Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

Machine Design

How-to, in-depth technical articles for machine design engineers

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W12 × 336
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 4060 in4) for the W12 × 336 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 4.95 × 10-6 9.40
400 5.90 × 10-6 11.2
500 7.37 × 10-6 14.0
600 8.84 × 10-6 16.8
700 1.03 × 10-5 19.6
800 1.18 × 10-5 22.4
900 1.33 × 10-5 25.2
1000 1.47 × 10-5 28.0
2000 2.95 × 10-5 55.9
3000 4.42 × 10-5 83.9
4000 5.90 × 10-5 112
5000 7.37 × 10-5 140
6000 8.84 × 10-5 168
7000 1.03 × 10-4 196
8000 1.18 × 10-4 224
9000 1.33 × 10-4 252
1.00 × 104 1.47 × 10-4 280
2.00 × 104 2.95 × 10-4 559
3.00 × 104 4.42 × 10-4 839
4.00 × 104 5.90 × 10-4 1120
5.00 × 104 7.37 × 10-4 1400
6.00 × 104 8.84 × 10-4 1680
7.00 × 104 0.00103 1960
8.00 × 104 0.00118 2240
9.00 × 104 0.00133 2520
1.00 × 105 0.00147 2800
2.00 × 105 0.00295 5590
3.00 × 105 0.00442 8390
4.00 × 105 0.00590 1.12 × 104
5.00 × 105 0.00737 1.40 × 104
6.00 × 105 0.00884 1.68 × 104
7.00 × 105 0.0103 1.96 × 104
8.00 × 105 0.0118 2.24 × 104
9.00 × 105 0.0133 2.52 × 104
1.00 × 106 0.0147 2.80 × 104
2.00 × 106 0.0295 5.59 × 104
3.00 × 106 0.0442 8.39 × 104
4.00 × 106 0.0590 1.12 × 105
5.00 × 106 0.0737 1.40 × 105
6.00 × 106 0.0884 1.68 × 105
7.00 × 106 0.103 1.96 × 105
8.00 × 106 0.118 2.24 × 105
9.00 × 106 0.133 2.52 × 105
1.00 × 107 0.147 2.80 × 105
1.06 × 107 0.157 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 3.82 × 10-5 26.1
400 4.55 × 10-5 31.1
500 5.69 × 10-5 38.8
600 6.82 × 10-5 46.6
700 7.96 × 10-5 54.4
800 9.10 × 10-5 62.1
900 1.02 × 10-4 69.9
1000 1.14 × 10-4 77.7
2000 2.27 × 10-4 155
3000 3.41 × 10-4 233
4000 4.55 × 10-4 311
5000 5.69 × 10-4 388
6000 6.82 × 10-4 466
7000 7.96 × 10-4 544
8000 9.10 × 10-4 621
9000 0.00102 699
1.00 × 104 0.00114 777
2.00 × 104 0.00227 1550
3.00 × 104 0.00341 2330
4.00 × 104 0.00455 3110
5.00 × 104 0.00569 3880
6.00 × 104 0.00682 4660
7.00 × 104 0.00796 5440
8.00 × 104 0.00910 6210
9.00 × 104 0.0102 6990
1.00 × 105 0.0114 7770
2.00 × 105 0.0227 1.55 × 104
3.00 × 105 0.0341 2.33 × 104
4.00 × 105 0.0455 3.11 × 104
5.00 × 105 0.0569 3.88 × 104
6.00 × 105 0.0682 4.66 × 104
7.00 × 105 0.0796 5.44 × 104
8.00 × 105 0.0910 6.21 × 104
9.00 × 105 0.102 6.99 × 104
1.00 × 106 0.114 7.77 × 104
2.00 × 106 0.227 1.55 × 105
3.00 × 106 0.341 2.33 × 105
3.82 × 106 0.435 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 6.11 × 10-4 104
400 7.28 × 10-4 124
500 9.10 × 10-4 155
600 0.00109 186
700 0.00127 218
800 0.00146 249
900 0.00164 280
1000 0.00182 311
2000 0.00364 621
3000 0.00546 932
4000 0.00728 1240
5000 0.00910 1550
