Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

World Pumps

Major news, innovation and real-life applications for pumps and ancillary equipment.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W21 × 132
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 3220 in4) for the W21 × 132 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 2.45 × 10-6 6.04
200 3.72 × 10-6 9.15
300 5.57 × 10-6 13.7
400 7.43 × 10-6 18.3
500 9.29 × 10-6 22.9
600 1.11 × 10-5 27.5
700 1.30 × 10-5 32.0
800 1.49 × 10-5 36.6
900 1.67 × 10-5 41.2
1000 1.86 × 10-5 45.8
2000 3.72 × 10-5 91.5
3000 5.57 × 10-5 137
4000 7.43 × 10-5 183
5000 9.29 × 10-5 229
6000 1.11 × 10-4 275
7000 1.30 × 10-4 320
8000 1.49 × 10-4 366
9000 1.67 × 10-4 412
1.00 × 104 1.86 × 10-4 458
2.00 × 104 3.72 × 10-4 915
3.00 × 104 5.57 × 10-4 1370
4.00 × 104 7.43 × 10-4 1830
5.00 × 104 9.29 × 10-4 2290
6.00 × 104 0.00111 2750
7.00 × 104 0.00130 3200
8.00 × 104 0.00149 3660
9.00 × 104 0.00167 4120
1.00 × 105 0.00186 4580
2.00 × 105 0.00372 9150
3.00 × 105 0.00557 1.37 × 104
4.00 × 105 0.00743 1.83 × 104
5.00 × 105 0.00929 2.29 × 104
6.00 × 105 0.0111 2.75 × 104
7.00 × 105 0.0130 3.20 × 104
8.00 × 105 0.0149 3.66 × 104
9.00 × 105 0.0167 4.12 × 104
1.00 × 106 0.0186 4.58 × 104
2.00 × 106 0.0372 9.15 × 104
3.00 × 106 0.0557 1.37 × 105
4.00 × 106 0.0743 1.83 × 105
5.00 × 106 0.0929 2.29 × 105
6.00 × 106 0.111 2.75 × 105
6.49 × 106 0.121 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 1.89 × 10-5 16.8
200 2.87 × 10-5 25.4
300 4.30 × 10-5 38.1
400 5.74 × 10-5 50.8
500 7.17 × 10-5 63.6
600 8.60 × 10-5 76.3
700 1.00 × 10-4 89.0
800 1.15 × 10-4 102
900 1.29 × 10-4 114
1000 1.43 × 10-4 127
2000 2.87 × 10-4 254
3000 4.30 × 10-4 381
4000 5.74 × 10-4 508
5000 7.17 × 10-4 636
6000 8.60 × 10-4 763
7000 0.00100 890
8000 0.00115 1020
9000 0.00129 1140
1.00 × 104 0.00143 1270
2.00 × 104 0.00287 2540
3.00 × 104 0.00430 3810
4.00 × 104 0.00574 5080
5.00 × 104 0.00717 6360
6.00 × 104 0.00860 7630
7.00 × 104 0.0100 8900
8.00 × 104 0.0115 1.02 × 104
9.00 × 104 0.0129 1.14 × 104
1.00 × 105 0.0143 1.27 × 104
2.00 × 105 0.0287 2.54 × 104
3.00 × 105 0.0430 3.81 × 104
4.00 × 105 0.0574 5.08 × 104
5.00 × 105 0.0717 6.36 × 104
6.00 × 105 0.0860 7.63 × 104
7.00 × 105 0.100 8.90 × 104
8.00 × 105 0.115 1.02 × 105
9.00 × 105 0.129 1.14 × 105
1.00 × 106 0.143 1.27 × 105
2.00 × 106 0.287 2.54 × 105
2.34 × 106 0.335 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 3.03 × 10-4 67.1
200 4.59 × 10-4 102
300 6.88 × 10-4 153
400 9.18 × 10-4 203
500 0.00115 254
600 0.00138 305
700 0.00161 356
800 0.00184 407
900 0.00206 458
1000 0.00229 508
2000 0.00459 1020
3000 0.00688 1530
4000 0.00918 2030
5000 0.0115 2540
6000 0.0138 3050
7000 0.0161 3560
8000 0.0184 4070
9000 0.0206 4580
1.00 × 104 0.0229 5080
