Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W24 × 94
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 2700 in4) for the W24 × 94 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
L = 200 ft
  
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 8.33 × 10-7 5.71
100 8.86 × 10-7 6.08
200 1.77 × 10-6 12.2
300 2.66 × 10-6 18.2
400 3.55 × 10-6 24.3
500 4.43 × 10-6 30.4
600 5.32 × 10-6 36.5
700 6.21 × 10-6 42.5
800 7.09 × 10-6 48.6
900 7.98 × 10-6 54.7
1000 8.86 × 10-6 60.8
2000 1.77 × 10-5 122
3000 2.66 × 10-5 182
4000 3.55 × 10-5 243
5000 4.43 × 10-5 304
6000 5.32 × 10-5 365
7000 6.21 × 10-5 425
8000 7.09 × 10-5 486
9000 7.98 × 10-5 547
1.00 × 104 8.86 × 10-5 608
2.00 × 104 1.77 × 10-4 1220
3.00 × 104 2.66 × 10-4 1820
4.00 × 104 3.55 × 10-4 2430
5.00 × 104 4.43 × 10-4 3040
6.00 × 104 5.32 × 10-4 3650
7.00 × 104 6.21 × 10-4 4250
8.00 × 104 7.09 × 10-4 4860
9.00 × 104 7.98 × 10-4 5470
1.00 × 105 8.86 × 10-4 6080
2.00 × 105 0.00177 1.22 × 104
3.00 × 105 0.00266 1.82 × 104
4.00 × 105 0.00355 2.43 × 104
5.00 × 105 0.00443 3.04 × 104
6.00 × 105 0.00532 3.65 × 104
7.00 × 105 0.00621 4.25 × 104
8.00 × 105 0.00709 4.86 × 104
9.00 × 105 0.00798 5.47 × 104
1.00 × 106 0.00886 6.08 × 104
2.00 × 106 0.0177 1.22 × 105
3.00 × 106 0.0266 1.82 × 105
4.00 × 106 0.0355 2.43 × 105
4.89 × 106 0.0433 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 6.43 × 10-6 15.9
100 6.84 × 10-6 16.9
200 1.37 × 10-5 33.8
300 2.05 × 10-5 50.6
400 2.74 × 10-5 67.5
500 3.42 × 10-5 84.4
600 4.10 × 10-5 101
700 4.79 × 10-5 118
800 5.47 × 10-5 135
900 6.16 × 10-5 152
1000 6.84 × 10-5 169
2000 1.37 × 10-4 338
3000 2.05 × 10-4 506
4000 2.74 × 10-4 675
5000 3.42 × 10-4 844
6000 4.10 × 10-4 1010
7000 4.79 × 10-4 1180
8000 5.47 × 10-4 1350
9000 6.16 × 10-4 1520
1.00 × 104 6.84 × 10-4 1690
2.00 × 104 0.00137 3380
3.00 × 104 0.00205 5060
4.00 × 104 0.00274 6750
5.00 × 104 0.00342 8440
6.00 × 104 0.00410 1.01 × 104
7.00 × 104 0.00479 1.18 × 104
8.00 × 104 0.00547 1.35 × 104
9.00 × 104 0.00616 1.52 × 104
1.00 × 105 0.00684 1.69 × 104
2.00 × 105 0.0137 3.38 × 104
3.00 × 105 0.0205 5.06 × 104
4.00 × 105 0.0274 6.75 × 104
5.00 × 105 0.0342 8.44 × 104
6.00 × 105 0.0410 1.01 × 105
7.00 × 105 0.0479 1.18 × 105
8.00 × 105 0.0547 1.35 × 105
9.00 × 105 0.0616 1.52 × 105
1.00 × 106 0.0684 1.69 × 105
1.76 × 106 0.120 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 1.03 × 10-4 63.5
100 1.09 × 10-4 67.5
200 2.19 × 10-4 135
300 3.28 × 10-4 203
400 4.38 × 10-4 270
500 5.47 × 10-4 338
600 6.57 × 10-4 405
700 7.66 × 10-4 473
800 8.76 × 10-4 540
900 9.85 × 10-4 608
1000 0.00109 675
2000 0.00219 1350
3000 0.00328 2030
4000 0.00438 2700
5000 0.00547 3380
6000 0.00657 4050
7000 0.00766 4730
8000 0.00876 5400
9000 0.00985 6080
1.00 × 104 0.0109 6750
2.00 × 104 0.0219 1.35 × 104
3.00 × 104 0.0328 2.03 × 104
4.00 × 104 0.0438 2.70 × 104
5.00 × 104 0.0547 3.38 × 104
6.00 × 104 0.0657 4.05 × 104
7.00 × 104 0.0766 4.73 × 104
8.00 × 104 0.0876 5.40 × 104
9.00 × 104 0.0985 6.08 × 104
1.00 × 105 0.109 6.75 × 104
