Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W14 × 500
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 8210 in4) for the W14 × 500 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 1.90 × 10-6 6.45
600 2.28 × 10-6 7.73
700 2.66 × 10-6 9.02
800 3.04 × 10-6 10.3
900 3.43 × 10-6 11.6
1000 3.81 × 10-6 12.9
2000 7.61 × 10-6 25.8
3000 1.14 × 10-5 38.7
4000 1.52 × 10-5 51.6
5000 1.90 × 10-5 64.5
6000 2.28 × 10-5 77.3
7000 2.66 × 10-5 90.2
8000 3.04 × 10-5 103
9000 3.43 × 10-5 116
1.00 × 104 3.81 × 10-5 129
2.00 × 104 7.61 × 10-5 258
3.00 × 104 1.14 × 10-4 387
4.00 × 104 1.52 × 10-4 516
5.00 × 104 1.90 × 10-4 645
6.00 × 104 2.28 × 10-4 773
7.00 × 104 2.66 × 10-4 902
8.00 × 104 3.04 × 10-4 1030
9.00 × 104 3.43 × 10-4 1160
1.00 × 105 3.81 × 10-4 1290
2.00 × 105 7.61 × 10-4 2580
3.00 × 105 0.00114 3870
4.00 × 105 0.00152 5160
5.00 × 105 0.00190 6450
6.00 × 105 0.00228 7730
7.00 × 105 0.00266 9020
8.00 × 105 0.00304 1.03 × 104
9.00 × 105 0.00343 1.16 × 104
1.00 × 106 0.00381 1.29 × 104
2.00 × 106 0.00761 2.58 × 104
3.00 × 106 0.0114 3.87 × 104
4.00 × 106 0.0152 5.16 × 104
5.00 × 106 0.0190 6.45 × 104
6.00 × 106 0.0228 7.73 × 104
7.00 × 106 0.0266 9.02 × 104
8.00 × 106 0.0304 1.03 × 105
9.00 × 106 0.0343 1.16 × 105
1.00 × 107 0.0381 1.29 × 105
2.00 × 107 0.0761 2.58 × 105
2.30 × 107 0.0877 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 1.47 × 10-5 17.9
600 1.76 × 10-5 21.5
700 2.06 × 10-5 25.1
800 2.35 × 10-5 28.6
900 2.64 × 10-5 32.2
1000 2.94 × 10-5 35.8
2000 5.87 × 10-5 71.6
3000 8.81 × 10-5 107
4000 1.17 × 10-4 143
5000 1.47 × 10-4 179
6000 1.76 × 10-4 215
7000 2.06 × 10-4 251
8000 2.35 × 10-4 286
9000 2.64 × 10-4 322
1.00 × 104 2.94 × 10-4 358
2.00 × 104 5.87 × 10-4 716
3.00 × 104 8.81 × 10-4 1070
4.00 × 104 0.00117 1430
5.00 × 104 0.00147 1790
6.00 × 104 0.00176 2150
7.00 × 104 0.00206 2510
8.00 × 104 0.00235 2860
9.00 × 104 0.00264 3220
1.00 × 105 0.00294 3580
2.00 × 105 0.00587 7160
3.00 × 105 0.00881 1.07 × 104
4.00 × 105 0.0117 1.43 × 104
5.00 × 105 0.0147 1.79 × 104
6.00 × 105 0.0176 2.15 × 104
7.00 × 105 0.0206 2.51 × 104
8.00 × 105 0.0235 2.86 × 104
9.00 × 105 0.0264 3.22 × 104
1.00 × 106 0.0294 3.58 × 104
2.00 × 106 0.0587 7.16 × 104
3.00 × 106 0.0881 1.07 × 105
4.00 × 106 0.117 1.43 × 105
5.00 × 106 0.147 1.79 × 105
6.00 × 106 0.176 2.15 × 105
7.00 × 106 0.206 2.51 × 105
8.00 × 106 0.235 2.86 × 105
8.29 × 106 0.244 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 2.35 × 10-4 71.6
600 2.82 × 10-4 85.9
700 3.29 × 10-4 100
800 3.76 × 10-4 115
900 4.23 × 10-4 129
1000 4.70 × 10-4 143
2000 9.40 × 10-4 286
3000 0.00141 430
4000 0.00188 573
5000 0.00235 716
6000 0.00282 859
7000 0.00329 1000
8000 0.00376 1150
9000 0.00423 1290
1.00 × 104 0.00470 1430
2.00 × 104 0.00940 2860
3.00 × 104 0.0141 4300
4.00 × 104 0.0188 5730
5.00 × 104 0.0235 7160
6.00 × 104 0.0282 8590
7.00 × 104 0.0329 1.00 × 104
8.00 × 104 0.0376 1.15 × 104
9.00 × 104 0.0423 1.29 × 104
1.00 × 105 0.0470 1.43 × 104
2.00 × 105 0.0940 2.86 × 104
3.00 × 105 0.141 4.30 × 104
4.00 × 105 0.188 5.73 × 104
