Chemical Engineering

The industry gateway for chemical engineering and plant operations.

Laser Focus World

Semiconductors, medical equipment, lasers, optics and aviation and aerospace.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W16 × 89
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1300 in4) for the W16 × 89 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.64 × 10-6 7.74
90.0 1.66 × 10-6 7.83
100 1.84 × 10-6 8.70
200 3.68 × 10-6 17.4
300 5.52 × 10-6 26.1
400 7.36 × 10-6 34.8
500 9.21 × 10-6 43.5
600 1.10 × 10-5 52.2
700 1.29 × 10-5 60.9
800 1.47 × 10-5 69.6
900 1.66 × 10-5 78.3
1000 1.84 × 10-5 87.0
2000 3.68 × 10-5 174
3000 5.52 × 10-5 261
4000 7.36 × 10-5 348
5000 9.21 × 10-5 435
6000 1.10 × 10-4 522
7000 1.29 × 10-4 609
8000 1.47 × 10-4 696
9000 1.66 × 10-4 783
1.00 × 104 1.84 × 10-4 870
2.00 × 104 3.68 × 10-4 1740
3.00 × 104 5.52 × 10-4 2610
4.00 × 104 7.36 × 10-4 3480
5.00 × 104 9.21 × 10-4 4350
6.00 × 104 0.00110 5220
7.00 × 104 0.00129 6090
8.00 × 104 0.00147 6960
9.00 × 104 0.00166 7830
1.00 × 105 0.00184 8700
2.00 × 105 0.00368 1.74 × 104
3.00 × 105 0.00552 2.61 × 104
4.00 × 105 0.00736 3.48 × 104
5.00 × 105 0.00921 4.35 × 104
6.00 × 105 0.0110 5.22 × 104
7.00 × 105 0.0129 6.09 × 104
8.00 × 105 0.0147 6.96 × 104
9.00 × 105 0.0166 7.83 × 104
1.00 × 106 0.0184 8.70 × 104
2.00 × 106 0.0368 1.74 × 105
3.00 × 106 0.0552 2.61 × 105
3.42 × 106 0.0629 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.26 × 10-5 21.5
90.0 1.28 × 10-5 21.7
100 1.42 × 10-5 24.2
200 2.84 × 10-5 48.3
300 4.26 × 10-5 72.5
400 5.68 × 10-5 96.6
500 7.10 × 10-5 121
600 8.52 × 10-5 145
700 9.94 × 10-5 169
800 1.14 × 10-4 193
900 1.28 × 10-4 217
1000 1.42 × 10-4 242
2000 2.84 × 10-4 483
3000 4.26 × 10-4 725
4000 5.68 × 10-4 966
5000 7.10 × 10-4 1210
6000 8.52 × 10-4 1450
7000 9.94 × 10-4 1690
8000 0.00114 1930
9000 0.00128 2170
1.00 × 104 0.00142 2420
2.00 × 104 0.00284 4830
3.00 × 104 0.00426 7250
4.00 × 104 0.00568 9660
5.00 × 104 0.00710 1.21 × 104
6.00 × 104 0.00852 1.45 × 104
7.00 × 104 0.00994 1.69 × 104
8.00 × 104 0.0114 1.93 × 104
9.00 × 104 0.0128 2.17 × 104
1.00 × 105 0.0142 2.42 × 104
2.00 × 105 0.0284 4.83 × 104
3.00 × 105 0.0426 7.25 × 104
4.00 × 105 0.0568 9.66 × 104
5.00 × 105 0.0710 1.21 × 105
6.00 × 105 0.0852 1.45 × 105
7.00 × 105 0.0994 1.69 × 105
8.00 × 105 0.114 1.93 × 105
9.00 × 105 0.128 2.17 × 105
1.00 × 106 0.142 2.42 × 105
1.23 × 106 0.175 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 2.02 × 10-4 86.0
90.0 2.05 × 10-4 87.0
100 2.27 × 10-4 96.6
200 4.55 × 10-4 193
300 6.82 × 10-4 290
400 9.09 × 10-4 387
500 0.00114 483
600 0.00136 580
700 0.00159 676
800 0.00182 773
900 0.00205 870
1000 0.00227 966
2000 0.00455 1930
3000 0.00682 2900
4000 0.00909 3870
5000 0.0114 4830
6000 0.0136 5800
7000 0.0159 6760
