Wind Systems

Towers, turbines, gearboxes; processes for shaping and finishing component parts.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Machine Design

How-to, in-depth technical articles for machine design engineers

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W18 × 106
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1910 in4) for the W18 × 106 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 3.32 × 10-6 7.02
200 6.27 × 10-6 13.2
300 9.40 × 10-6 19.9
400 1.25 × 10-5 26.5
500 1.57 × 10-5 33.1
600 1.88 × 10-5 39.7
700 2.19 × 10-5 46.3
800 2.51 × 10-5 53.0
900 2.82 × 10-5 59.6
1000 3.13 × 10-5 66.2
2000 6.27 × 10-5 132
3000 9.40 × 10-5 199
4000 1.25 × 10-4 265
5000 1.57 × 10-4 331
6000 1.88 × 10-4 397
7000 2.19 × 10-4 463
8000 2.51 × 10-4 530
9000 2.82 × 10-4 596
1.00 × 104 3.13 × 10-4 662
2.00 × 104 6.27 × 10-4 1320
3.00 × 104 9.40 × 10-4 1990
4.00 × 104 0.00125 2650
5.00 × 104 0.00157 3310
6.00 × 104 0.00188 3970
7.00 × 104 0.00219 4630
8.00 × 104 0.00251 5300
9.00 × 104 0.00282 5960
1.00 × 105 0.00313 6620
2.00 × 105 0.00627 1.32 × 104
3.00 × 105 0.00940 1.99 × 104
4.00 × 105 0.0125 2.65 × 104
5.00 × 105 0.0157 3.31 × 104
6.00 × 105 0.0188 3.97 × 104
7.00 × 105 0.0219 4.63 × 104
8.00 × 105 0.0251 5.30 × 104
9.00 × 105 0.0282 5.96 × 104
1.00 × 106 0.0313 6.62 × 104
2.00 × 106 0.0627 1.32 × 105
3.00 × 106 0.0940 1.99 × 105
4.00 × 106 0.125 2.65 × 105
4.49 × 106 0.141 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.56 × 10-5 19.5
200 4.83 × 10-5 36.8
300 7.25 × 10-5 55.2
400 9.67 × 10-5 73.5
500 1.21 × 10-4 91.9
600 1.45 × 10-4 110
700 1.69 × 10-4 129
800 1.93 × 10-4 147
900 2.18 × 10-4 165
1000 2.42 × 10-4 184
2000 4.83 × 10-4 368
3000 7.25 × 10-4 552
4000 9.67 × 10-4 735
5000 0.00121 919
6000 0.00145 1100
7000 0.00169 1290
8000 0.00193 1470
9000 0.00218 1650
1.00 × 104 0.00242 1840
2.00 × 104 0.00483 3680
3.00 × 104 0.00725 5520
4.00 × 104 0.00967 7350
5.00 × 104 0.0121 9190
6.00 × 104 0.0145 1.10 × 104
7.00 × 104 0.0169 1.29 × 104
8.00 × 104 0.0193 1.47 × 104
9.00 × 104 0.0218 1.65 × 104
1.00 × 105 0.0242 1.84 × 104
2.00 × 105 0.0483 3.68 × 104
3.00 × 105 0.0725 5.52 × 104
4.00 × 105 0.0967 7.35 × 104
5.00 × 105 0.121 9.19 × 104
6.00 × 105 0.145 1.10 × 105
7.00 × 105 0.169 1.29 × 105
8.00 × 105 0.193 1.47 × 105
9.00 × 105 0.218 1.65 × 105
1.00 × 106 0.242 1.84 × 105
1.62 × 106 0.391 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 4.10 × 10-4 78.0
200 7.74 × 10-4 147
300 0.00116 221
400 0.00155 294
500 0.00193 368
600 0.00232 441
700 0.00271 515
800 0.00309 588
900 0.00348 662
1000 0.00387 735
2000 0.00774 1470
3000 0.0116 2210
4000 0.0155 2940
5000 0.0193 3680
6000 0.0232 4410
7000 0.0271 5150
8000 0.0309 5880
9000 0.0348 6620
1.00 × 104 0.0387 7350
2.00 × 104 0.0774 1.47 × 104
3.00 × 104 0.116 2.21 × 104
4.00 × 104 0.155 2.94 × 104
5.00 × 104 0.193 3.68 × 104
6.00 × 104 0.232 4.41 × 104
7.00 × 104 0.271 5.15 × 104
8.00 × 104 0.309 5.88 × 104
9.00 × 104 0.348 6.62 × 104
1.00 × 105 0.387 7.35 × 104
2.00 × 105 0.774 1.47 × 105
3.00 × 105 1.16 2.21 × 105
4.00 × 105 1.55 2.94 × 105
4.04 × 105 1.56 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00208 175
200 0.00392 331
300 0.00587 496
400 0.00783 662
500 0.00979 827
600 0.0117 993
700 0.0137 1160
800 0.0157 1320
900 0.0176 1490
1000 0.0196 1650
2000 0.0392 3310
3000 0.0587 4960
4000 0.0783 6620
5000 0.0979 8270
6000 0.117 9930
7000 0.137 1.16 × 104
8000 0.157 1.32 × 104
9000 0.176 1.49 × 104
1.00 × 104 0.196 1.65 × 104
2.00 × 104 0.392 3.31 × 104
3.00 × 104 0.587 4.96 × 104
4.00 × 104 0.783 6.62 × 104
5.00 × 104 0.979 8.27 × 104
6.00 × 104 1.17 9.93 × 104
7.00 × 104 1.37 1.16 × 105
8.00 × 104 1.57 1.32 × 105
9.00 × 104 1.76 1.49 × 105
1.00 × 105 1.96 1.65 × 105