5.00 × 105 0.235 7.16 × 104
6.00 × 105 0.282 8.59 × 104
7.00 × 105 0.329 1.00 × 105
8.00 × 105 0.376 1.15 × 105
9.00 × 105 0.423 1.29 × 105
1.00 × 106 0.470 1.43 × 105
2.00 × 106 0.940 2.86 × 105
2.07 × 106 0.974 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.00119 161
600 0.00143 193
700 0.00167 226
800 0.00190 258
900 0.00214 290
1000 0.00238 322
2000 0.00476 645
3000 0.00714 967
4000 0.00952 1290
5000 0.0119 1610
6000 0.0143 1930
7000 0.0167 2260
8000 0.0190 2580
9000 0.0214 2900
1.00 × 104 0.0238 3220
2.00 × 104 0.0476 6450
3.00 × 104 0.0714 9670
4.00 × 104 0.0952 1.29 × 104
5.00 × 104 0.119 1.61 × 104
6.00 × 104 0.143 1.93 × 104
7.00 × 104 0.167 2.26 × 104
8.00 × 104 0.190 2.58 × 104
9.00 × 104 0.214 2.90 × 104
1.00 × 105 0.238 3.22 × 104
2.00 × 105 0.476 6.45 × 104
3.00 × 105 0.714 9.67 × 104
4.00 × 105 0.952 1.29 × 105
5.00 × 105 1.19 1.61 × 105
6.00 × 105 1.43 1.93 × 105
7.00 × 105 1.67 2.26 × 105
8.00 × 105 1.90 2.58 × 105
9.00 × 105 2.14 2.90 × 105
9.22 × 105 2.19 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.00376 286
600 0.00451 344
700 0.00526 401
800 0.00601 458
900 0.00677 516
1000 0.00752 573
2000 0.0150 1150
3000 0.0226 1720
4000 0.0301 2290
5000 0.0376 2860
6000 0.0451 3440
7000 0.0526 4010
8000 0.0601 4580
9000 0.0677 5160
1.00 × 104 0.0752 5730
2.00 × 104 0.150 1.15 × 104
3.00 × 104 0.226 1.72 × 104
4.00 × 104 0.301 2.29 × 104
5.00 × 104 0.376 2.86 × 104
6.00 × 104 0.451 3.44 × 104
7.00 × 104 0.526 4.01 × 104
8.00 × 104 0.601 4.58 × 104
9.00 × 104 0.677 5.16 × 104
1.00 × 105 0.752 5.73 × 104
2.00 × 105 1.50 1.15 × 105
3.00 × 105 2.26 1.72 × 105
4.00 × 105 3.01 2.29 × 105
5.00 × 105 3.76 2.86 × 105
5.18 × 105 3.90 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.00918 448
600 0.0110 537
700 0.0128 627
800 0.0147 716
900 0.0165 806
1000 0.0184 895
2000 0.0367 1790
3000 0.0551 2690
4000 0.0734 3580
5000 0.0918 4480
6000 0.110 5370
7000 0.128 6270
8000 0.147 7160
9000 0.165 8060
1.00 × 104 0.184 8950
2.00 × 104 0.367 1.79 × 104
3.00 × 104 0.551 2.69 × 104
4.00 × 104 0.734 3.58 × 104
5.00 × 104 0.918 4.48 × 104
6.00 × 104 1.10 5.37 × 104
7.00 × 104 1.28 6.27 × 104
8.00 × 104 1.47 7.16 × 104
9.00 × 104 1.65 8.06 × 104
1.00 × 105 1.84 8.95 × 104
2.00 × 105 3.67 1.79 × 105
3.00 × 105 5.51 2.69 × 105
3.32 × 105 6.09 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.0190 645
600 0.0228 773
700 0.0266 902
800 0.0304 1030
900 0.0343 1160
1000 0.0381 1290
2000 0.0761 2580
3000 0.114 3870
4000 0.152 5160
5000 0.190 6450
6000 0.228 7730
7000 0.266 9020
8000 0.304 1.03 × 104
9000 0.343 1.16 × 104
1.00 × 104 0.381 1.29 × 104
2.00 × 104 0.761 2.58 × 104
3.00 × 104 1.14 3.87 × 104
4.00 × 104 1.52 5.16 × 104
5.00 × 104 1.90 6.45 × 104
6.00 × 104 2.28 7.73 × 104
7.00 × 104 2.66 9.02 × 104
8.00 × 104 3.04 1.03 × 105
9.00 × 104 3.43 1.16 × 105
1.00 × 105 3.81 1.29 × 105
2.00 × 105 7.61 2.58 × 105
2.30 × 105 8.77 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.0601 1150
600 0.0722 1380
700 0.0842 1600
800 0.0962 1830
900 0.108 2060
1000 0.120 2290
2000 0.241 4580