8000 0.0182 7730
9000 0.0205 8700
1.00 × 104 0.0227 9660
2.00 × 104 0.0455 1.93 × 104
3.00 × 104 0.0682 2.90 × 104
4.00 × 104 0.0909 3.87 × 104
5.00 × 104 0.114 4.83 × 104
6.00 × 104 0.136 5.80 × 104
7.00 × 104 0.159 6.76 × 104
8.00 × 104 0.182 7.73 × 104
9.00 × 104 0.205 8.70 × 104
1.00 × 105 0.227 9.66 × 104
2.00 × 105 0.455 1.93 × 105
3.00 × 105 0.682 2.90 × 105
3.07 × 105 0.699 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.00102 194
90.0 0.00104 196
100 0.00115 217
200 0.00230 435
300 0.00345 652
400 0.00460 870
500 0.00575 1090
600 0.00690 1300
700 0.00805 1520
800 0.00921 1740
900 0.0104 1960
1000 0.0115 2170
2000 0.0230 4350
3000 0.0345 6520
4000 0.0460 8700
5000 0.0575 1.09 × 104
6000 0.0690 1.30 × 104
7000 0.0805 1.52 × 104
8000 0.0921 1.74 × 104
9000 0.104 1.96 × 104
1.00 × 104 0.115 2.17 × 104
2.00 × 104 0.230 4.35 × 104
3.00 × 104 0.345 6.52 × 104
4.00 × 104 0.460 8.70 × 104
5.00 × 104 0.575 1.09 × 105
6.00 × 104 0.690 1.30 × 105
7.00 × 104 0.805 1.52 × 105
8.00 × 104 0.921 1.74 × 105
9.00 × 104 1.04 1.96 × 105
1.00 × 105 1.15 2.17 × 105
1.37 × 105 1.57 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.00324 344
90.0 0.00327 348
100 0.00364 387
200 0.00727 773
300 0.0109 1160
400 0.0145 1550
500 0.0182 1930
600 0.0218 2320
700 0.0255 2710
800 0.0291 3090
900 0.0327 3480
1000 0.0364 3870
2000 0.0727 7730
3000 0.109 1.16 × 104
4000 0.145 1.55 × 104
5000 0.182 1.93 × 104
6000 0.218 2.32 × 104
7000 0.255 2.71 × 104
8000 0.291 3.09 × 104
9000 0.327 3.48 × 104
1.00 × 104 0.364 3.87 × 104
2.00 × 104 0.727 7.73 × 104
3.00 × 104 1.09 1.16 × 105
4.00 × 104 1.45 1.55 × 105
5.00 × 104 1.82 1.93 × 105
6.00 × 104 2.18 2.32 × 105
7.00 × 104 2.55 2.71 × 105
7.68 × 104 2.79 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.00790 538
90.0 0.00799 544
100 0.00888 604
200 0.0178 1210
300 0.0266 1810
400 0.0355 2420
500 0.0444 3020
600 0.0533 3620
700 0.0622 4230
800 0.0710 4830
900 0.0799 5440
1000 0.0888 6040
2000 0.178 1.21 × 104
3000 0.266 1.81 × 104
4000 0.355 2.42 × 104
5000 0.444 3.02 × 104
6000 0.533 3.62 × 104
7000 0.622 4.23 × 104
8000 0.710 4.83 × 104
9000 0.799 5.44 × 104
1.00 × 104 0.888 6.04 × 104
2.00 × 104 1.78 1.21 × 105
3.00 × 104 2.66 1.81 × 105
4.00 × 104 3.55 2.42 × 105
4.92 × 104 4.37 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.0164 774
90.0 0.0166 783
100 0.0184 870
200 0.0368 1740
300 0.0552 2610
400 0.0736 3480
500 0.0921 4350
600 0.110 5220
700 0.129 6090
800 0.147 6960
900 0.166 7830
1000 0.184 8700
2000 0.368 1.74 × 104
3000 0.552 2.61 × 104
4000 0.736 3.48 × 104
5000 0.921 4.35 × 104
6000 1.10 5.22 × 104
7000 1.29 6.09 × 104
8000 1.47 6.96 × 104
9000 1.66 7.83 × 104
1.00 × 104 1.84 8.70 × 104
2.00 × 104 3.68 1.74 × 105
3.00 × 104 5.52 2.61 × 105
3.42 × 104 6.29 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.0518 1380
