Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Laser Focus World

Semiconductors, medical equipment, lasers, optics and aviation and aerospace.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free magazines
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W27 × 114
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 4090 in4) for the W27 × 114 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
L = 200 ft
  
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 6.67 × 10-7 5.13
200 1.17 × 10-6 9.01
300 1.76 × 10-6 13.5
400 2.34 × 10-6 18.0
500 2.93 × 10-6 22.5
600 3.51 × 10-6 27.0
700 4.10 × 10-6 31.5
800 4.68 × 10-6 36.0
900 5.27 × 10-6 40.5
1000 5.85 × 10-6 45.0
2000 1.17 × 10-5 90.1
3000 1.76 × 10-5 135
4000 2.34 × 10-5 180
5000 2.93 × 10-5 225
6000 3.51 × 10-5 270
7000 4.10 × 10-5 315
8000 4.68 × 10-5 360
9000 5.27 × 10-5 405
1.00 × 104 5.85 × 10-5 450
2.00 × 104 1.17 × 10-4 901
3.00 × 104 1.76 × 10-4 1350
4.00 × 104 2.34 × 10-4 1800
5.00 × 104 2.93 × 10-4 2250
6.00 × 104 3.51 × 10-4 2700
7.00 × 104 4.10 × 10-4 3150
8.00 × 104 4.68 × 10-4 3600
9.00 × 104 5.27 × 10-4 4050
1.00 × 105 5.85 × 10-4 4500
2.00 × 105 0.00117 9010
3.00 × 105 0.00176 1.35 × 104
4.00 × 105 0.00234 1.80 × 104
5.00 × 105 0.00293 2.25 × 104
6.00 × 105 0.00351 2.70 × 104
7.00 × 105 0.00410 3.15 × 104
8.00 × 105 0.00468 3.60 × 104
9.00 × 105 0.00527 4.05 × 104
1.00 × 106 0.00585 4.50 × 104
2.00 × 106 0.0117 9.01 × 104
3.00 × 106 0.0176 1.35 × 105
4.00 × 106 0.0234 1.80 × 105
5.00 × 106 0.0293 2.25 × 105
6.00 × 106 0.0351 2.70 × 105
6.60 × 106 0.0386 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 5.15 × 10-6 14.3
200 9.03 × 10-6 25.0
300 1.35 × 10-5 37.5
400 1.81 × 10-5 50.0
500 2.26 × 10-5 62.6
600 2.71 × 10-5 75.1
700 3.16 × 10-5 87.6
800 3.61 × 10-5 100
900 4.06 × 10-5 113
1000 4.52 × 10-5 125
2000 9.03 × 10-5 250
3000 1.35 × 10-4 375
4000 1.81 × 10-4 500
5000 2.26 × 10-4 626
6000 2.71 × 10-4 751
7000 3.16 × 10-4 876
8000 3.61 × 10-4 1000
9000 4.06 × 10-4 1130
1.00 × 104 4.52 × 10-4 1250
2.00 × 104 9.03 × 10-4 2500
3.00 × 104 0.00135 3750
4.00 × 104 0.00181 5000
5.00 × 104 0.00226 6260
6.00 × 104 0.00271 7510
7.00 × 104 0.00316 8760
8.00 × 104 0.00361 1.00 × 104
9.00 × 104 0.00406 1.13 × 104
1.00 × 105 0.00452 1.25 × 104
2.00 × 105 0.00903 2.50 × 104
3.00 × 105 0.0135 3.75 × 104
4.00 × 105 0.0181 5.00 × 104
5.00 × 105 0.0226 6.26 × 104
6.00 × 105 0.0271 7.51 × 104
7.00 × 105 0.0316 8.76 × 104
8.00 × 105 0.0361 1.00 × 105
9.00 × 105 0.0406 1.13 × 105
1.00 × 106 0.0452 1.25 × 105
2.00 × 106 0.0903 2.50 × 105
2.37 × 106 0.107 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 8.24 × 10-5 57.0
200 1.44 × 10-4 100
300 2.17 × 10-4 150
400 2.89 × 10-4 200
500 3.61 × 10-4 250
600 4.33 × 10-4 300
700 5.06 × 10-4 350
800 5.78 × 10-4 400
900 6.50 × 10-4 450
1000 7.22 × 10-4 500
2000 0.00144 1000
3000 0.00217 1500
4000 0.00289 2000
5000 0.00361 2500
6000 0.00433 3000
7000 0.00506 3500
8000 0.00578 4000
9000 0.00650 4500
1.00 × 104 0.00722 5000
2.00 × 104 0.0144 1.00 × 104
3.00 × 104 0.0217 1.50 × 104
4.00 × 104 0.0289 2.00 × 104
5.00 × 104 0.0361 2.50 × 104
6.00 × 104 0.0433 3.00 × 104
7.00 × 104 0.0506 3.50 × 104
