3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W24 × 131
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 4020 in4) for the W24 × 131 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
L = 200 ft
  
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 1.02 × 10-6 4.31
200 1.55 × 10-6 6.58
300 2.33 × 10-6 9.87
400 3.11 × 10-6 13.2
500 3.89 × 10-6 16.4
600 4.66 × 10-6 19.7
700 5.44 × 10-6 23.0
800 6.22 × 10-6 26.3
900 7.00 × 10-6 29.6
1000 7.77 × 10-6 32.9
2000 1.55 × 10-5 65.8
3000 2.33 × 10-5 98.7
4000 3.11 × 10-5 132
5000 3.89 × 10-5 164
6000 4.66 × 10-5 197
7000 5.44 × 10-5 230
8000 6.22 × 10-5 263
9000 7.00 × 10-5 296
1.00 × 104 7.77 × 10-5 329
2.00 × 104 1.55 × 10-4 658
3.00 × 104 2.33 × 10-4 987
4.00 × 104 3.11 × 10-4 1320
5.00 × 104 3.89 × 10-4 1640
6.00 × 104 4.66 × 10-4 1970
7.00 × 104 5.44 × 10-4 2300
8.00 × 104 6.22 × 10-4 2630
9.00 × 104 7.00 × 10-4 2960
1.00 × 105 7.77 × 10-4 3290
2.00 × 105 0.00155 6580
3.00 × 105 0.00233 9870
4.00 × 105 0.00311 1.32 × 104
5.00 × 105 0.00389 1.64 × 104
6.00 × 105 0.00466 1.97 × 104
7.00 × 105 0.00544 2.30 × 104
8.00 × 105 0.00622 2.63 × 104
9.00 × 105 0.00700 2.96 × 104
1.00 × 106 0.00777 3.29 × 104
2.00 × 106 0.0155 6.58 × 104
3.00 × 106 0.0233 9.87 × 104
4.00 × 106 0.0311 1.32 × 105
5.00 × 106 0.0389 1.64 × 105
6.00 × 106 0.0466 1.97 × 105
7.00 × 106 0.0544 2.30 × 105
8.00 × 106 0.0622 2.63 × 105
9.00 × 106 0.0700 2.96 × 105
9.03 × 106 0.0702 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 7.86 × 10-6 12.0
200 1.20 × 10-5 18.3
300 1.80 × 10-5 27.4
400 2.40 × 10-5 36.5
500 3.00 × 10-5 45.7
600 3.60 × 10-5 54.8
700 4.20 × 10-5 63.9
800 4.80 × 10-5 73.1
900 5.40 × 10-5 82.2
1000 6.00 × 10-5 91.3
2000 1.20 × 10-4 183
3000 1.80 × 10-4 274
4000 2.40 × 10-4 365
5000 3.00 × 10-4 457
6000 3.60 × 10-4 548
7000 4.20 × 10-4 639
8000 4.80 × 10-4 731
9000 5.40 × 10-4 822
1.00 × 104 6.00 × 10-4 913
2.00 × 104 0.00120 1830
3.00 × 104 0.00180 2740
4.00 × 104 0.00240 3650
5.00 × 104 0.00300 4570
6.00 × 104 0.00360 5480
7.00 × 104 0.00420 6390
8.00 × 104 0.00480 7310
9.00 × 104 0.00540 8220
1.00 × 105 0.00600 9130
2.00 × 105 0.0120 1.83 × 104
3.00 × 105 0.0180 2.74 × 104
4.00 × 105 0.0240 3.65 × 104
5.00 × 105 0.0300 4.57 × 104
6.00 × 105 0.0360 5.48 × 104
7.00 × 105 0.0420 6.39 × 104
8.00 × 105 0.0480 7.31 × 104
9.00 × 105 0.0540 8.22 × 104
1.00 × 106 0.0600 9.13 × 104
2.00 × 106 0.120 1.83 × 105
3.00 × 106 0.180 2.74 × 105
3.25 × 106 0.195 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 1.26 × 10-4 47.9
200 1.92 × 10-4 73.1
300 2.88 × 10-4 110
400 3.84 × 10-4 146
500 4.80 × 10-4 183
600 5.76 × 10-4 219
700 6.72 × 10-4 256
800 7.68 × 10-4 292
900 8.64 × 10-4 329
1000 9.60 × 10-4 365
2000 0.00192 731
3000 0.00288 1100
4000 0.00384 1460
5000 0.00480 1830
6000 0.00576 2190
7000 0.00672 2560
8000 0.00768 2920
9000 0.00864 3290
1.00 × 104 0.00960 3650
2.00 × 104 0.0192 7310
3.00 × 104 0.0288 1.10 × 104
4.00 × 104 0.0384 1.46 × 104
5.00 × 104 0.0480 1.83 × 104
6.00 × 104 0.0576 2.19 × 104
7.00 × 104 0.0672 2.56 × 104
8.00 × 104 0.0768 2.92 × 104
9.00 × 104 0.0864 3.29 × 104
1.00 × 105 0.0960 3.65 × 104