6000 0.0109 1860
7000 0.0127 2180
8000 0.0146 2490
9000 0.0164 2800
1.00 × 104 0.0182 3110
2.00 × 104 0.0364 6210
3.00 × 104 0.0546 9320
4.00 × 104 0.0728 1.24 × 104
5.00 × 104 0.0910 1.55 × 104
6.00 × 104 0.109 1.86 × 104
7.00 × 104 0.127 2.18 × 104
8.00 × 104 0.146 2.49 × 104
9.00 × 104 0.164 2.80 × 104
1.00 × 105 0.182 3.11 × 104
2.00 × 105 0.364 6.21 × 104
3.00 × 105 0.546 9.32 × 104
4.00 × 105 0.728 1.24 × 105
5.00 × 105 0.910 1.55 × 105
6.00 × 105 1.09 1.86 × 105
7.00 × 105 1.27 2.18 × 105
8.00 × 105 1.46 2.49 × 105
9.00 × 105 1.64 2.80 × 105
9.56 × 105 1.74 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.00309 235
400 0.00368 280
500 0.00461 350
600 0.00553 419
700 0.00645 489
800 0.00737 559
900 0.00829 629
1000 0.00921 699
2000 0.0184 1400
3000 0.0276 2100
4000 0.0368 2800
5000 0.0461 3500
6000 0.0553 4190
7000 0.0645 4890
8000 0.0737 5590
9000 0.0829 6290
1.00 × 104 0.0921 6990
2.00 × 104 0.184 1.40 × 104
3.00 × 104 0.276 2.10 × 104
4.00 × 104 0.368 2.80 × 104
5.00 × 104 0.461 3.50 × 104
6.00 × 104 0.553 4.19 × 104
7.00 × 104 0.645 4.89 × 104
8.00 × 104 0.737 5.59 × 104
9.00 × 104 0.829 6.29 × 104
1.00 × 105 0.921 6.99 × 104
2.00 × 105 1.84 1.40 × 105
3.00 × 105 2.76 2.10 × 105
4.00 × 105 3.68 2.80 × 105
4.25 × 105 3.91 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.00978 418
400 0.0116 497
500 0.0146 621
600 0.0175 746
700 0.0204 870
800 0.0233 994
900 0.0262 1120
1000 0.0291 1240
2000 0.0582 2490
3000 0.0873 3730
4000 0.116 4970
5000 0.146 6210
6000 0.175 7460
7000 0.204 8700
8000 0.233 9940
9000 0.262 1.12 × 104
1.00 × 104 0.291 1.24 × 104
2.00 × 104 0.582 2.49 × 104
3.00 × 104 0.873 3.73 × 104
4.00 × 104 1.16 4.97 × 104
5.00 × 104 1.46 6.21 × 104
6.00 × 104 1.75 7.46 × 104
7.00 × 104 2.04 8.70 × 104
8.00 × 104 2.33 9.94 × 104
9.00 × 104 2.62 1.12 × 105
1.00 × 105 2.91 1.24 × 105
2.00 × 105 5.82 2.49 × 105
2.39 × 105 6.96 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.0239 653
400 0.0284 777
500 0.0355 971
600 0.0426 1170
700 0.0498 1360
800 0.0569 1550
900 0.0640 1750
1000 0.0711 1940
2000 0.142 3880
3000 0.213 5830
4000 0.284 7770
5000 0.355 9710
6000 0.426 1.17 × 104
7000 0.498 1.36 × 104
8000 0.569 1.55 × 104
9000 0.640 1.75 × 104
1.00 × 104 0.711 1.94 × 104
2.00 × 104 1.42 3.88 × 104
3.00 × 104 2.13 5.83 × 104
4.00 × 104 2.84 7.77 × 104
5.00 × 104 3.55 9.71 × 104
6.00 × 104 4.26 1.17 × 105
7.00 × 104 4.98 1.36 × 105
8.00 × 104 5.69 1.55 × 105
9.00 × 104 6.40 1.75 × 105
1.00 × 105 7.11 1.94 × 105
1.53 × 105 10.9 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.0495 940
400 0.0590 1120
500 0.0737 1400
600 0.0884 1680
700 0.103 1960
800 0.118 2240
900 0.133 2520
1000 0.147 2800
2000 0.295 5590
