Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

World Pumps

Major news, innovation and real-life applications for pumps and ancillary equipment.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W16 × 89
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1300 in4) for the W16 × 89 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 2.14 × 10-6 6.19
90.0 2.16 × 10-6 6.26
100 2.40 × 10-6 6.96
200 4.81 × 10-6 13.9
300 7.21 × 10-6 20.9
400 9.62 × 10-6 27.8
500 1.20 × 10-5 34.8
600 1.44 × 10-5 41.7
700 1.68 × 10-5 48.7
800 1.92 × 10-5 55.7
900 2.16 × 10-5 62.6
1000 2.40 × 10-5 69.6
2000 4.81 × 10-5 139
3000 7.21 × 10-5 209
4000 9.62 × 10-5 278
5000 1.20 × 10-4 348
6000 1.44 × 10-4 417
7000 1.68 × 10-4 487
8000 1.92 × 10-4 557
9000 2.16 × 10-4 626
1.00 × 104 2.40 × 10-4 696
2.00 × 104 4.81 × 10-4 1390
3.00 × 104 7.21 × 10-4 2090
4.00 × 104 9.62 × 10-4 2780
5.00 × 104 0.00120 3480
6.00 × 104 0.00144 4170
7.00 × 104 0.00168 4870
8.00 × 104 0.00192 5570
9.00 × 104 0.00216 6260
1.00 × 105 0.00240 6960
2.00 × 105 0.00481 1.39 × 104
3.00 × 105 0.00721 2.09 × 104
4.00 × 105 0.00962 2.78 × 104
5.00 × 105 0.0120 3.48 × 104
6.00 × 105 0.0144 4.17 × 104
7.00 × 105 0.0168 4.87 × 104
8.00 × 105 0.0192 5.57 × 104
9.00 × 105 0.0216 6.26 × 104
1.00 × 106 0.0240 6.96 × 104
2.00 × 106 0.0481 1.39 × 105
3.00 × 106 0.0721 2.09 × 105
4.00 × 106 0.0962 2.78 × 105
4.27 × 106 0.103 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.65 × 10-5 17.2
90.0 1.67 × 10-5 17.4
100 1.85 × 10-5 19.3
200 3.71 × 10-5 38.7
300 5.56 × 10-5 58.0
400 7.42 × 10-5 77.3
500 9.27 × 10-5 96.6
600 1.11 × 10-4 116
700 1.30 × 10-4 135
800 1.48 × 10-4 155
900 1.67 × 10-4 174
1000 1.85 × 10-4 193
2000 3.71 × 10-4 387
3000 5.56 × 10-4 580
4000 7.42 × 10-4 773
5000 9.27 × 10-4 966
6000 0.00111 1160
7000 0.00130 1350
8000 0.00148 1550
9000 0.00167 1740
1.00 × 104 0.00185 1930
2.00 × 104 0.00371 3870
3.00 × 104 0.00556 5800
4.00 × 104 0.00742 7730
5.00 × 104 0.00927 9660
6.00 × 104 0.0111 1.16 × 104
7.00 × 104 0.0130 1.35 × 104
8.00 × 104 0.0148 1.55 × 104
9.00 × 104 0.0167 1.74 × 104
1.00 × 105 0.0185 1.93 × 104
2.00 × 105 0.0371 3.87 × 104
3.00 × 105 0.0556 5.80 × 104
4.00 × 105 0.0742 7.73 × 104
5.00 × 105 0.0927 9.66 × 104
6.00 × 105 0.111 1.16 × 105
7.00 × 105 0.130 1.35 × 105
8.00 × 105 0.148 1.55 × 105
9.00 × 105 0.167 1.74 × 105
1.00 × 106 0.185 1.93 × 105
1.54 × 106 0.285 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 2.64 × 10-4 68.8
90.0 2.67 × 10-4 69.6
100 2.97 × 10-4 77.3
200 5.94 × 10-4 155
300 8.90 × 10-4 232
400 0.00119 309
500 0.00148 387
600 0.00178 464
700 0.00208 541
800 0.00237 618
900 0.00267 696
1000 0.00297 773
2000 0.00594 1550
3000 0.00890 2320
4000 0.0119 3090
5000 0.0148 3870
