Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Reinforced Plastics

Informed and impartial coverage on the global composites industry.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W12 × 96
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 833 in4) for the W12 × 96 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
  
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 6.90 × 10-6 9.89
100 7.18 × 10-6 10.3
200 1.44 × 10-5 20.6
300 2.15 × 10-5 30.9
400 2.87 × 10-5 41.2
500 3.59 × 10-5 51.5
600 4.31 × 10-5 61.8
700 5.03 × 10-5 72.1
800 5.75 × 10-5 82.4
900 6.46 × 10-5 92.7
1000 7.18 × 10-5 103
2000 1.44 × 10-4 206
3000 2.15 × 10-4 309
4000 2.87 × 10-4 412
5000 3.59 × 10-4 515
6000 4.31 × 10-4 618
7000 5.03 × 10-4 721
8000 5.75 × 10-4 824
9000 6.46 × 10-4 927
1.00 × 104 7.18 × 10-4 1030
2.00 × 104 0.00144 2060
3.00 × 104 0.00215 3090
4.00 × 104 0.00287 4120
5.00 × 104 0.00359 5150
6.00 × 104 0.00431 6180
7.00 × 104 0.00503 7210
8.00 × 104 0.00575 8240
9.00 × 104 0.00646 9270
1.00 × 105 0.00718 1.03 × 104
2.00 × 105 0.0144 2.06 × 104
3.00 × 105 0.0215 3.09 × 104
4.00 × 105 0.0287 4.12 × 104
5.00 × 105 0.0359 5.15 × 104
6.00 × 105 0.0431 6.18 × 104
7.00 × 105 0.0503 7.21 × 104
8.00 × 105 0.0575 8.24 × 104
9.00 × 105 0.0646 9.27 × 104
1.00 × 106 0.0718 1.03 × 105
2.00 × 106 0.144 2.06 × 105
2.88 × 106 0.207 2.97 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 5.32 × 10-5 27.5
100 5.54 × 10-5 28.6
200 1.11 × 10-4 57.2
300 1.66 × 10-4 85.8
400 2.22 × 10-4 114
500 2.77 × 10-4 143
600 3.33 × 10-4 172
700 3.88 × 10-4 200
800 4.43 × 10-4 229
900 4.99 × 10-4 257
1000 5.54 × 10-4 286
2000 0.00111 572
3000 0.00166 858
4000 0.00222 1140
5000 0.00277 1430
6000 0.00333 1720
7000 0.00388 2000
8000 0.00443 2290
9000 0.00499 2570
1.00 × 104 0.00554 2860
2.00 × 104 0.0111 5720
3.00 × 104 0.0166 8580
4.00 × 104 0.0222 1.14 × 104
5.00 × 104 0.0277 1.43 × 104
6.00 × 104 0.0333 1.72 × 104
7.00 × 104 0.0388 2.00 × 104
8.00 × 104 0.0443 2.29 × 104
9.00 × 104 0.0499 2.57 × 104
1.00 × 105 0.0554 2.86 × 104
2.00 × 105 0.111 5.72 × 104
3.00 × 105 0.166 8.58 × 104
4.00 × 105 0.222 1.14 × 105
5.00 × 105 0.277 1.43 × 105
6.00 × 105 0.333 1.72 × 105
7.00 × 105 0.388 2.00 × 105
8.00 × 105 0.443 2.29 × 105
9.00 × 105 0.499 2.57 × 105
1.00 × 106 0.554 2.86 × 105
1.04 × 106 0.575 2.97 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 8.51 × 10-4 110
100 8.87 × 10-4 114
200 0.00177 229
300 0.00266 343
400 0.00355 458
500 0.00443 572
600 0.00532 687
700 0.00621 801
800 0.00709 915
900 0.00798 1030
1000 0.00887 1140
2000 0.0177 2290
3000 0.0266 3430
4000 0.0355 4580
5000 0.0443 5720
6000 0.0532 6870
7000 0.0621 8010
8000 0.0709 9150
9000 0.0798 1.03 × 104
1.00 × 104 0.0887 1.14 × 104
2.00 × 104 0.177 2.29 × 104
3.00 × 104 0.266 3.43 × 104
4.00 × 104 0.355 4.58 × 104
5.00 × 104 0.443 5.72 × 104
6.00 × 104 0.532 6.87 × 104
7.00 × 104 0.621 8.01 × 104
8.00 × 104 0.709 9.15 × 104
9.00 × 104 0.798 1.03 × 105
1.00 × 105 0.887 1.14 × 105
2.00 × 105 1.77 2.29 × 105
2.60 × 105 2.30 2.97 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.00431 247
100 0.00449 257
200 0.00898 515
300 0.0135 772
400 0.0180 1030
500 0.0224 1290
600 0.0269 1540
700 0.0314 1800
800 0.0359 2060
900 0.0404 2320
1000 0.0449 2570
2000 0.0898 5150
3000 0.135 7720
4000 0.180 1.03 × 104
5000 0.224 1.29 × 104
6000 0.269 1.54 × 104