1.79 × 105 3.51 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00656 312
200 0.0124 588
300 0.0186 883
400 0.0248 1180
500 0.0309 1470
600 0.0371 1770
700 0.0433 2060
800 0.0495 2350
900 0.0557 2650
1000 0.0619 2940
2000 0.124 5880
3000 0.186 8830
4000 0.248 1.18 × 104
5000 0.309 1.47 × 104
6000 0.371 1.77 × 104
7000 0.433 2.06 × 104
8000 0.495 2.35 × 104
9000 0.557 2.65 × 104
1.00 × 104 0.619 2.94 × 104
2.00 × 104 1.24 5.88 × 104
3.00 × 104 1.86 8.83 × 104
4.00 × 104 2.48 1.18 × 105
5.00 × 104 3.09 1.47 × 105
6.00 × 104 3.71 1.77 × 105
7.00 × 104 4.33 2.06 × 105
8.00 × 104 4.95 2.35 × 105
9.00 × 104 5.57 2.65 × 105
1.00 × 105 6.19 2.94 × 105
1.01 × 105 6.25 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0160 487
200 0.0302 919
300 0.0453 1380
400 0.0604 1840
500 0.0755 2300
600 0.0906 2760
700 0.106 3220
800 0.121 3680
900 0.136 4140
1000 0.151 4600
2000 0.302 9190
3000 0.453 1.38 × 104
4000 0.604 1.84 × 104
5000 0.755 2.30 × 104
6000 0.906 2.76 × 104
7000 1.06 3.22 × 104
8000 1.21 3.68 × 104
9000 1.36 4.14 × 104
1.00 × 104 1.51 4.60 × 104
2.00 × 104 3.02 9.19 × 104
3.00 × 104 4.53 1.38 × 105
4.00 × 104 6.04 1.84 × 105
5.00 × 104 7.55 2.30 × 105
6.00 × 104 9.06 2.76 × 105
6.46 × 104 9.76 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0332 702
200 0.0627 1320
300 0.0940 1990
400 0.125 2650
500 0.157 3310
600 0.188 3970
700 0.219 4630
800 0.251 5300
900 0.282 5960
1000 0.313 6620
2000 0.627 1.32 × 104
3000 0.940 1.99 × 104
4000 1.25 2.65 × 104
5000 1.57 3.31 × 104
6000 1.88 3.97 × 104
7000 2.19 4.63 × 104
8000 2.51 5.30 × 104
9000 2.82 5.96 × 104
1.00 × 104 3.13 6.62 × 104
2.00 × 104 6.27 1.32 × 105
3.00 × 104 9.40 1.99 × 105
4.00 × 104 12.5 2.65 × 105
4.49 × 104 14.1 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.105 1250
200 0.198 2350
300 0.297 3530
400 0.396 4710
500 0.495 5880
600 0.594 7060
700 0.693 8240
800 0.792 9410
900 0.891 1.06 × 104
1000 0.990 1.18 × 104
2000 1.98 2.35 × 104
3000 2.97 3.53 × 104
4000 3.96 4.71 × 104
5000 4.95 5.88 × 104
6000 5.94 7.06 × 104
7000 6.93 8.24 × 104
8000 7.92 9.41 × 104
9000 8.91 1.06 × 105
1.00 × 104 9.90 1.18 × 105
1.89 × 104 18.7 2.23 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.256 1950
200 0.483 3680
300 0.725 5520
400 0.967 7350
500 1.21 9190
600 1.45 1.10 × 104
700 1.69 1.29 × 104
800 1.93 1.47 × 104
900 2.18 1.65 × 104
1000 2.42 1.84 × 104
2000 4.83 3.68 × 104
3000 7.25 5.52 × 104
4000 9.67 7.35 × 104
5000 12.1 9.19 × 104
6000 14.5 1.10 × 105
7000 16.9 1.29 × 105
7750 18.7 1.42 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.531 2810
200 1.00 5300
300 1.50 7940
400 2.00 1.06 × 104
500 2.51 1.32 × 104
600 3.01 1.59 × 104
700 3.51 1.85 × 104
800 4.01 2.12 × 104
900 4.51 2.38 × 104
1000 5.01 2.65 × 104
2000 10.0 5.30 × 104
3000 15.0 7.94 × 104
3740 18.7 9.89 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.984 3820
200 1.86 7210
300 2.79 1.08 × 104
400 3.71 1.44 × 104
500 4.64 1.80 × 104
600 5.57 2.16 × 104
700 6.50 2.52 × 104
800 7.43 2.88 × 104
900 8.36 3.24 × 104
1000 9.29 3.60 × 104
2000 18.6 7.21 × 104
2020 18.7 7.27 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.68 4990
200 3.17 9410
300 4.75 1.41 × 104
400 6.34 1.88 × 104
500 7.92 2.35 × 104
600 9.51 2.82 × 104
700 11.1 3.29 × 104
800 12.7 3.77 × 104
900 14.3 4.24 × 104
1000 15.8 4.71 × 104
1180 18.7 5.57 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.69 6310
200 5.08 1.19 × 104
300 7.61 1.79 × 104
400 10.2 2.38 × 104
500 12.7 2.98 × 104
600 15.2 3.57 × 104
700 17.8 4.17 × 104
738 18.7 4.40 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 4.10 7800
200 7.74 1.47 × 104
300 11.6 2.21 × 104
400 15.5 2.94 × 104
484 18.7 3.56 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 10.0 1.22 × 104
198 18.7 2.28 × 104
Additional Information