3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Chemical Engineering

The industry gateway for chemical engineering and plant operations.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W18 × 50
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 800 in4) for the W18 × 50 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 1.50 × 10-6 7.59
60.0 1.80 × 10-6 9.11
70.0 2.09 × 10-6 10.6
80.0 2.39 × 10-6 12.1
90.0 2.69 × 10-6 13.7
100 2.99 × 10-6 15.2
200 5.98 × 10-6 30.4
300 8.98 × 10-6 45.5
400 1.20 × 10-5 60.7
500 1.50 × 10-5 75.9
600 1.80 × 10-5 91.1
700 2.09 × 10-5 106
800 2.39 × 10-5 121
900 2.69 × 10-5 137
1000 2.99 × 10-5 152
2000 5.98 × 10-5 304
3000 8.98 × 10-5 455
4000 1.20 × 10-4 607
5000 1.50 × 10-4 759
6000 1.80 × 10-4 911
7000 2.09 × 10-4 1060
8000 2.39 × 10-4 1210
9000 2.69 × 10-4 1370
1.00 × 104 2.99 × 10-4 1520
2.00 × 104 5.98 × 10-4 3040
3.00 × 104 8.98 × 10-4 4550
4.00 × 104 0.00120 6070
5.00 × 104 0.00150 7590
6.00 × 104 0.00180 9110
7.00 × 104 0.00209 1.06 × 104
8.00 × 104 0.00239 1.21 × 104
9.00 × 104 0.00269 1.37 × 104
1.00 × 105 0.00299 1.52 × 104
2.00 × 105 0.00598 3.04 × 104
3.00 × 105 0.00898 4.55 × 104
4.00 × 105 0.0120 6.07 × 104
5.00 × 105 0.0150 7.59 × 104
6.00 × 105 0.0180 9.11 × 104
7.00 × 105 0.0209 1.06 × 105
8.00 × 105 0.0239 1.21 × 105
9.00 × 105 0.0269 1.37 × 105
1.00 × 106 0.0299 1.52 × 105
1.96 × 106 0.0585 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 1.15 × 10-5 21.1
60.0 1.39 × 10-5 25.3
70.0 1.62 × 10-5 29.5
80.0 1.85 × 10-5 33.7
90.0 2.08 × 10-5 37.9
100 2.31 × 10-5 42.2
200 4.62 × 10-5 84.3
300 6.93 × 10-5 126
400 9.23 × 10-5 169
500 1.15 × 10-4 211
600 1.39 × 10-4 253
700 1.62 × 10-4 295
800 1.85 × 10-4 337
900 2.08 × 10-4 379
1000 2.31 × 10-4 422
2000 4.62 × 10-4 843
3000 6.93 × 10-4 1260
4000 9.23 × 10-4 1690
5000 0.00115 2110
6000 0.00139 2530
7000 0.00162 2950
8000 0.00185 3370
9000 0.00208 3790
1.00 × 104 0.00231 4220
2.00 × 104 0.00462 8430
3.00 × 104 0.00693 1.26 × 104
4.00 × 104 0.00923 1.69 × 104
5.00 × 104 0.0115 2.11 × 104
6.00 × 104 0.0139 2.53 × 104
7.00 × 104 0.0162 2.95 × 104
8.00 × 104 0.0185 3.37 × 104
9.00 × 104 0.0208 3.79 × 104
1.00 × 105 0.0231 4.22 × 104
2.00 × 105 0.0462 8.43 × 104
3.00 × 105 0.0693 1.26 × 105
4.00 × 105 0.0923 1.69 × 105
5.00 × 105 0.115 2.11 × 105
6.00 × 105 0.139 2.53 × 105
7.00 × 105 0.162 2.95 × 105
7.04 × 105 0.163 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 1.85 × 10-4 84.3
60.0 2.22 × 10-4 101
70.0 2.59 × 10-4 118
80.0 2.95 × 10-4 135
90.0 3.32 × 10-4 152
100 3.69 × 10-4 169
200 7.39 × 10-4 337
300 0.00111 506
400 0.00148 675
500 0.00185 843
600 0.00222 1010
700 0.00259 1180
800 0.00295 1350
900 0.00332 1520
1000 0.00369 1690
2000 0.00739 3370
3000 0.0111 5060
4000 0.0148 6750
5000 0.0185 8430
6000 0.0222 1.01 × 104
7000 0.0259 1.18 × 104
8000 0.0295 1.35 × 104
9000 0.0332 1.52 × 104