8.00 × 104 0.0578 4.00 × 104
9.00 × 104 0.0650 4.50 × 104
1.00 × 105 0.0722 5.00 × 104
2.00 × 105 0.144 1.00 × 105
3.00 × 105 0.217 1.50 × 105
4.00 × 105 0.289 2.00 × 105
5.00 × 105 0.361 2.50 × 105
5.94 × 105 0.429 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 4.17 × 10-4 128
200 7.31 × 10-4 225
300 0.00110 338
400 0.00146 450
500 0.00183 563
600 0.00219 676
700 0.00256 788
800 0.00293 901
900 0.00329 1010
1000 0.00366 1130
2000 0.00731 2250
3000 0.0110 3380
4000 0.0146 4500
5000 0.0183 5630
6000 0.0219 6760
7000 0.0256 7880
8000 0.0293 9010
9000 0.0329 1.01 × 104
1.00 × 104 0.0366 1.13 × 104
2.00 × 104 0.0731 2.25 × 104
3.00 × 104 0.110 3.38 × 104
4.00 × 104 0.146 4.50 × 104
5.00 × 104 0.183 5.63 × 104
6.00 × 104 0.219 6.76 × 104
7.00 × 104 0.256 7.88 × 104
8.00 × 104 0.293 9.01 × 104
9.00 × 104 0.329 1.01 × 105
1.00 × 105 0.366 1.13 × 105
2.00 × 105 0.731 2.25 × 105
2.64 × 105 0.965 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.00132 228
200 0.00231 400
300 0.00347 601
400 0.00462 801
500 0.00578 1000
600 0.00694 1200
700 0.00809 1400
800 0.00925 1600
900 0.0104 1800
1000 0.0116 2000
2000 0.0231 4000
3000 0.0347 6010
4000 0.0462 8010
5000 0.0578 1.00 × 104
6000 0.0694 1.20 × 104
7000 0.0809 1.40 × 104
8000 0.0925 1.60 × 104
9000 0.104 1.80 × 104
1.00 × 104 0.116 2.00 × 104
2.00 × 104 0.231 4.00 × 104
3.00 × 104 0.347 6.01 × 104
4.00 × 104 0.462 8.01 × 104
5.00 × 104 0.578 1.00 × 105
6.00 × 104 0.694 1.20 × 105
7.00 × 104 0.809 1.40 × 105
8.00 × 104 0.925 1.60 × 105
9.00 × 104 1.04 1.80 × 105
1.00 × 105 1.16 2.00 × 105
1.48 × 105 1.72 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.00322 357
200 0.00564 626
300 0.00847 938
400 0.0113 1250
500 0.0141 1560
600 0.0169 1880
700 0.0198 2190
800 0.0226 2500
900 0.0254 2810
1000 0.0282 3130
2000 0.0564 6260
3000 0.0847 9380
4000 0.113 1.25 × 104
5000 0.141 1.56 × 104
6000 0.169 1.88 × 104
7000 0.198 2.19 × 104
8000 0.226 2.50 × 104
9000 0.254 2.81 × 104
1.00 × 104 0.282 3.13 × 104
2.00 × 104 0.564 6.26 × 104
3.00 × 104 0.847 9.38 × 104
4.00 × 104 1.13 1.25 × 105
5.00 × 104 1.41 1.56 × 105
6.00 × 104 1.69 1.88 × 105
7.00 × 104 1.98 2.19 × 105
8.00 × 104 2.26 2.50 × 105
9.00 × 104 2.54 2.81 × 105
9.50 × 104 2.68 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.00667 513
200 0.0117 901
300 0.0176 1350
400 0.0234 1800
500 0.0293 2250
600 0.0351 2700
700 0.0410 3150
800 0.0468 3600
900 0.0527 4050
1000 0.0585 4500
2000 0.117 9010
3000 0.176 1.35 × 104
4000 0.234 1.80 × 104
5000 0.293 2.25 × 104
6000 0.351 2.70 × 104
7000 0.410 3.15 × 104
8000 0.468 3.60 × 104
9000 0.527 4.05 × 104
1.00 × 104 0.585 4.50 × 104
2.00 × 104 1.17 9.01 × 104
3.00 × 104 1.76 1.35 × 105
4.00 × 104 2.34 1.80 × 105
5.00 × 104 2.93 2.25 × 105
6.00 × 104 3.51 2.70 × 105
6.60 × 104 3.86 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.0211 913
200 0.0370 1600
300 0.0555 2400
400 0.0740 3200
500 0.0925 4000
600 0.111 4800
700 0.129 5600
800 0.148 6410
900 0.166 7210
1000 0.185 8010
2000 0.370 1.60 × 104
3000 0.555 2.40 × 104
4000 0.740 3.20 × 104
5000 0.925 4.00 × 104
6000 1.11 4.80 × 104
7000 1.29 5.60 × 104
8000 1.48 6.41 × 104
9000 1.66 7.21 × 104