6000 0.0178 4640
7000 0.0208 5410
8000 0.0237 6180
9000 0.0267 6960
1.00 × 104 0.0297 7730
2.00 × 104 0.0594 1.55 × 104
3.00 × 104 0.0890 2.32 × 104
4.00 × 104 0.119 3.09 × 104
5.00 × 104 0.148 3.87 × 104
6.00 × 104 0.178 4.64 × 104
7.00 × 104 0.208 5.41 × 104
8.00 × 104 0.237 6.18 × 104
9.00 × 104 0.267 6.96 × 104
1.00 × 105 0.297 7.73 × 104
2.00 × 105 0.594 1.55 × 105
3.00 × 105 0.890 2.32 × 105
3.84 × 105 1.14 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.00134 155
90.0 0.00135 157
100 0.00150 174
200 0.00300 348
300 0.00451 522
400 0.00601 696
500 0.00751 870
600 0.00901 1040
700 0.0105 1220
800 0.0120 1390
900 0.0135 1570
1000 0.0150 1740
2000 0.0300 3480
3000 0.0451 5220
4000 0.0601 6960
5000 0.0751 8700
6000 0.0901 1.04 × 104
7000 0.105 1.22 × 104
8000 0.120 1.39 × 104
9000 0.135 1.57 × 104
1.00 × 104 0.150 1.74 × 104
2.00 × 104 0.300 3.48 × 104
3.00 × 104 0.451 5.22 × 104
4.00 × 104 0.601 6.96 × 104
5.00 × 104 0.751 8.70 × 104
6.00 × 104 0.901 1.04 × 105
7.00 × 104 1.05 1.22 × 105
8.00 × 104 1.20 1.39 × 105
9.00 × 104 1.35 1.57 × 105
1.00 × 105 1.50 1.74 × 105
1.71 × 105 2.57 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.00423 275
90.0 0.00427 278
100 0.00475 309
200 0.00950 618
300 0.0142 928
400 0.0190 1240
500 0.0237 1550
600 0.0285 1860
700 0.0332 2160
800 0.0380 2470
900 0.0427 2780
1000 0.0475 3090
2000 0.0950 6180
3000 0.142 9280
4000 0.190 1.24 × 104
5000 0.237 1.55 × 104
6000 0.285 1.86 × 104
7000 0.332 2.16 × 104
8000 0.380 2.47 × 104
9000 0.427 2.78 × 104
1.00 × 104 0.475 3.09 × 104
2.00 × 104 0.950 6.18 × 104
3.00 × 104 1.42 9.28 × 104
4.00 × 104 1.90 1.24 × 105
5.00 × 104 2.37 1.55 × 105
6.00 × 104 2.85 1.86 × 105
7.00 × 104 3.32 2.16 × 105
8.00 × 104 3.80 2.47 × 105
9.00 × 104 4.27 2.78 × 105
9.61 × 104 4.56 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.0103 430
90.0 0.0104 435
100 0.0116 483
200 0.0232 966
300 0.0348 1450
400 0.0464 1930
500 0.0580 2420
600 0.0696 2900
700 0.0811 3380
800 0.0927 3870
900 0.104 4350
1000 0.116 4830
2000 0.232 9660
3000 0.348 1.45 × 104
4000 0.464 1.93 × 104
5000 0.580 2.42 × 104
6000 0.696 2.90 × 104
7000 0.811 3.38 × 104
8000 0.927 3.87 × 104
9000 1.04 4.35 × 104
1.00 × 104 1.16 4.83 × 104
2.00 × 104 2.32 9.66 × 104
3.00 × 104 3.48 1.45 × 105
4.00 × 104 4.64 1.93 × 105
5.00 × 104 5.80 2.42 × 105
6.00 × 104 6.96 2.90 × 105
6.15 × 104 7.13 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.0214 619
90.0 0.0216 626
100 0.0240 696
200 0.0481 1390
300 0.0721 2090
400 0.0962 2780
500 0.120 3480
600 0.144 4170
700 0.168 4870
800 0.192 5570
900 0.216 6260
1000 0.240 6960
2000 0.481 1.39 × 104
3000 0.721 2.09 × 104
4000 0.962 2.78 × 104
5000 1.20 3.48 × 104
6000 1.44 4.17 × 104
7000 1.68 4.87 × 104
