AA 5252 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 97.5% Aluminum (Al) and 2.5% Magnesium (Mg). It can be seen in the form of sheet.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions.
Additional Information

Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages

Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Fluoroplastics: THV-500
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Polymers: Polycarbonate: 2% Silicone, 30% Glass Fiber Reinforced: Lubricated
Glossary: Materials: Alloys: Steel: Tool Steel: AISI O2
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5147
Glossary: Materials: Polymers: Thermoplastic Elastomers: Block Copolymer of Styrene and Ethylene And/or Butylene
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Fluoroplastics: Poly(vinylidene Fluoride)
Glossary: Materials: Polymers: Fluoroplastics: THV-500
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Polymers: Polycarbonate: 2% Silicone, 30% Glass Fiber Reinforced: Lubricated
Glossary: Materials: Alloys: Steel: Tool Steel: AISI O2
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5147
Glossary: Materials: Polymers: Thermoplastic Elastomers: Block Copolymer of Styrene and Ethylene And/or Butylene
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Fluoroplastics: Poly(vinylidene Fluoride)
Related Pages

Stamping: Machining of Sheet Metals
Drilling, tapping, counterboring, and countersinking are the usual operations done in sheet metal.
eFunda: Properties of Aluminum Alloy AA 5252
eFunda: Properties of Aluminum Alloy AA 5252. ... Aluminum Alloy AA 5252 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an ...
eFunda: Listing of AA 5xxx Aluminum Alloys
AA 5005, Wrought. AA 5050, Wrought. AA 5052, Wrought. AA 5056, Wrought. AA 5083, Wrought. AA 5086, Wrought. AA 5154, Wrought. AA 5182, Wrought. AA 5252 ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5252
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5252.
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda: Properties of Aluminum Alloy AA 3004
eFunda: Properties of Aluminum Alloy AA 3004. ... Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys ...
eFunda: Listing of Titanium Alloys
Ti-5Al-2.5Sn, Wrought, Alpha alloy. Ti-5Al-2.5Sn-ELI (low O2), Wrought, Alpha alloy. Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Wrought, Near alpha alloy ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
eFunda Polymers: Properties of Allyl {allyl diglycol carbonate ...
eFunda Polymers: Properties of Allyl {allyl diglycol carbonate, cast sheet} ... State: allyl diglycol carbonate. Application: cast sheet ...