 × 104
600 15.1 3.75 × 104
700 17.6 4.38 × 104
800 20.1 5.00 × 104
900 22.6 5.63 × 104
975 24.5 6.09 × 104
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 6.50 1.04 × 104
200 12.3 1.95 × 104
300 18.4 2.93 × 104
399 24.5 3.90 × 104
Steel I Beam: S24 × 106 (S Section 24 inch tall × 106 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 13.5 1.49 × 104
193 24.5 2.71 × 104