2.00 × 105 0.219 1.35 × 105
3.00 × 105 0.328 2.03 × 105
4.00 × 105 0.438 2.70 × 105
4.40 × 105 0.481 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 5.21 × 10-4 143
100 5.54 × 10-4 152
200 0.00111 304
300 0.00166 456
400 0.00222 608
500 0.00277 760
600 0.00332 912
700 0.00388 1060
800 0.00443 1220
900 0.00499 1370
1000 0.00554 1520
2000 0.0111 3040
3000 0.0166 4560
4000 0.0222 6080
5000 0.0277 7600
6000 0.0332 9120
7000 0.0388 1.06 × 104
8000 0.0443 1.22 × 104
9000 0.0499 1.37 × 104
1.00 × 104 0.0554 1.52 × 104
2.00 × 104 0.111 3.04 × 104
3.00 × 104 0.166 4.56 × 104
4.00 × 104 0.222 6.08 × 104
5.00 × 104 0.277 7.60 × 104
6.00 × 104 0.332 9.12 × 104
7.00 × 104 0.388 1.06 × 105
8.00 × 104 0.443 1.22 × 105
9.00 × 104 0.499 1.37 × 105
1.00 × 105 0.554 1.52 × 105
1.96 × 105 1.08 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.00165 254
100 0.00175 270
200 0.00350 540
300 0.00525 810
400 0.00700 1080
500 0.00876 1350
600 0.0105 1620
700 0.0123 1890
800 0.0140 2160
900 0.0158 2430
1000 0.0175 2700
2000 0.0350 5400
3000 0.0525 8100
4000 0.0700 1.08 × 104
5000 0.0876 1.35 × 104
6000 0.105 1.62 × 104
7000 0.123 1.89 × 104
8000 0.140 2.16 × 104
9000 0.158 2.43 × 104
1.00 × 104 0.175 2.70 × 104
2.00 × 104 0.350 5.40 × 104
3.00 × 104 0.525 8.10 × 104
4.00 × 104 0.700 1.08 × 105
5.00 × 104 0.876 1.35 × 105
6.00 × 104 1.05 1.62 × 105
7.00 × 104 1.23 1.89 × 105
8.00 × 104 1.40 2.16 × 105
9.00 × 104 1.58 2.43 × 105
1.00 × 105 1.75 2.70 × 105
1.10 × 105 1.93 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.00402 397
100 0.00428 422
200 0.00855 844
300 0.0128 1270
400 0.0171 1690
500 0.0214 2110
600 0.0257 2530
700 0.0299 2950
800 0.0342 3380
900 0.0385 3800
1000 0.0428 4220
2000 0.0855 8440
3000 0.128 1.27 × 104
4000 0.171 1.69 × 104
5000 0.214 2.11 × 104
6000 0.257 2.53 × 104
7000 0.299 2.95 × 104
8000 0.342 3.38 × 104
9000 0.385 3.80 × 104
1.00 × 104 0.428 4.22 × 104
2.00 × 104 0.855 8.44 × 104
3.00 × 104 1.28 1.27 × 105
4.00 × 104 1.71 1.69 × 105
5.00 × 104 2.14 2.11 × 105
6.00 × 104 2.57 2.53 × 105
7.00 × 104 2.99 2.95 × 105
7.04 × 104 3.01 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.00833 571
100 0.00886 608
200 0.0177 1220
300 0.0266 1820
400 0.0355 2430
500 0.0443 3040
600 0.0532 3650
700 0.0621 4250
800 0.0709 4860
900 0.0798 5470
1000 0.0886 6080
2000 0.177 1.22 × 104
3000 0.266 1.82 × 104
4000 0.355 2.43 × 104
5000 0.443 3.04 × 104
6000 0.532 3.65 × 104
7000 0.621 4.25 × 104
8000 0.709 4.86 × 104
9000 0.798 5.47 × 104
1.00 × 104 0.886 6.08 × 104
2.00 × 104 1.77 1.22 × 105
3.00 × 104 2.66 1.82 × 105
4.00 × 104 3.55 2.43 × 105
4.89 × 104 4.33 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.0263 1020
100 0.0280 1080
200 0.0560 2160
300 0.0841 3240
400 0.112 4320
500 0.140 5400
600 0.168 6480
700 0.196 7560
800 0.224 8640
900 0.252 9720
1000 0.280 1.08 × 104
2000 0.560 2.16 × 104
3000 0.841 3.24 × 104
4000 1.12 4.32 × 104
5000 1.40 5.40 × 104
6000 1.68 6.48 × 104
7000 1.96 7.56 × 104
8000 2.24 8.64 × 104
9000 2.52 9.72 × 104
1.00 × 104 2.80 1.08 × 105
