Reinforced Plastics

Informed and impartial coverage on the global composites industry.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W21 × 93
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 2070 in4) for the W21 × 93 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 2.69 × 10-6 6.56
100 2.89 × 10-6 7.05
200 5.78 × 10-6 14.1
300 8.67 × 10-6 21.1
400 1.16 × 10-5 28.2
500 1.45 × 10-5 35.3
600 1.73 × 10-5 42.3
700 2.02 × 10-5 49.4
800 2.31 × 10-5 56.4
900 2.60 × 10-5 63.5
1000 2.89 × 10-5 70.5
2000 5.78 × 10-5 141
3000 8.67 × 10-5 212
4000 1.16 × 10-4 282
5000 1.45 × 10-4 353
6000 1.73 × 10-4 423
7000 2.02 × 10-4 494
8000 2.31 × 10-4 564
9000 2.60 × 10-4 635
1.00 × 104 2.89 × 10-4 705
2.00 × 104 5.78 × 10-4 1410
3.00 × 104 8.67 × 10-4 2120
4.00 × 104 0.00116 2820
5.00 × 104 0.00145 3530
6.00 × 104 0.00173 4230
7.00 × 104 0.00202 4940
8.00 × 104 0.00231 5640
9.00 × 104 0.00260 6350
1.00 × 105 0.00289 7050
2.00 × 105 0.00578 1.41 × 104
3.00 × 105 0.00867 2.12 × 104
4.00 × 105 0.0116 2.82 × 104
5.00 × 105 0.0145 3.53 × 104
6.00 × 105 0.0173 4.23 × 104
7.00 × 105 0.0202 4.94 × 104
8.00 × 105 0.0231 5.64 × 104
9.00 × 105 0.0260 6.35 × 104
1.00 × 106 0.0289 7.05 × 104
2.00 × 106 0.0578 1.41 × 105
3.00 × 106 0.0867 2.12 × 105
4.00 × 106 0.116 2.82 × 105
4.21 × 106 0.122 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 2.07 × 10-5 18.2
100 2.23 × 10-5 19.6
200 4.46 × 10-5 39.2
300 6.69 × 10-5 58.8
400 8.92 × 10-5 78.3
500 1.12 × 10-4 97.9
600 1.34 × 10-4 118
700 1.56 × 10-4 137
800 1.78 × 10-4 157
900 2.01 × 10-4 176
1000 2.23 × 10-4 196
2000 4.46 × 10-4 392
3000 6.69 × 10-4 588
4000 8.92 × 10-4 783
5000 0.00112 979
6000 0.00134 1180
7000 0.00156 1370
8000 0.00178 1570
9000 0.00201 1760
1.00 × 104 0.00223 1960
2.00 × 104 0.00446 3920
3.00 × 104 0.00669 5880
4.00 × 104 0.00892 7830
5.00 × 104 0.0112 9790
6.00 × 104 0.0134 1.18 × 104
7.00 × 104 0.0156 1.37 × 104
8.00 × 104 0.0178 1.57 × 104
9.00 × 104 0.0201 1.76 × 104
1.00 × 105 0.0223 1.96 × 104
2.00 × 105 0.0446 3.92 × 104
3.00 × 105 0.0669 5.88 × 104
4.00 × 105 0.0892 7.83 × 104
5.00 × 105 0.112 9.79 × 104
6.00 × 105 0.134 1.18 × 105
7.00 × 105 0.156 1.37 × 105
8.00 × 105 0.178 1.57 × 105
9.00 × 105 0.201 1.76 × 105
1.00 × 106 0.223 1.96 × 105
1.52 × 106 0.338 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 3.32 × 10-4 72.8
100 3.57 × 10-4 78.3
200 7.14 × 10-4 157
300 0.00107 235
400 0.00143 313
500 0.00178 392
600 0.00214 470
700 0.00250 548
800 0.00285 627
900 0.00321 705
1000 0.00357 783
2000 0.00714 1570
3000 0.0107 2350
4000 0.0143 3130
5000 0.0178 3920
6000 0.0214 4700
7000 0.0250 5480
8000 0.0285 6270
9000 0.0321 7050