2.00 × 105 0.192 7.31 × 104
3.00 × 105 0.288 1.10 × 105
4.00 × 105 0.384 1.46 × 105
5.00 × 105 0.480 1.83 × 105
6.00 × 105 0.576 2.19 × 105
7.00 × 105 0.672 2.56 × 105
8.00 × 105 0.768 2.92 × 105
8.13 × 105 0.780 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 6.36 × 10-4 108
200 9.72 × 10-4 164
300 0.00146 247
400 0.00194 329
500 0.00243 411
600 0.00292 493
700 0.00340 575
800 0.00389 658
900 0.00437 740
1000 0.00486 822
2000 0.00972 1640
3000 0.0146 2470
4000 0.0194 3290
5000 0.0243 4110
6000 0.0292 4930
7000 0.0340 5750
8000 0.0389 6580
9000 0.0437 7400
1.00 × 104 0.0486 8220
2.00 × 104 0.0972 1.64 × 104
3.00 × 104 0.146 2.47 × 104
4.00 × 104 0.194 3.29 × 104
5.00 × 104 0.243 4.11 × 104
6.00 × 104 0.292 4.93 × 104
7.00 × 104 0.340 5.75 × 104
8.00 × 104 0.389 6.58 × 104
9.00 × 104 0.437 7.40 × 104
1.00 × 105 0.486 8.22 × 104
2.00 × 105 0.972 1.64 × 105
3.00 × 105 1.46 2.47 × 105
3.61 × 105 1.76 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.00201 191
200 0.00307 292
300 0.00461 438
400 0.00614 585
500 0.00768 731
600 0.00921 877
700 0.0107 1020
800 0.0123 1170
900 0.0138 1320
1000 0.0154 1460
2000 0.0307 2920
3000 0.0461 4380
4000 0.0614 5850
5000 0.0768 7310
6000 0.0921 8770
7000 0.107 1.02 × 104
8000 0.123 1.17 × 104
9000 0.138 1.32 × 104
1.00 × 104 0.154 1.46 × 104
2.00 × 104 0.307 2.92 × 104
3.00 × 104 0.461 4.38 × 104
4.00 × 104 0.614 5.85 × 104
5.00 × 104 0.768 7.31 × 104
6.00 × 104 0.921 8.77 × 104
7.00 × 104 1.07 1.02 × 105
8.00 × 104 1.23 1.17 × 105
9.00 × 104 1.38 1.32 × 105
1.00 × 105 1.54 1.46 × 105
2.00 × 105 3.07 2.92 × 105
2.03 × 105 3.12 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.00491 299
200 0.00750 457
300 0.0112 685
400 0.0150 913
500 0.0187 1140
600 0.0225 1370
700 0.0262 1600
800 0.0300 1830
900 0.0337 2060
1000 0.0375 2280
2000 0.0750 4570
3000 0.112 6850
4000 0.150 9130
5000 0.187 1.14 × 104
6000 0.225 1.37 × 104
7000 0.262 1.60 × 104
8000 0.300 1.83 × 104
9000 0.337 2.06 × 104
1.00 × 104 0.375 2.28 × 104
2.00 × 104 0.750 4.57 × 104
3.00 × 104 1.12 6.85 × 104
4.00 × 104 1.50 9.13 × 104
5.00 × 104 1.87 1.14 × 105
6.00 × 104 2.25 1.37 × 105
7.00 × 104 2.62 1.60 × 105
8.00 × 104 3.00 1.83 × 105
9.00 × 104 3.37 2.06 × 105
1.00 × 105 3.75 2.28 × 105
1.30 × 105 4.88 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.0102 431
200 0.0155 658
300 0.0233 987
400 0.0311 1320
500 0.0389 1640
600 0.0466 1970
700 0.0544 2300
800 0.0622 2630
900 0.0700 2960
1000 0.0777 3290
2000 0.155 6580
3000 0.233 9870
4000 0.311 1.32 × 104
5000 0.389 1.64 × 104
6000 0.466 1.97 × 104
7000 0.544 2.30 × 104
8000 0.622 2.63 × 104
9000 0.700 2.96 × 104
1.00 × 104 0.777 3.29 × 104
2.00 × 104 1.55 6.58 × 104
3.00 × 104 2.33 9.87 × 104
4.00 × 104 3.11 1.32 × 105
5.00 × 104 3.89 1.64 × 105
6.00 × 104 4.66 1.97 × 105
7.00 × 104 5.44 2.30 × 105
8.00 × 104 6.22 2.63 × 105
9.00 × 104 7.00 2.96 × 105
9.03 × 104 7.02 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.0322 766
200 0.0491 1170
300 0.0737 1750
400 0.0983 2340
500 0.123 2920
600 0.147 3510
700 0.172 4090
800 0.197 4680
900 0.221 5260
1000 0.246 5850
2000 0.491 1.17 × 104
3000 0.737 1.75 × 104