1.00 × 104 0.0369 1.69 × 104
2.00 × 104 0.0739 3.37 × 104
3.00 × 104 0.111 5.06 × 104
4.00 × 104 0.148 6.75 × 104
5.00 × 104 0.185 8.43 × 104
6.00 × 104 0.222 1.01 × 105
7.00 × 104 0.259 1.18 × 105
8.00 × 104 0.295 1.35 × 105
9.00 × 104 0.332 1.52 × 105
1.00 × 105 0.369 1.69 × 105
1.76 × 105 0.651 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 9.35 × 10-4 190
60.0 0.00112 228
70.0 0.00131 266
80.0 0.00150 304
90.0 0.00168 342
100 0.00187 379
200 0.00374 759
300 0.00561 1140
400 0.00748 1520
500 0.00935 1900
600 0.0112 2280
700 0.0131 2660
800 0.0150 3040
900 0.0168 3420
1000 0.0187 3790
2000 0.0374 7590
3000 0.0561 1.14 × 104
4000 0.0748 1.52 × 104
5000 0.0935 1.90 × 104
6000 0.112 2.28 × 104
7000 0.131 2.66 × 104
8000 0.150 3.04 × 104
9000 0.168 3.42 × 104
1.00 × 104 0.187 3.79 × 104
2.00 × 104 0.374 7.59 × 104
3.00 × 104 0.561 1.14 × 105
4.00 × 104 0.748 1.52 × 105
5.00 × 104 0.935 1.90 × 105
6.00 × 104 1.12 2.28 × 105
7.00 × 104 1.31 2.66 × 105
7.83 × 104 1.46 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.00295 337
60.0 0.00355 405
70.0 0.00414 472
80.0 0.00473 540
90.0 0.00532 607
100 0.00591 675
200 0.0118 1350
300 0.0177 2020
400 0.0236 2700
500 0.0295 3370
600 0.0355 4050
700 0.0414 4720
800 0.0473 5400
900 0.0532 6070
1000 0.0591 6750
2000 0.118 1.35 × 104
3000 0.177 2.02 × 104
4000 0.236 2.70 × 104
5000 0.295 3.37 × 104
6000 0.355 4.05 × 104
7000 0.414 4.72 × 104
8000 0.473 5.40 × 104
9000 0.532 6.07 × 104
1.00 × 104 0.591 6.75 × 104
2.00 × 104 1.18 1.35 × 105
3.00 × 104 1.77 2.02 × 105
4.00 × 104 2.36 2.70 × 105
4.40 × 104 2.60 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.00721 527
60.0 0.00866 632
70.0 0.0101 738
80.0 0.0115 843
90.0 0.0130 949
100 0.0144 1050
200 0.0289 2110
300 0.0433 3160
400 0.0577 4220
500 0.0721 5270
600 0.0866 6320
700 0.101 7380
800 0.115 8430
900 0.130 9490
1000 0.144 1.05 × 104
2000 0.289 2.11 × 104
3000 0.433 3.16 × 104
4000 0.577 4.22 × 104
5000 0.721 5.27 × 104
6000 0.866 6.32 × 104
7000 1.01 7.38 × 104
8000 1.15 8.43 × 104
9000 1.30 9.49 × 104
1.00 × 104 1.44 1.05 × 105
2.00 × 104 2.89 2.11 × 105
2.82 × 104 4.07 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.0150 759
60.0 0.0180 911
70.0 0.0209 1060
80.0 0.0239 1210
90.0 0.0269 1370
100 0.0299 1520
200 0.0598 3040
300 0.0898 4550
400 0.120 6070
500 0.150 7590
600 0.180 9110
700 0.209 1.06 × 104
800 0.239 1.21 × 104
900 0.269 1.37 × 104
1000 0.299 1.52 × 104
2000 0.598 3.04 × 104
3000 0.898 4.55 × 104
4000 1.20 6.07 × 104
5000 1.50 7.59 × 104
6000 1.80 9.11 × 104
7000 2.09 1.06 × 105
8000 2.39 1.21 × 105
9000 2.69 1.37 × 105
1.00 × 104 2.99 1.52 × 105
1.96 × 104 5.85 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.0473 1350
60.0 0.0567 1620
70.0 0.0662 1890
80.0 0.0756 2160
90.0 0.0851 2430
100 0.0946 2700
200 0.189 5400
300 0.284 8100
400 0.378 1.08 × 104
500 0.473 1.35 × 104
