Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Laser Focus World

Semiconductors, medical equipment, lasers, optics and aviation and aerospace.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 342
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 4900 in4) for the W14 × 342 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 4.18 × 10-6 8.26
400 4.88 × 10-6 9.66
500 6.11 × 10-6 12.1
600 7.33 × 10-6 14.5
700 8.55 × 10-6 16.9
800 9.77 × 10-6 19.3
900 1.10 × 10-5 21.7
1000 1.22 × 10-5 24.2
2000 2.44 × 10-5 48.3
3000 3.66 × 10-5 72.5
4000 4.88 × 10-5 96.6
5000 6.11 × 10-5 121
6000 7.33 × 10-5 145
7000 8.55 × 10-5 169
8000 9.77 × 10-5 193
9000 1.10 × 10-4 217
1.00 × 104 1.22 × 10-4 242
2.00 × 104 2.44 × 10-4 483
3.00 × 104 3.66 × 10-4 725
4.00 × 104 4.88 × 10-4 966
5.00 × 104 6.11 × 10-4 1210
6.00 × 104 7.33 × 10-4 1450
7.00 × 104 8.55 × 10-4 1690
8.00 × 104 9.77 × 10-4 1930
9.00 × 104 0.00110 2170
1.00 × 105 0.00122 2420
2.00 × 105 0.00244 4830
3.00 × 105 0.00366 7250
4.00 × 105 0.00488 9660
5.00 × 105 0.00611 1.21 × 104
6.00 × 105 0.00733 1.45 × 104
7.00 × 105 0.00855 1.69 × 104
8.00 × 105 0.00977 1.93 × 104
9.00 × 105 0.0110 2.17 × 104
1.00 × 106 0.0122 2.42 × 104
2.00 × 106 0.0244 4.83 × 104
3.00 × 106 0.0366 7.25 × 104
4.00 × 106 0.0488 9.66 × 104
5.00 × 106 0.0611 1.21 × 105
6.00 × 106 0.0733 1.45 × 105
7.00 × 106 0.0855 1.69 × 105
8.00 × 106 0.0977 1.93 × 105
9.00 × 106 0.110 2.17 × 105
1.00 × 107 0.122 2.42 × 105
1.23 × 107 0.150 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 3.22 × 10-5 23.0
400 3.77 × 10-5 26.8
500 4.71 × 10-5 33.6
600 5.65 × 10-5 40.3
700 6.60 × 10-5 47.0
800 7.54 × 10-5 53.7
900 8.48 × 10-5 60.4
1000 9.42 × 10-5 67.1
2000 1.88 × 10-4 134
3000 2.83 × 10-4 201
4000 3.77 × 10-4 268
5000 4.71 × 10-4 336
6000 5.65 × 10-4 403
7000 6.60 × 10-4 470
8000 7.54 × 10-4 537
9000 8.48 × 10-4 604
1.00 × 104 9.42 × 10-4 671
2.00 × 104 0.00188 1340
3.00 × 104 0.00283 2010
4.00 × 104 0.00377 2680
5.00 × 104 0.00471 3360
6.00 × 104 0.00565 4030
7.00 × 104 0.00660 4700
8.00 × 104 0.00754 5370
9.00 × 104 0.00848 6040
1.00 × 105 0.00942 6710
2.00 × 105 0.0188 1.34 × 104
3.00 × 105 0.0283 2.01 × 104
4.00 × 105 0.0377 2.68 × 104
5.00 × 105 0.0471 3.36 × 104
6.00 × 105 0.0565 4.03 × 104
7.00 × 105 0.0660 4.70 × 104
8.00 × 105 0.0754 5.37 × 104
9.00 × 105 0.0848 6.04 × 104
1.00 × 106 0.0942 6.71 × 104
2.00 × 106 0.188 1.34 × 105
3.00 × 106 0.283 2.01 × 105
4.00 × 106 0.377 2.68 × 105
4.43 × 106 0.417 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 5.16 × 10-4 91.8
400 6.03 × 10-4 107
500 7.54 × 10-4 134
600 9.05 × 10-4 161
700 0.00106 188
800 0.00121 215
900 0.00136 242
1000 0.00151 268
2000 0.00302 537
3000 0.00452 805
4000 0.00603 1070