8000 1.92 5.57 × 104
9000 2.16 6.26 × 104
1.00 × 104 2.40 6.96 × 104
2.00 × 104 4.81 1.39 × 105
3.00 × 104 7.21 2.09 × 105
4.00 × 104 9.62 2.78 × 105
4.27 × 104 10.3 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.0676 1100
90.0 0.0684 1110
100 0.0760 1240
200 0.152 2470
300 0.228 3710
400 0.304 4950
500 0.380 6180
600 0.456 7420
700 0.532 8660
800 0.608 9900
900 0.684 1.11 × 104
1000 0.760 1.24 × 104
2000 1.52 2.47 × 104
3000 2.28 3.71 × 104
4000 3.04 4.95 × 104
5000 3.80 6.18 × 104
6000 4.56 7.42 × 104
7000 5.32 8.66 × 104
8000 6.08 9.90 × 104
9000 6.84 1.11 × 105
1.00 × 104 7.60 1.24 × 105
2.00 × 104 15.2 2.47 × 105
2.40 × 104 18.2 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.165 1720
90.0 0.167 1740
100 0.185 1930
200 0.371 3870
300 0.556 5800
400 0.742 7730
500 0.927 9660
600 1.11 1.16 × 104
700 1.30 1.35 × 104
800 1.48 1.55 × 104
900 1.67 1.74 × 104
1000 1.85 1.93 × 104
2000 3.71 3.87 × 104
3000 5.56 5.80 × 104
4000 7.42 7.73 × 104
5000 9.27 9.66 × 104
6000 11.1 1.16 × 105
7000 13.0 1.35 × 105
8000 14.8 1.55 × 105
9000 16.7 1.74 × 105
9030 16.8 1.75 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.342 2480
90.0 0.346 2500
100 0.385 2780
200 0.769 5570
300 1.15 8350
400 1.54 1.11 × 104
500 1.92 1.39 × 104
600 2.31 1.67 × 104
700 2.69 1.95 × 104
800 3.08 2.23 × 104
900 3.46 2.50 × 104
1000 3.85 2.78 × 104
2000 7.69 5.57 × 104
3000 11.5 8.35 × 104
4000 15.4 1.11 × 105
4360 16.8 1.21 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.634 3370
90.0 0.641 3410
100 0.713 3790
200 1.43 7580
300 2.14 1.14 × 104
400 2.85 1.52 × 104
500 3.56 1.89 × 104
600 4.28 2.27 × 104
700 4.99 2.65 × 104
800 5.70 3.03 × 104
900 6.41 3.41 × 104
1000 7.13 3.79 × 104
2000 14.3 7.58 × 104
2350 16.8 8.90 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.08 4400
90.0 1.09 4450
100 1.22 4950
200 2.43 9900
300 3.65 1.48 × 104
400 4.86 1.98 × 104
500 6.08 2.47 × 104
600 7.29 2.97 × 104
700 8.51 3.46 × 104
800 9.72 3.96 × 104
900 10.9 4.45 × 104
1000 12.2 4.95 × 104
1380 16.8 6.82 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.73 5570
90.0 1.75 5640
100 1.95 6260
200 3.89 1.25 × 104
300 5.84 1.88 × 104
400 7.79 2.50 × 104
500 9.74 3.13 × 104
600 11.7 3.76 × 104
700 13.6 4.38 × 104
800 15.6 5.01 × 104
860 16.8 5.39 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 2.64 6880
90.0 2.67 6960
100 2.97 7730
200 5.94 1.55 × 104
300 8.90 2.32 × 104
400 11.9 3.09 × 104
500 14.8 3.87 × 104
564 16.8 4.36 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 6.45 1.08 × 104
90.0 6.52 1.09 × 104
100 7.25 1.21 × 104
200 14.5 2.42 × 104
231 16.8 2.79 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 13.4 1.55 × 104
90.0 13.5 1.57 × 104
100 15.0 1.74 × 104
111 16.8 1.94 × 104