4000 0.983 2.34 × 104
5000 1.23 2.92 × 104
6000 1.47 3.51 × 104
7000 1.72 4.09 × 104
8000 1.97 4.68 × 104
9000 2.21 5.26 × 104
1.00 × 104 2.46 5.85 × 104
2.00 × 104 4.91 1.17 × 105
3.00 × 104 7.37 1.75 × 105
4.00 × 104 9.83 2.34 × 105
5.00 × 104 12.3 2.92 × 105
5.08 × 104 12.5 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.0786 1200
200 0.120 1830
300 0.180 2740
400 0.240 3650
500 0.300 4570
600 0.360 5480
700 0.420 6390
800 0.480 7310
900 0.540 8220
1000 0.600 9130
2000 1.20 1.83 × 104
3000 1.80 2.74 × 104
4000 2.40 3.65 × 104
5000 3.00 4.57 × 104
6000 3.60 5.48 × 104
7000 4.20 6.39 × 104
8000 4.80 7.31 × 104
9000 5.40 8.22 × 104
1.00 × 104 6.00 9.13 × 104
2.00 × 104 12.0 1.83 × 105
3.00 × 104 18.0 2.74 × 105
3.25 × 104 19.5 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.163 1720
200 0.249 2630
300 0.373 3950
400 0.497 5260
500 0.622 6580
600 0.746 7890
700 0.871 9210
800 0.995 1.05 × 104
900 1.12 1.18 × 104
1000 1.24 1.32 × 104
2000 2.49 2.63 × 104
3000 3.73 3.95 × 104
4000 4.97 5.26 × 104
5000 6.22 6.58 × 104
6000 7.46 7.89 × 104
7000 8.71 9.21 × 104
8000 9.95 1.05 × 105
9000 11.2 1.18 × 105
1.00 × 104 12.4 1.32 × 105
1.97 × 104 24.5 2.59 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.302 2350
200 0.461 3580
300 0.691 5370
400 0.922 7160
500 1.15 8950
600 1.38 1.07 × 104
700 1.61 1.25 × 104
800 1.84 1.43 × 104
900 2.07 1.61 × 104
1000 2.30 1.79 × 104
2000 4.61 3.58 × 104
3000 6.91 5.37 × 104
4000 9.22 7.16 × 104
5000 11.5 8.95 × 104
6000 13.8 1.07 × 105
7000 16.1 1.25 × 105
8000 18.4 1.43 × 105
9000 20.7 1.61 × 105
1.00 × 104 23.0 1.79 × 105
1.66 × 104 38.2 2.97 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.515 3060
200 0.786 4680
300 1.18 7020
400 1.57 9350
500 1.97 1.17 × 104
600 2.36 1.40 × 104
700 2.75 1.64 × 104
800 3.14 1.87 × 104
900 3.54 2.10 × 104
1000 3.93 2.34 × 104
2000 7.86 4.68 × 104
3000 11.8 7.02 × 104
4000 15.7 9.35 × 104
5000 19.7 1.17 × 105
6000 23.6 1.40 × 105
6230 24.5 1.46 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 0.825 3880
200 1.26 5920
300 1.89 8880
400 2.52 1.18 × 104
500 3.15 1.48 × 104
600 3.78 1.78 × 104
700 4.41 2.07 × 104
800 5.04 2.37 × 104
900 5.67 2.66 × 104
1000 6.30 2.96 × 104
2000 12.6 5.92 × 104
3000 18.9 8.88 × 104
3890 24.5 1.15 × 105
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 1.26 4790
200 1.92 7310
300 2.88 1.10 × 104
400 3.84 1.46 × 104
500 4.80 1.83 × 104
600 5.76 2.19 × 104
700 6.72 2.56 × 104
800 7.68 2.92 × 104
900 8.64 3.29 × 104
1000 9.60 3.65 × 104
2000 19.2 7.31 × 104
2550 24.5 9.32 × 104
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 3.07 7480
200 4.69 1.14 × 104
300 7.03 1.71 × 104
400 9.37 2.28 × 104
500 11.7 2.85 × 104
600 14.1 3.43 × 104
700 16.4 4.00 × 104
800 18.7 4.57 × 104
900 21.1 5.14 × 104
1000 23.4 5.71 × 104
1040 24.5 5.96 × 104
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 6.36 1.08 × 104
200 9.72 1.64 × 104
300 14.6 2.47 × 104
400 19.4 3.29 × 104
500 24.3 4.11 × 104
504 24.5 4.14 × 104
Steel I Beam: W24 × 131 (Wide Flange 24 inch tall × 131 lbf/ft)
L = 200 ft
P (lbf/ft) w_max (in) stress_max (psi)
131 20.1 1.91 × 104
159 24.5 2.33 × 104