5000 0.00754 1340
6000 0.00905 1610
7000 0.0106 1880
8000 0.0121 2150
9000 0.0136 2420
1.00 × 104 0.0151 2680
2.00 × 104 0.0302 5370
3.00 × 104 0.0452 8050
4.00 × 104 0.0603 1.07 × 104
5.00 × 104 0.0754 1.34 × 104
6.00 × 104 0.0905 1.61 × 104
7.00 × 104 0.106 1.88 × 104
8.00 × 104 0.121 2.15 × 104
9.00 × 104 0.136 2.42 × 104
1.00 × 105 0.151 2.68 × 104
2.00 × 105 0.302 5.37 × 104
3.00 × 105 0.452 8.05 × 104
4.00 × 105 0.603 1.07 × 105
5.00 × 105 0.754 1.34 × 105
6.00 × 105 0.905 1.61 × 105
7.00 × 105 1.06 1.88 × 105
8.00 × 105 1.21 2.15 × 105
9.00 × 105 1.36 2.42 × 105
1.00 × 106 1.51 2.68 × 105
1.11 × 106 1.67 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.00261 207
400 0.00305 242
500 0.00382 302
600 0.00458 362
700 0.00534 423
800 0.00611 483
900 0.00687 544
1000 0.00763 604
2000 0.0153 1210
3000 0.0229 1810
4000 0.0305 2420
5000 0.0382 3020
6000 0.0458 3620
7000 0.0534 4230
8000 0.0611 4830
9000 0.0687 5440
1.00 × 104 0.0763 6040
2.00 × 104 0.153 1.21 × 104
3.00 × 104 0.229 1.81 × 104
4.00 × 104 0.305 2.42 × 104
5.00 × 104 0.382 3.02 × 104
6.00 × 104 0.458 3.62 × 104
7.00 × 104 0.534 4.23 × 104
8.00 × 104 0.611 4.83 × 104
9.00 × 104 0.687 5.44 × 104
1.00 × 105 0.763 6.04 × 104
2.00 × 105 1.53 1.21 × 105
3.00 × 105 2.29 1.81 × 105
4.00 × 105 3.05 2.42 × 105
4.92 × 105 3.75 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.00825 367
400 0.00965 430
500 0.0121 537
600 0.0145 644
700 0.0169 752
800 0.0193 859
900 0.0217 966
1000 0.0241 1070
2000 0.0482 2150
3000 0.0724 3220
4000 0.0965 4300
5000 0.121 5370
6000 0.145 6440
7000 0.169 7520
8000 0.193 8590
9000 0.217 9660
1.00 × 104 0.241 1.07 × 104
2.00 × 104 0.482 2.15 × 104
3.00 × 104 0.724 3.22 × 104
4.00 × 104 0.965 4.30 × 104
5.00 × 104 1.21 5.37 × 104
6.00 × 104 1.45 6.44 × 104
7.00 × 104 1.69 7.52 × 104
8.00 × 104 1.93 8.59 × 104
9.00 × 104 2.17 9.66 × 104
1.00 × 105 2.41 1.07 × 105
2.00 × 105 4.82 2.15 × 105
2.77 × 105 6.67 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.0201 574
400 0.0236 671
500 0.0294 839
600 0.0353 1010
700 0.0412 1170
800 0.0471 1340
900 0.0530 1510
1000 0.0589 1680
2000 0.118 3360
3000 0.177 5030
4000 0.236 6710
5000 0.294 8390
6000 0.353 1.01 × 104
7000 0.412 1.17 × 104
8000 0.471 1.34 × 104
9000 0.530 1.51 × 104
1.00 × 104 0.589 1.68 × 104
2.00 × 104 1.18 3.36 × 104
3.00 × 104 1.77 5.03 × 104
4.00 × 104 2.36 6.71 × 104
5.00 × 104 2.94 8.39 × 104
6.00 × 104 3.53 1.01 × 105
7.00 × 104 4.12 1.17 × 105
8.00 × 104 4.71 1.34 × 105
9.00 × 104 5.30 1.51 × 105
1.00 × 105 5.89 1.68 × 105
1.77 × 105 10.4 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.0418 826
400 0.0488 966
500 0.0611 1210
600 0.0733 1450
700 0.0855 1690
800 0.0977 1930
900 0.110 2170
