30% Glass Fiber Reinforced Injection Molding Grade ABS is a subcategory of Acrylonitrile-Butadiene-Styrene. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 1000 to 1200 MPa. Its tensile strength ranges from 13000 to 16000 MPa at break. Its flexural strength ranges from 17000 to 19000 MPa. Its compressive strength ranges from 15000 to 17000 MPa. Its Izod Impact strength ranges from 1.2 to 1.3 J/cm. Its elongation at break ranges from 1.5 to 1.8 %. Its hardness ranges from 75 to 85 Rockwell M. Its melting temperature ranges from 100 to 110 °C.
Acrylonitrile-Butadiene-Styrene, also known as ABS, is a thermoplastic. Common trade names are Cycolac and Lustran. It is tough, hard and rigid. It has good chemical resistance, dimensional stability, and creep resistance. It is electroplatable and inexpensive. It has moderate mechanical strength but with a tendency to stress crack. Also, it will be degraded (dissolved) when exposed to acetone. ABS is commonly used in electronic housings, auto parts, consumer products, pipe fittings, waste pipes, computer housings (electroplated on the inside), and automotive interior and exterior trim. ABS is considered superior for its hardness, gloss, toughness, and electrical insulation properties. Although ABS plastics are used primarily for their mechanical properties, they also have good electrical properties that are fairly constant over a wide range of frequencies.
Additional Information
Other common Acrylonitrile-Butadiene-Styrene (ABS) include Extrusion Grade ABS, Flame-Retardant Grades, Molding and Extrusion ABS, ABS / PVC Flame-Retardant Grades, Molding and Extrusion ABS, ABS / PC Flame-Retardant Grades, Molding and Extrusion ABS, ABS / Nylon ABS, ABS / PC Injection Molding and Extrusion ABS, Injection Molding Grade, Heat Resistant ABS, Injection Molding Grade, Medium Impact ABS, Injection Molding Grade, High Impact ABS, Injection Molding Grade, Platable ABS, Injection Molding Grade ABS, 20% Glass Fiber Reinforced Injection Molding Grade ABS, 20% Long Glass Fiber Reinforced Injection Molding Grade ABS, 40% Long Glass Fiber Reinforced Injection Molding Grade ABS, 6% Stainless Steel Fiber EMI Shielding (conductive) ABS, 7% Stainless Steel Fiber EMI Shielding (conductive) ABS, 10% Stainless Steel Fiber EMI Shielding (conductive) ABS, 20% PAN Carbon Fiber EMI Shielding (conductive) ABS, 20% Graphite Fiber EMI Shielding (conductive) ABS, 40% Aluminum Flake EMI Shielding (conductive) ABS, and Rubber Modified Injection Molding and Extrusion Grades ABS.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8822
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Platable
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-24
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4118H
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A678 Grade B
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-26
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1042
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Platable
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-24
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4118H
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A678 Grade B
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-26
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1042
Related Pages
eFunda Polymers: Properties of Polypropylene {homopolymer, 10 - 30 ...
... Polymers: Properties of Polypropylene {homopolymer, 10 - 30% glass fiber reinforced} ... State: homopolymer. Additives: 10 - 30% glass fiber reinforced ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 20 - 30 ...
... Properties of Polypropylene {homopolymer, 20 - 30% long glass fiber reinforced} ... State: homopolymer. Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda: Introduction to Injection Molding
Polystyrene (PS); Acrylonitrile Butadiene Styrene (ABS); Polyamide (PA); Polypropylene (PP); Polyethylene (PE); Polyvinylchloride (PVC); Other short fiber ...
eFunda Polymers: Properties of ABS {6% stainless steel fiber, EMI ...
eFunda Polymers: Properties of ABS {6% stainless steel fiber, EMI shielding (conductive)}
eFunda Polymers: Properties of ABS {injection molding grade, heat ...
eFunda Polymers: Properties of ABS {injection molding grade, heat resistant}
eFunda Polymers: Listing of Polystyrene (Novacor 555)
Polystyrene and styrene copolymers, ASA with acrylonitrile / butadiene / styrene copolymer, clear styrene butadiene copolymers. ...
eFunda: Listing of Common Polymers (Plastics)
Acrylonitrile-Butadiene-Styrene, (ABS), Thermoplastic. ... Polyacrylonitrile, (PAN), (Acrylonitrile), Thermoplastic. ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone ...
State: polysulfone. Application: injection molding, platable grade ... Compression Ratio, 2. Linear Mold Shrinkage (cm/cm), 0.0025, D955 ...