90.0 0.0524 1390
100 0.0582 1550
200 0.116 3090
300 0.175 4640
400 0.233 6180
500 0.291 7730
600 0.349 9280
700 0.407 1.08 × 104
800 0.466 1.24 × 104
900 0.524 1.39 × 104
1000 0.582 1.55 × 104
2000 1.16 3.09 × 104
3000 1.75 4.64 × 104
4000 2.33 6.18 × 104
5000 2.91 7.73 × 104
6000 3.49 9.28 × 104
7000 4.07 1.08 × 105
8000 4.66 1.24 × 105
9000 5.24 1.39 × 105
1.00 × 104 5.82 1.55 × 105
1.92 × 104 11.2 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.126 2150
90.0 0.128 2170
100 0.142 2420
200 0.284 4830
300 0.426 7250
400 0.568 9660
500 0.710 1.21 × 104
600 0.852 1.45 × 104
700 0.994 1.69 × 104
800 1.14 1.93 × 104
900 1.28 2.17 × 104
1000 1.42 2.42 × 104
2000 2.84 4.83 × 104
3000 4.26 7.25 × 104
4000 5.68 9.66 × 104
5000 7.10 1.21 × 105
6000 8.52 1.45 × 105
7000 9.94 1.69 × 105
8000 11.4 1.93 × 105
9000 12.8 2.17 × 105
1.00 × 104 14.2 2.42 × 105
1.23 × 104 17.5 2.97 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.262 3100
90.0 0.265 3130
100 0.295 3480
200 0.589 6960
300 0.884 1.04 × 104
400 1.18 1.39 × 104
500 1.47 1.74 × 104
600 1.77 2.09 × 104
700 2.06 2.44 × 104
800 2.36 2.78 × 104
900 2.65 3.13 × 104
1000 2.95 3.48 × 104
2000 5.89 6.96 × 104
3000 8.84 1.04 × 105
4000 11.8 1.39 × 105
5000 14.7 1.74 × 105
5690 16.8 1.98 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.486 4210
90.0 0.491 4260
100 0.546 4740
200 1.09 9470
300 1.64 1.42 × 104
400 2.18 1.89 × 104
500 2.73 2.37 × 104
600 3.27 2.84 × 104
700 3.82 3.31 × 104
800 4.37 3.79 × 104
900 4.91 4.26 × 104
1000 5.46 4.74 × 104
2000 10.9 9.47 × 104
3000 16.4 1.42 × 105
3070 16.8 1.45 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 0.829 5500
90.0 0.838 5570
100 0.931 6180
200 1.86 1.24 × 104
300 2.79 1.86 × 104
400 3.72 2.47 × 104
500 4.66 3.09 × 104
600 5.59 3.71 × 104
700 6.52 4.33 × 104
800 7.45 4.95 × 104
900 8.38 5.57 × 104
1000 9.31 6.18 × 104
1800 16.8 1.11 × 105
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 1.33 6970
90.0 1.34 7040
100 1.49 7830
200 2.98 1.57 × 104
300 4.47 2.35 × 104
400 5.97 3.13 × 104
500 7.46 3.91 × 104
600 8.95 4.70 × 104
700 10.4 5.48 × 104
800 11.9 6.26 × 104
900 13.4 7.04 × 104
1000 14.9 7.83 × 104
1120 16.8 8.79 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 2.02 8600
90.0 2.05 8700
100 2.27 9660
200 4.55 1.93 × 104
300 6.82 2.90 × 104
400 9.09 3.87 × 104
500 11.4 4.83 × 104
600 13.6 5.80 × 104
700 15.9 6.76 × 104
737 16.8 7.12 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 4.94 1.34 × 104
90.0 4.99 1.36 × 104
100 5.55 1.51 × 104
200 11.1 3.02 × 104
300 16.6 4.53 × 104
302 16.8 4.56 × 104
Steel I Beam: W16 × 89 (Wide Flange 16 inch tall × 89 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
89.0 10.2 1.94 × 104
90.0 10.4 1.96 × 104
100 11.5 2.17 × 104
146 16.8 3.16 × 104