2.00 × 104 5.60 2.16 × 105
2.75 × 104 7.70 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.0643 1590
100 0.0684 1690
200 0.137 3380
300 0.205 5060
400 0.274 6750
500 0.342 8440
600 0.410 1.01 × 104
700 0.479 1.18 × 104
800 0.547 1.35 × 104
900 0.616 1.52 × 104
1000 0.684 1.69 × 104
2000 1.37 3.38 × 104
3000 2.05 5.06 × 104
4000 2.74 6.75 × 104
5000 3.42 8.44 × 104
6000 4.10 1.01 × 105
7000 4.79 1.18 × 105
8000 5.47 1.35 × 105
9000 6.16 1.52 × 105
1.00 × 104 6.84 1.69 × 105
1.76 × 104 12.0 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.133 2290
100 0.142 2430
200 0.284 4860
300 0.426 7290
400 0.567 9720
500 0.709 1.22 × 104
600 0.851 1.46 × 104
700 0.993 1.70 × 104
800 1.13 1.94 × 104
900 1.28 2.19 × 104
1000 1.42 2.43 × 104
2000 2.84 4.86 × 104
3000 4.26 7.29 × 104
4000 5.67 9.72 × 104
5000 7.09 1.22 × 105
6000 8.51 1.46 × 105
7000 9.93 1.70 × 105
8000 11.3 1.94 × 105
9000 12.8 2.19 × 105
1.00 × 104 14.2 2.43 × 105
1.22 × 104 17.3 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.247 3110
100 0.263 3310
200 0.526 6620
300 0.788 9930
400 1.05 1.32 × 104
500 1.31 1.65 × 104
600 1.58 1.99 × 104
700 1.84 2.32 × 104
800 2.10 2.65 × 104
900 2.36 2.98 × 104
1000 2.63 3.31 × 104
2000 5.26 6.62 × 104
3000 7.88 9.93 × 104
4000 10.5 1.32 × 105
5000 13.1 1.65 × 105
6000 15.8 1.99 × 105
7000 18.4 2.32 × 105
8000 21.0 2.65 × 105
8980 23.6 2.97 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.421 4060
100 0.448 4320
200 0.897 8640
300 1.34 1.30 × 104
400 1.79 1.73 × 104
500 2.24 2.16 × 104
600 2.69 2.59 × 104
700 3.14 3.03 × 104
800 3.59 3.46 × 104
900 4.03 3.89 × 104
1000 4.48 4.32 × 104
2000 8.97 8.64 × 104
3000 13.4 1.30 × 105
4000 17.9 1.73 × 105
5000 22.4 2.16 × 105
5420 24.3 2.34 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 0.675 5140
100 0.718 5470
200 1.44 1.09 × 104
300 2.15 1.64 × 104
400 2.87 2.19 × 104
500 3.59 2.73 × 104
600 4.31 3.28 × 104
700 5.03 3.83 × 104
800 5.74 4.38 × 104
900 6.46 4.92 × 104
1000 7.18 5.47 × 104
2000 14.4 1.09 × 105
3000 21.5 1.64 × 105
3390 24.3 1.85 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 1.03 6350
100 1.09 6750
200 2.19 1.35 × 104
300 3.28 2.03 × 104
400 4.38 2.70 × 104
500 5.47 3.38 × 104
600 6.57 4.05 × 104
700 7.66 4.73 × 104
800 8.76 5.40 × 104
900 9.85 6.08 × 104
1000 10.9 6.75 × 104
2000 21.9 1.35 × 105
2220 24.3 1.50 × 105
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 2.51 9920
100 2.67 1.06 × 104
200 5.34 2.11 × 104
300 8.02 3.17 × 104
400 10.7 4.22 × 104
500 13.4 5.28 × 104
600 16.0 6.33 × 104
700 18.7 7.39 × 104
800 21.4 8.44 × 104
900 24.0 9.50 × 104
910 24.3 9.60 × 104
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 5.21 1.43 × 104
100 5.54 1.52 × 104
200 11.1 3.04 × 104
300 16.6 4.56 × 104
400 22.2 6.08 × 104
439 24.3 6.67 × 104
Steel I Beam: W24 × 94 (Wide Flange 24 inch tall × 94 lbf/ft)
L = 200 ft
P (lbf/ft) w_max (in) stress_max (psi)
94.0 16.5 2.54 × 104
100 17.5 2.70 × 104
139 24.3 3.75 × 104
Additional Information
Related Pages
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.