7000 0.314 1.80 × 104
8000 0.359 2.06 × 104
9000 0.404 2.32 × 104
1.00 × 104 0.449 2.57 × 104
2.00 × 104 0.898 5.15 × 104
3.00 × 104 1.35 7.72 × 104
4.00 × 104 1.80 1.03 × 105
5.00 × 104 2.24 1.29 × 105
6.00 × 104 2.69 1.54 × 105
7.00 × 104 3.14 1.80 × 105
8.00 × 104 3.59 2.06 × 105
9.00 × 104 4.04 2.32 × 105
1.00 × 105 4.49 2.57 × 105
1.15 × 105 5.18 2.97 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.0136 439
100 0.0142 458
200 0.0284 915
300 0.0426 1370
400 0.0568 1830
500 0.0709 2290
600 0.0851 2750
700 0.0993 3200
800 0.114 3660
900 0.128 4120
1000 0.142 4580
2000 0.284 9150
3000 0.426 1.37 × 104
4000 0.568 1.83 × 104
5000 0.709 2.29 × 104
6000 0.851 2.75 × 104
7000 0.993 3.20 × 104
8000 1.14 3.66 × 104
9000 1.28 4.12 × 104
1.00 × 104 1.42 4.58 × 104
2.00 × 104 2.84 9.15 × 104
3.00 × 104 4.26 1.37 × 105
4.00 × 104 5.68 1.83 × 105
5.00 × 104 7.09 2.29 × 105
6.00 × 104 8.51 2.75 × 105
6.49 × 104 9.21 2.97 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.0333 687
100 0.0346 715
200 0.0693 1430
300 0.104 2150
400 0.139 2860
500 0.173 3580
600 0.208 4290
700 0.242 5010
800 0.277 5720
900 0.312 6440
1000 0.346 7150
2000 0.693 1.43 × 104
3000 1.04 2.15 × 104
4000 1.39 2.86 × 104
5000 1.73 3.58 × 104
6000 2.08 4.29 × 104
7000 2.42 5.01 × 104
8000 2.77 5.72 × 104
9000 3.12 6.44 × 104
1.00 × 104 3.46 7.15 × 104
2.00 × 104 6.93 1.43 × 105
3.00 × 104 10.4 2.15 × 105
3.67 × 104 12.7 2.62 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.0690 989
100 0.0718 1030
200 0.144 2060
300 0.215 3090
400 0.287 4120
500 0.359 5150
600 0.431 6180
700 0.503 7210
800 0.575 8240
900 0.646 9270
1000 0.718 1.03 × 104
2000 1.44 2.06 × 104
3000 2.15 3.09 × 104
4000 2.87 4.12 × 104
5000 3.59 5.15 × 104
6000 4.31 6.18 × 104
7000 5.03 7.21 × 104
8000 5.75 8.24 × 104
9000 6.46 9.27 × 104
1.00 × 104 7.18 1.03 × 105
1.77 × 104 12.7 1.82 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.218 1760
100 0.227 1830
200 0.454 3660
300 0.681 5490
400 0.908 7320
500 1.14 9150
600 1.36 1.10 × 104
700 1.59 1.28 × 104
800 1.82 1.46 × 104
900 2.04 1.65 × 104
1000 2.27 1.83 × 104
2000 4.54 3.66 × 104
3000 6.81 5.49 × 104
4000 9.08 7.32 × 104
5000 11.4 9.15 × 104
5600 12.7 1.03 × 105
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 0.532 2750
100 0.554 2860
200 1.11 5720
300 1.66 8580
400 2.22 1.14 × 104
500 2.77 1.43 × 104
600 3.33 1.72 × 104
700 3.88 2.00 × 104
800 4.43 2.29 × 104
900 4.99 2.57 × 104
1000 5.54 2.86 × 104
2000 11.1 5.72 × 104
2290 12.7 6.56 × 104
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 1.10 3950
100 1.15 4120
200 2.30 8240
300 3.45 1.24 × 104
400 4.60 1.65 × 104
500 5.75 2.06 × 104
600 6.90 2.47 × 104
700 8.05 2.88 × 104
800 9.19 3.30 × 104
900 10.3 3.71 × 104
1000 11.5 4.12 × 104
1110 12.7 4.56 × 104
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 2.04 5380
100 2.13 5610
200 4.26 1.12 × 104
300 6.39 1.68 × 104
400 8.52 2.24 × 104
500 10.6 2.80 × 104
597 12.7 3.35 × 104
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 3.49 7030
100 3.63 7320
200 7.26 1.46 × 104
300 10.9 2.20 × 104
350 12.7 2.56 × 104
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 5.59 8900
100 5.82 9270
200 11.6 1.85 × 104
218 12.7 2.02 × 104
Steel I Beam: W12 × 96 (Wide Flange 12 inch tall × 96 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
96.0 8.51 1.10 × 104
100 8.87 1.14 × 104
143 12.7 1.64 × 104