2.00 × 104 0.0459 1.02 × 104
3.00 × 104 0.0688 1.53 × 104
4.00 × 104 0.0918 2.03 × 104
5.00 × 104 0.115 2.54 × 104
6.00 × 104 0.138 3.05 × 104
7.00 × 104 0.161 3.56 × 104
8.00 × 104 0.184 4.07 × 104
9.00 × 104 0.206 4.58 × 104
1.00 × 105 0.229 5.08 × 104
2.00 × 105 0.459 1.02 × 105
3.00 × 105 0.688 1.53 × 105
4.00 × 105 0.918 2.03 × 105
5.00 × 105 1.15 2.54 × 105
5.84 × 105 1.34 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.00153 151
200 0.00232 229
300 0.00348 343
400 0.00465 458
500 0.00581 572
600 0.00697 686
700 0.00813 801
800 0.00929 915
900 0.0105 1030
1000 0.0116 1140
2000 0.0232 2290
3000 0.0348 3430
4000 0.0465 4580
5000 0.0581 5720
6000 0.0697 6860
7000 0.0813 8010
8000 0.0929 9150
9000 0.105 1.03 × 104
1.00 × 104 0.116 1.14 × 104
2.00 × 104 0.232 2.29 × 104
3.00 × 104 0.348 3.43 × 104
4.00 × 104 0.465 4.58 × 104
5.00 × 104 0.581 5.72 × 104
6.00 × 104 0.697 6.86 × 104
7.00 × 104 0.813 8.01 × 104
8.00 × 104 0.929 9.15 × 104
9.00 × 104 1.05 1.03 × 105
1.00 × 105 1.16 1.14 × 105
2.00 × 105 2.32 2.29 × 105
2.60 × 105 3.02 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.00485 268
200 0.00734 407
300 0.0110 610
400 0.0147 814
500 0.0184 1020
600 0.0220 1220
700 0.0257 1420
800 0.0294 1630
900 0.0330 1830
1000 0.0367 2030
2000 0.0734 4070
3000 0.110 6100
4000 0.147 8140
5000 0.184 1.02 × 104
6000 0.220 1.22 × 104
7000 0.257 1.42 × 104
8000 0.294 1.63 × 104
9000 0.330 1.83 × 104
1.00 × 104 0.367 2.03 × 104
2.00 × 104 0.734 4.07 × 104
3.00 × 104 1.10 6.10 × 104
4.00 × 104 1.47 8.14 × 104
5.00 × 104 1.84 1.02 × 105
6.00 × 104 2.20 1.22 × 105
7.00 × 104 2.57 1.42 × 105
8.00 × 104 2.94 1.63 × 105
9.00 × 104 3.30 1.83 × 105
1.00 × 105 3.67 2.03 × 105
1.46 × 105 5.36 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.0118 419
200 0.0179 636
300 0.0269 953
400 0.0358 1270
500 0.0448 1590
600 0.0538 1910
700 0.0627 2220
800 0.0717 2540
900 0.0807 2860
1000 0.0896 3180
2000 0.179 6360
3000 0.269 9530
4000 0.358 1.27 × 104
5000 0.448 1.59 × 104
6000 0.538 1.91 × 104
7000 0.627 2.22 × 104
8000 0.717 2.54 × 104
9000 0.807 2.86 × 104
1.00 × 104 0.896 3.18 × 104
2.00 × 104 1.79 6.36 × 104
3.00 × 104 2.69 9.53 × 104
4.00 × 104 3.58 1.27 × 105
5.00 × 104 4.48 1.59 × 105
6.00 × 104 5.38 1.91 × 105
7.00 × 104 6.27 2.22 × 105
8.00 × 104 7.17 2.54 × 105
9.00 × 104 8.07 2.86 × 105
9.35 × 104 8.38 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.0245 604
200 0.0372 915
300 0.0557 1370
400 0.0743 1830
500 0.0929 2290
600 0.111 2750
700 0.130 3200
800 0.149 3660
900 0.167 4120
1000 0.186 4580
2000 0.372 9150
3000 0.557 1.37 × 104
4000 0.743 1.83 × 104
5000 0.929 2.29 × 104
6000 1.11 2.75 × 104
7000 1.30 3.20 × 104
8000 1.49 3.66 × 104
9000 1.67 4.12 × 104
1.00 × 104 1.86 4.58 × 104
2.00 × 104 3.72 9.15 × 104