1.00 × 104 0.0357 7830
2.00 × 104 0.0714 1.57 × 104
3.00 × 104 0.107 2.35 × 104
4.00 × 104 0.143 3.13 × 104
5.00 × 104 0.178 3.92 × 104
6.00 × 104 0.214 4.70 × 104
7.00 × 104 0.250 5.48 × 104
8.00 × 104 0.285 6.27 × 104
9.00 × 104 0.321 7.05 × 104
1.00 × 105 0.357 7.83 × 104
2.00 × 105 0.714 1.57 × 105
3.00 × 105 1.07 2.35 × 105
3.79 × 105 1.35 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.00168 164
100 0.00181 176
200 0.00361 353
300 0.00542 529
400 0.00723 705
500 0.00903 881
600 0.0108 1060
700 0.0126 1230
800 0.0145 1410
900 0.0163 1590
1000 0.0181 1760
2000 0.0361 3530
3000 0.0542 5290
4000 0.0723 7050
5000 0.0903 8810
6000 0.108 1.06 × 104
7000 0.126 1.23 × 104
8000 0.145 1.41 × 104
9000 0.163 1.59 × 104
1.00 × 104 0.181 1.76 × 104
2.00 × 104 0.361 3.53 × 104
3.00 × 104 0.542 5.29 × 104
4.00 × 104 0.723 7.05 × 104
5.00 × 104 0.903 8.81 × 104
6.00 × 104 1.08 1.06 × 105
7.00 × 104 1.26 1.23 × 105
8.00 × 104 1.45 1.41 × 105
9.00 × 104 1.63 1.59 × 105
1.00 × 105 1.81 1.76 × 105
1.69 × 105 3.04 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.00531 291
100 0.00571 313
200 0.0114 627
300 0.0171 940
400 0.0228 1250
500 0.0285 1570
600 0.0343 1880
700 0.0400 2190
800 0.0457 2510
900 0.0514 2820
1000 0.0571 3130
2000 0.114 6270
3000 0.171 9400
4000 0.228 1.25 × 104
5000 0.285 1.57 × 104
6000 0.343 1.88 × 104
7000 0.400 2.19 × 104
8000 0.457 2.51 × 104
9000 0.514 2.82 × 104
1.00 × 104 0.571 3.13 × 104
2.00 × 104 1.14 6.27 × 104
3.00 × 104 1.71 9.40 × 104
4.00 × 104 2.28 1.25 × 105
5.00 × 104 2.85 1.57 × 105
6.00 × 104 3.43 1.88 × 105
7.00 × 104 4.00 2.19 × 105
8.00 × 104 4.57 2.51 × 105
9.00 × 104 5.14 2.82 × 105
9.48 × 104 5.41 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.0130 455
100 0.0139 490
200 0.0279 979
300 0.0418 1470
400 0.0558 1960
500 0.0697 2450
600 0.0836 2940
700 0.0976 3430
800 0.112 3920
900 0.125 4410
1000 0.139 4900
2000 0.279 9790
3000 0.418 1.47 × 104
4000 0.558 1.96 × 104
5000 0.697 2.45 × 104
6000 0.836 2.94 × 104
7000 0.976 3.43 × 104
8000 1.12 3.92 × 104
9000 1.25 4.41 × 104
1.00 × 104 1.39 4.90 × 104
2.00 × 104 2.79 9.79 × 104
3.00 × 104 4.18 1.47 × 105
4.00 × 104 5.58 1.96 × 105
5.00 × 104 6.97 2.45 × 105
6.00 × 104 8.36 2.94 × 105
6.07 × 104 8.46 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.0269 656
100 0.0289 705
200 0.0578 1410
300 0.0867 2120
400 0.116 2820
500 0.145 3530
600 0.173 4230
700 0.202 4940
800 0.231 5640
900 0.260 6350
1000 0.289 7050
2000 0.578 1.41 × 104
3000 0.867 2.12 × 104
4000 1.16 2.82 × 104
5000 1.45 3.53 × 104
6000 1.73 4.23 × 104
7000 2.02 4.94 × 104
8000 2.31 5.64 × 104
9000 2.60 6.35 × 104
1.00 × 104 2.89 7.05 × 104