3000 0.361 6880
4000 0.481 9170
5000 0.601 1.15 × 104
6000 0.722 1.38 × 104
7000 0.842 1.60 × 104
8000 0.962 1.83 × 104
9000 1.08 2.06 × 104
1.00 × 104 1.20 2.29 × 104
2.00 × 104 2.41 4.58 × 104
3.00 × 104 3.61 6.88 × 104
4.00 × 104 4.81 9.17 × 104
5.00 × 104 6.01 1.15 × 105
6.00 × 104 7.22 1.38 × 105
7.00 × 104 8.42 1.60 × 105
8.00 × 104 9.62 1.83 × 105
9.00 × 104 10.8 2.06 × 105
1.00 × 105 12.0 2.29 × 105
1.30 × 105 15.6 2.97 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.147 1790
600 0.176 2150
700 0.206 2510
800 0.235 2860
900 0.264 3220
1000 0.294 3580
2000 0.587 7160
3000 0.881 1.07 × 104
4000 1.17 1.43 × 104
5000 1.47 1.79 × 104
6000 1.76 2.15 × 104
7000 2.06 2.51 × 104
8000 2.35 2.86 × 104
9000 2.64 3.22 × 104
1.00 × 104 2.94 3.58 × 104
2.00 × 104 5.87 7.16 × 104
3.00 × 104 8.81 1.07 × 105
4.00 × 104 11.7 1.43 × 105
5.00 × 104 14.7 1.79 × 105
6.00 × 104 17.6 2.15 × 105
6.67 × 104 19.6 2.39 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.304 2580
600 0.365 3090
700 0.426 3610
800 0.487 4130
900 0.548 4640
1000 0.609 5160
2000 1.22 1.03 × 104
3000 1.83 1.55 × 104
4000 2.44 2.06 × 104
5000 3.04 2.58 × 104
6000 3.65 3.09 × 104
7000 4.26 3.61 × 104
8000 4.87 4.13 × 104
9000 5.48 4.64 × 104
1.00 × 104 6.09 5.16 × 104
2.00 × 104 12.2 1.03 × 105
3.00 × 104 18.3 1.55 × 105
3.22 × 104 19.6 1.66 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.564 3510
600 0.677 4210
700 0.790 4910
800 0.903 5620
900 1.02 6320
1000 1.13 7020
2000 2.26 1.40 × 104
3000 3.38 2.11 × 104
4000 4.51 2.81 × 104
5000 5.64 3.51 × 104
6000 6.77 4.21 × 104
7000 7.90 4.91 × 104
8000 9.03 5.62 × 104
9000 10.2 6.32 × 104
1.00 × 104 11.3 7.02 × 104
1.74 × 104 19.6 1.22 × 105
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 0.962 4580
600 1.15 5500
700 1.35 6420
800 1.54 7330
900 1.73 8250
1000 1.92 9170
2000 3.85 1.83 × 104
3000 5.77 2.75 × 104
4000 7.70 3.67 × 104
5000 9.62 4.58 × 104
6000 11.5 5.50 × 104
7000 13.5 6.42 × 104
8000 15.4 7.33 × 104
9000 17.3 8.25 × 104
1.00 × 104 19.2 9.17 × 104
1.02 × 104 19.6 9.34 × 104
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 1.54 5800
600 1.85 6960
700 2.16 8120
800 2.47 9280
900 2.77 1.04 × 104
1000 3.08 1.16 × 104
2000 6.17 2.32 × 104
3000 9.25 3.48 × 104
4000 12.3 4.64 × 104
5000 15.4 5.80 × 104
6000 18.5 6.96 × 104
6360 19.6 7.38 × 104
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 2.35 7160
600 2.82 8590
700 3.29 1.00 × 104
800 3.76 1.15 × 104
900 4.23 1.29 × 104
1000 4.70 1.43 × 104
2000 9.40 2.86 × 104
3000 14.1 4.30 × 104
4000 18.8 5.73 × 104
4170 19.6 5.97 × 104
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 5.74 1.12 × 104
600 6.88 1.34 × 104
700 8.03 1.57 × 104
800 9.18 1.79 × 104
900 10.3 2.01 × 104
1000 11.5 2.24 × 104
1710 19.6 3.82 × 104
Steel I Beam: W14 × 500 (Wide Flange 14 inch tall × 500 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
500 11.9 1.61 × 104
600 14.3 1.93 × 104
700 16.7 2.26 × 104
800 19.0 2.58 × 104
824 19.6 2.66 × 104
Additional Information
Related Pages
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.