3.00 × 104 5.57 1.37 × 105
4.00 × 104 7.43 1.83 × 105
5.00 × 104 9.29 2.29 × 105
6.00 × 104 11.1 2.75 × 105
6.49 × 104 12.1 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.0775 1070
200 0.117 1630
300 0.176 2440
400 0.235 3250
500 0.294 4070
600 0.352 4880
700 0.411 5690
800 0.470 6510
900 0.529 7320
1000 0.587 8140
2000 1.17 1.63 × 104
3000 1.76 2.44 × 104
4000 2.35 3.25 × 104
5000 2.94 4.07 × 104
6000 3.52 4.88 × 104
7000 4.11 5.69 × 104
8000 4.70 6.51 × 104
9000 5.29 7.32 × 104
1.00 × 104 5.87 8.14 × 104
2.00 × 104 11.7 1.63 × 105
3.00 × 104 17.6 2.44 × 105
3.65 × 104 21.4 2.97 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.189 1680
200 0.287 2540
300 0.430 3810
400 0.574 5080
500 0.717 6360
600 0.860 7630
700 1.00 8900
800 1.15 1.02 × 104
900 1.29 1.14 × 104
1000 1.43 1.27 × 104
2000 2.87 2.54 × 104
3000 4.30 3.81 × 104
4000 5.74 5.08 × 104
5000 7.17 6.36 × 104
6000 8.60 7.63 × 104
7000 10.0 8.90 × 104
8000 11.5 1.02 × 105
9000 12.9 1.14 × 105
1.00 × 104 14.3 1.27 × 105
1.52 × 104 21.8 1.94 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.392 2420
200 0.595 3660
300 0.892 5490
400 1.19 7320
500 1.49 9150
600 1.78 1.10 × 104
700 2.08 1.28 × 104
800 2.38 1.46 × 104
900 2.68 1.65 × 104
1000 2.97 1.83 × 104
2000 5.95 3.66 × 104
3000 8.92 5.49 × 104
4000 11.9 7.32 × 104
5000 14.9 9.15 × 104
6000 17.8 1.10 × 105
7000 20.8 1.28 × 105
7340 21.8 1.34 × 105
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 0.727 3290
200 1.10 4980
300 1.65 7470
400 2.20 9970
500 2.75 1.25 × 104
600 3.30 1.49 × 104
700 3.86 1.74 × 104
800 4.41 1.99 × 104
900 4.96 2.24 × 104
1000 5.51 2.49 × 104
2000 11.0 4.98 × 104
3000 16.5 7.47 × 104
3960 21.8 9.87 × 104
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 1.24 4300
200 1.88 6510
300 2.82 9760
400 3.76 1.30 × 104
500 4.70 1.63 × 104
600 5.64 1.95 × 104
700 6.58 2.28 × 104
800 7.52 2.60 × 104
900 8.46 2.93 × 104
1000 9.40 3.25 × 104
2000 18.8 6.51 × 104
2320 21.8 7.56 × 104
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 1.99 5440
200 3.01 8240
300 4.52 1.24 × 104
400 6.02 1.65 × 104
500 7.53 2.06 × 104
600 9.03 2.47 × 104
700 10.5 2.88 × 104
800 12.0 3.29 × 104
900 13.5 3.71 × 104
1000 15.1 4.12 × 104
1450 21.8 5.97 × 104
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 3.03 6710
200 4.59 1.02 × 104
300 6.88 1.53 × 104
400 9.18 2.03 × 104
500 11.5 2.54 × 104
600 13.8 3.05 × 104
700 16.1 3.56 × 104
800 18.4 4.07 × 104
900 20.6 4.58 × 104
952 21.8 4.84 × 104
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 7.39 1.05 × 104
200 11.2 1.59 × 104
300 16.8 2.38 × 104
390 21.8 3.10 × 104
Steel I Beam: W21 × 132 (Wide Flange 21 inch tall × 132 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
132 15.3 1.51 × 104
188 21.8 2.15 × 104
Additional Information