1000 0.122 2420
2000 0.244 4830
3000 0.366 7250
4000 0.488 9660
5000 0.611 1.21 × 104
6000 0.733 1.45 × 104
7000 0.855 1.69 × 104
8000 0.977 1.93 × 104
9000 1.10 2.17 × 104
1.00 × 104 1.22 2.42 × 104
2.00 × 104 2.44 4.83 × 104
3.00 × 104 3.66 7.25 × 104
4.00 × 104 4.88 9.66 × 104
5.00 × 104 6.11 1.21 × 105
6.00 × 104 7.33 1.45 × 105
7.00 × 104 8.55 1.69 × 105
8.00 × 104 9.77 1.93 × 105
9.00 × 104 11.0 2.17 × 105
1.00 × 105 12.2 2.42 × 105
1.23 × 105 15.0 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.132 1470
400 0.154 1720
500 0.193 2150
600 0.232 2580
700 0.270 3010
800 0.309 3440
900 0.347 3870
1000 0.386 4300
2000 0.772 8590
3000 1.16 1.29 × 104
4000 1.54 1.72 × 104
5000 1.93 2.15 × 104
6000 2.32 2.58 × 104
7000 2.70 3.01 × 104
8000 3.09 3.44 × 104
9000 3.47 3.87 × 104
1.00 × 104 3.86 4.30 × 104
2.00 × 104 7.72 8.59 × 104
3.00 × 104 11.6 1.29 × 105
4.00 × 104 15.4 1.72 × 105
4.54 × 104 17.5 1.95 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.322 2300
400 0.377 2680
500 0.471 3360
600 0.565 4030
700 0.660 4700
800 0.754 5370
900 0.848 6040
1000 0.942 6710
2000 1.88 1.34 × 104
3000 2.83 2.01 × 104
4000 3.77 2.68 × 104
5000 4.71 3.36 × 104
6000 5.65 4.03 × 104
7000 6.60 4.70 × 104
8000 7.54 5.37 × 104
9000 8.48 6.04 × 104
1.00 × 104 9.42 6.71 × 104
1.86 × 104 17.5 1.25 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.668 3310
400 0.782 3870
500 0.977 4830
600 1.17 5800
700 1.37 6770
800 1.56 7730
900 1.76 8700
1000 1.95 9660
2000 3.91 1.93 × 104
3000 5.86 2.90 × 104
4000 7.82 3.87 × 104
5000 9.77 4.83 × 104
6000 11.7 5.80 × 104
7000 13.7 6.77 × 104
8000 15.6 7.73 × 104
8980 17.5 8.68 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 1.24 4500
400 1.45 5260
500 1.81 6580
600 2.17 7890
700 2.53 9210
800 2.90 1.05 × 104
900 3.26 1.18 × 104
1000 3.62 1.32 × 104
2000 7.24 2.63 × 104
3000 10.9 3.95 × 104
4000 14.5 5.26 × 104
4850 17.5 6.37 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 2.11 5880
400 2.47 6870
500 3.09 8590
600 3.71 1.03 × 104
700 4.32 1.20 × 104
800 4.94 1.37 × 104
900 5.56 1.55 × 104
1000 6.18 1.72 × 104
2000 12.4 3.44 × 104
2840 17.5 4.88 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 3.38 7440
400 3.96 8700
500 4.95 1.09 × 104
600 5.93 1.30 × 104
700 6.92 1.52 × 104
800 7.91 1.74 × 104
900 8.90 1.96 × 104
1000 9.89 2.17 × 104
1770 17.5 3.86 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 5.16 9180
400 6.03 1.07 × 104
500 7.54 1.34 × 104
600 9.05 1.61 × 104
700 10.6 1.88 × 104
800 12.1 2.15 × 104
900 13.6 2.42 × 104
1000 15.1 2.68 × 104
1160 17.5 3.12 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 12.6 1.43 × 104
400 14.7 1.68 × 104
477 17.5 2.00 × 104
Additional Information
Related Pages
Glossary