600 0.567 1.62 × 104
700 0.662 1.89 × 104
800 0.756 2.16 × 104
900 0.851 2.43 × 104
1000 0.946 2.70 × 104
2000 1.89 5.40 × 104
3000 2.84 8.10 × 104
4000 3.78 1.08 × 105
5000 4.73 1.35 × 105
6000 5.67 1.62 × 105
7000 6.62 1.89 × 105
8000 7.56 2.16 × 105
9000 8.51 2.43 × 105
1.00 × 104 9.46 2.70 × 105
1.10 × 104 10.4 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.115 2110
60.0 0.139 2530
70.0 0.162 2950
80.0 0.185 3370
90.0 0.208 3790
100 0.231 4220
200 0.462 8430
300 0.693 1.26 × 104
400 0.923 1.69 × 104
500 1.15 2.11 × 104
600 1.39 2.53 × 104
700 1.62 2.95 × 104
800 1.85 3.37 × 104
900 2.08 3.79 × 104
1000 2.31 4.22 × 104
2000 4.62 8.43 × 104
3000 6.93 1.26 × 105
4000 9.23 1.69 × 105
5000 11.5 2.11 × 105
6000 13.9 2.53 × 105
7000 16.2 2.95 × 105
7040 16.3 2.97 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.239 3040
60.0 0.287 3640
70.0 0.335 4250
80.0 0.383 4860
90.0 0.431 5460
100 0.479 6070
200 0.957 1.21 × 104
300 1.44 1.82 × 104
400 1.91 2.43 × 104
500 2.39 3.04 × 104
600 2.87 3.64 × 104
700 3.35 4.25 × 104
800 3.83 4.86 × 104
900 4.31 5.46 × 104
1000 4.79 6.07 × 104
2000 9.57 1.21 × 105
3000 14.4 1.82 × 105
3760 18.0 2.28 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.443 4130
60.0 0.532 4960
70.0 0.621 5780
80.0 0.709 6610
90.0 0.798 7440
100 0.887 8260
200 1.77 1.65 × 104
300 2.66 2.48 × 104
400 3.55 3.31 × 104
500 4.43 4.13 × 104
600 5.32 4.96 × 104
700 6.21 5.78 × 104
800 7.09 6.61 × 104
900 7.98 7.44 × 104
1000 8.87 8.26 × 104
2000 17.7 1.65 × 105
2030 18.0 1.68 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 0.756 5400
60.0 0.908 6480
70.0 1.06 7560
80.0 1.21 8640
90.0 1.36 9710
100 1.51 1.08 × 104
200 3.03 2.16 × 104
300 4.54 3.24 × 104
400 6.05 4.32 × 104
500 7.56 5.40 × 104
600 9.08 6.48 × 104
700 10.6 7.56 × 104
800 12.1 8.64 × 104
900 13.6 9.71 × 104
1000 15.1 1.08 × 105
1190 18.0 1.28 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 1.21 6830
60.0 1.45 8200
70.0 1.70 9560
80.0 1.94 1.09 × 104
90.0 2.18 1.23 × 104
100 2.42 1.37 × 104
200 4.85 2.73 × 104
300 7.27 4.10 × 104
400 9.69 5.46 × 104
500 12.1 6.83 × 104
600 14.5 8.20 × 104
700 17.0 9.56 × 104
742 18.0 1.01 × 105
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 1.85 8430
60.0 2.22 1.01 × 104
70.0 2.59 1.18 × 104
80.0 2.95 1.35 × 104
90.0 3.32 1.52 × 104
100 3.69 1.69 × 104
200 7.39 3.37 × 104
300 11.1 5.06 × 104
400 14.8 6.75 × 104
487 18.0 8.21 × 104
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 4.51 1.32 × 104
60.0 5.41 1.58 × 104
70.0 6.31 1.84 × 104
80.0 7.21 2.11 × 104
90.0 8.12 2.37 × 104
100 9.02 2.64 × 104
199 18.0 5.26 × 104
Steel I Beam: W18 × 50 (Wide Flange 18 inch tall × 50 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
50.0 9.35 1.90 × 104
60.0 11.2 2.28 × 104
70.0 13.1 2.66 × 104
80.0 15.0 3.04 × 104
90.0 16.8 3.42 × 104
96.2 18.0 3.65 × 104
Additional Information