3000 0.442 8390
4000 0.590 1.12 × 104
5000 0.737 1.40 × 104
6000 0.884 1.68 × 104
7000 1.03 1.96 × 104
8000 1.18 2.24 × 104
9000 1.33 2.52 × 104
1.00 × 104 1.47 2.80 × 104
2.00 × 104 2.95 5.59 × 104
3.00 × 104 4.42 8.39 × 104
4.00 × 104 5.90 1.12 × 105
5.00 × 104 7.37 1.40 × 105
6.00 × 104 8.84 1.68 × 105
7.00 × 104 10.3 1.96 × 105
8.00 × 104 11.8 2.24 × 105
9.00 × 104 13.3 2.52 × 105
1.00 × 105 14.7 2.80 × 105
1.06 × 105 15.7 2.97 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.157 1670
400 0.186 1990
500 0.233 2490
600 0.279 2980
700 0.326 3480
800 0.373 3980
900 0.419 4470
1000 0.466 4970
2000 0.932 9940
3000 1.40 1.49 × 104
4000 1.86 1.99 × 104
5000 2.33 2.49 × 104
6000 2.79 2.98 × 104
7000 3.26 3.48 × 104
8000 3.73 3.98 × 104
9000 4.19 4.47 × 104
1.00 × 104 4.66 4.97 × 104
2.00 × 104 9.32 9.94 × 104
3.00 × 104 14.0 1.49 × 105
3.61 × 104 16.8 1.80 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.382 2610
400 0.455 3110
500 0.569 3880
600 0.682 4660
700 0.796 5440
800 0.910 6210
900 1.02 6990
1000 1.14 7770
2000 2.27 1.55 × 104
3000 3.41 2.33 × 104
4000 4.55 3.11 × 104
5000 5.69 3.88 × 104
6000 6.82 4.66 × 104
7000 7.96 5.44 × 104
8000 9.10 6.21 × 104
9000 10.2 6.99 × 104
1.00 × 104 11.4 7.77 × 104
1.48 × 104 16.8 1.15 × 105
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 0.792 3760
400 0.943 4470
500 1.18 5590
600 1.41 6710
700 1.65 7830
800 1.89 8950
900 2.12 1.01 × 104
1000 2.36 1.12 × 104
2000 4.72 2.24 × 104
3000 7.07 3.36 × 104
4000 9.43 4.47 × 104
5000 11.8 5.59 × 104
6000 14.1 6.71 × 104
7000 16.5 7.83 × 104
7130 16.8 7.98 × 104
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 1.47 5120
400 1.75 6090
500 2.18 7610
600 2.62 9140
700 3.06 1.07 × 104
800 3.49 1.22 × 104
900 3.93 1.37 × 104
1000 4.37 1.52 × 104
2000 8.74 3.05 × 104
3000 13.1 4.57 × 104
3850 16.8 5.86 × 104
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 2.50 6680
400 2.98 7950
500 3.73 9940
600 4.47 1.19 × 104
700 5.22 1.39 × 104
800 5.96 1.59 × 104
900 6.71 1.79 × 104
1000 7.45 1.99 × 104
2000 14.9 3.98 × 104
2260 16.8 4.49 × 104
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 4.01 8460
400 4.78 1.01 × 104
500 5.97 1.26 × 104
600 7.16 1.51 × 104
700 8.36 1.76 × 104
800 9.55 2.01 × 104
900 10.7 2.27 × 104
1000 11.9 2.52 × 104
1410 16.8 3.55 × 104
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 6.11 1.04 × 104
400 7.28 1.24 × 104
500 9.10 1.55 × 104
600 10.9 1.86 × 104
700 12.7 2.18 × 104
800 14.6 2.49 × 104
900 16.4 2.80 × 104
924 16.8 2.87 × 104
Steel I Beam: W12 × 336 (Wide Flange 12 inch tall × 336 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
336 14.9 1.63 × 104
379 16.8 1.84 × 104
Additional Information