2.00 × 104 5.78 1.41 × 105
3.00 × 104 8.67 2.12 × 105
4.00 × 104 11.6 2.82 × 105
4.21 × 104 12.2 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.0850 1170
100 0.0914 1250
200 0.183 2510
300 0.274 3760
400 0.365 5010
500 0.457 6270
600 0.548 7520
700 0.640 8770
800 0.731 1.00 × 104
900 0.822 1.13 × 104
1000 0.914 1.25 × 104
2000 1.83 2.51 × 104
3000 2.74 3.76 × 104
4000 3.65 5.01 × 104
5000 4.57 6.27 × 104
6000 5.48 7.52 × 104
7000 6.40 8.77 × 104
8000 7.31 1.00 × 105
9000 8.22 1.13 × 105
1.00 × 104 9.14 1.25 × 105
2.00 × 104 18.3 2.51 × 105
2.37 × 104 21.7 2.97 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.207 1820
100 0.223 1960
200 0.446 3920
300 0.669 5880
400 0.892 7830
500 1.12 9790
600 1.34 1.18 × 104
700 1.56 1.37 × 104
800 1.78 1.57 × 104
900 2.01 1.76 × 104
1000 2.23 1.96 × 104
2000 4.46 3.92 × 104
3000 6.69 5.88 × 104
4000 8.92 7.83 × 104
5000 11.2 9.79 × 104
6000 13.4 1.18 × 105
7000 15.6 1.37 × 105
8000 17.8 1.57 × 105
9000 20.1 1.76 × 105
9690 21.6 1.90 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.430 2620
100 0.463 2820
200 0.925 5640
300 1.39 8460
400 1.85 1.13 × 104
500 2.31 1.41 × 104
600 2.78 1.69 × 104
700 3.24 1.97 × 104
800 3.70 2.26 × 104
900 4.16 2.54 × 104
1000 4.63 2.82 × 104
2000 9.25 5.64 × 104
3000 13.9 8.46 × 104
4000 18.5 1.13 × 105
4670 21.6 1.32 × 105
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 0.797 3570
100 0.857 3840
200 1.71 7680
300 2.57 1.15 × 104
400 3.43 1.54 × 104
500 4.28 1.92 × 104
600 5.14 2.30 × 104
700 6.00 2.69 × 104
800 6.85 3.07 × 104
900 7.71 3.45 × 104
1000 8.57 3.84 × 104
2000 17.1 7.68 × 104
2520 21.6 9.68 × 104
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 1.36 4660
100 1.46 5010
200 2.92 1.00 × 104
300 4.39 1.50 × 104
400 5.85 2.01 × 104
500 7.31 2.51 × 104
600 8.77 3.01 × 104
700 10.2 3.51 × 104
800 11.7 4.01 × 104
900 13.2 4.51 × 104
1000 14.6 5.01 × 104
1480 21.6 7.42 × 104
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 2.18 5900
100 2.34 6350
200 4.68 1.27 × 104
300 7.02 1.90 × 104
400 9.37 2.54 × 104
500 11.7 3.17 × 104
600 14.0 3.81 × 104
700 16.4 4.44 × 104
800 18.7 5.08 × 104
900 21.1 5.71 × 104
923 21.6 5.86 × 104
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 3.32 7290
100 3.57 7830
200 7.14 1.57 × 104
300 10.7 2.35 × 104
400 14.3 3.13 × 104
500 17.8 3.92 × 104
600 21.4 4.70 × 104
606 21.6 4.75 × 104
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 8.10 1.14 × 104
100 8.71 1.22 × 104
200 17.4 2.45 × 104
248 21.6 3.04 × 104
Steel I Beam: W21 × 93 (Wide Flange 21 inch tall × 93 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
93.0 16.8 1.64 × 104
100 18.1 1.76 × 104
120 21.6 2.11 × 104