1.00 × 104 1.85 8.01 × 104
2.00 × 104 3.70 1.60 × 105
3.00 × 104 5.55 2.40 × 105
3.71 × 104 6.86 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.0515 1430
200 0.0903 2500
300 0.135 3750
400 0.181 5000
500 0.226 6260
600 0.271 7510
700 0.316 8760
800 0.361 1.00 × 104
900 0.406 1.13 × 104
1000 0.452 1.25 × 104
2000 0.903 2.50 × 104
3000 1.35 3.75 × 104
4000 1.81 5.00 × 104
5000 2.26 6.26 × 104
6000 2.71 7.51 × 104
7000 3.16 8.76 × 104
8000 3.61 1.00 × 105
9000 4.06 1.13 × 105
1.00 × 104 4.52 1.25 × 105
2.00 × 104 9.03 2.50 × 105
2.37 × 104 10.7 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.107 2050
200 0.187 3600
300 0.281 5400
400 0.375 7210
500 0.468 9010
600 0.562 1.08 × 104
700 0.655 1.26 × 104
800 0.749 1.44 × 104
900 0.843 1.62 × 104
1000 0.936 1.80 × 104
2000 1.87 3.60 × 104
3000 2.81 5.40 × 104
4000 3.75 7.21 × 104
5000 4.68 9.01 × 104
6000 5.62 1.08 × 105
7000 6.55 1.26 × 105
8000 7.49 1.44 × 105
9000 8.43 1.62 × 105
1.00 × 104 9.36 1.80 × 105
1.65 × 104 15.4 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.198 2800
200 0.347 4900
300 0.520 7360
400 0.694 9810
500 0.867 1.23 × 104
600 1.04 1.47 × 104
700 1.21 1.72 × 104
800 1.39 1.96 × 104
900 1.56 2.21 × 104
1000 1.73 2.45 × 104
2000 3.47 4.90 × 104
3000 5.20 7.36 × 104
4000 6.94 9.81 × 104
5000 8.67 1.23 × 105
6000 10.4 1.47 × 105
7000 12.1 1.72 × 105
8000 13.9 1.96 × 105
9000 15.6 2.21 × 105
1.00 × 104 17.3 2.45 × 105
1.21 × 104 21.0 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.337 3650
200 0.592 6410
300 0.888 9610
400 1.18 1.28 × 104
500 1.48 1.60 × 104
600 1.78 1.92 × 104
700 2.07 2.24 × 104
800 2.37 2.56 × 104
900 2.66 2.88 × 104
1000 2.96 3.20 × 104
2000 5.92 6.41 × 104
3000 8.88 9.61 × 104
4000 11.8 1.28 × 105
5000 14.8 1.60 × 105
6000 17.8 1.92 × 105
7000 20.7 2.24 × 105
8000 23.7 2.56 × 105
9000 26.6 2.88 × 105
9270 27.4 2.97 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.540 4620
200 0.948 8110
300 1.42 1.22 × 104
400 1.90 1.62 × 104
500 2.37 2.03 × 104
600 2.84 2.43 × 104
700 3.32 2.84 × 104
800 3.79 3.24 × 104
900 4.27 3.65 × 104
1000 4.74 4.05 × 104
2000 9.48 8.11 × 104
3000 14.2 1.22 × 105
4000 19.0 1.62 × 105
5000 23.7 2.03 × 105
5760 27.3 2.33 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 0.824 5700
200 1.44 1.00 × 104
300 2.17 1.50 × 104
400 2.89 2.00 × 104
500 3.61 2.50 × 104
600 4.33 3.00 × 104
700 5.06 3.50 × 104
800 5.78 4.00 × 104
900 6.50 4.50 × 104
1000 7.22 5.00 × 104
2000 14.4 1.00 × 105
3000 21.7 1.50 × 105
3780 27.3 1.89 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 2.01 8910
200 3.53 1.56 × 104
300 5.29 2.35 × 104
400 7.06 3.13 × 104
500 8.82 3.91 × 104
600 10.6 4.69 × 104
700 12.3 5.47 × 104
800 14.1 6.26 × 104
900 15.9 7.04 × 104
1000 17.6 7.82 × 104
1550 27.3 1.21 × 105
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 4.17 1.28 × 104
200 7.31 2.25 × 104
300 11.0 3.38 × 104
400 14.6 4.50 × 104
500 18.3 5.63 × 104
600 21.9 6.76 × 104
700 25.6 7.88 × 104
746 27.3 8.40 × 104
Steel I Beam: W27 × 114 (Wide Flange 27 inch tall × 114 lbf/ft)
L = 200 ft
P (lbf/ft) w_max (in) stress_max (psi)
114 13.2 2.28 × 104
200 23.1 4.00 × 104
236 27.3 4.73 × 104