Glossary » Materials » Polymers » Allyl Resin » DAP » Glass Filled » Molding Compound
Glass Filled Molding Compound Allyl is a subcategory of Allyl Resin. The additative is added during the manufacturing process. Its elastic modulus ranges from 1400 to 2200 MPa. Its flexural modulus ranges from 1200 to 1500 MPa. Its tensile strength ranges from 6000 to 11000 MPa at break. Its flexural strength ranges from 9000 to 20000 MPa. Its compressive strength ranges from 25000 to 35000 MPa. Its Izod Impact strength ranges from 0.4 to 15 J/cm. Its elongation at break ranges from 3 to 5 %. Its hardness ranges from 80 to 87 Rockwell E. Its specific gravity ranges from 1.7 to 1.98. Its coefficient of thermal expansion ranges from 10 to 36 x 10-6/°C. Its molding pressure ranges from 2 to 6 MPa.
Allyl Resin, also known as Allyl, is a thermoset polycondensate. DAP Allyl is commonly used in molding compounds.
Additional Information
Other common Allyl Resin (Allyl) include Cast Sheet Allyl, and Mineral Filled Molding Compound Allyl.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polysulfone: Poly(arylsulfone)
Glossary: Materials: Alloys: Aluminum Alloy: Cast: A390.0
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2024
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, Impact Modified
Glossary: Materials: Polymers: Liquid Crystal Polymer: 30% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 5% Molydenum Disulfide and 30% PTFE: Lubricated
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8630
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polysulfone: Poly(arylsulfone)
Glossary: Materials: Alloys: Aluminum Alloy: Cast: A390.0
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2024
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, Impact Modified
Glossary: Materials: Polymers: Liquid Crystal Polymer: 30% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 5% Molydenum Disulfide and 30% PTFE: Lubricated
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8630
Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 11), molding ...
State: nylon (PA 11). Application: molding and extrusion compound ... Compression Ratio, 2.7 - 3.3. Linear Mold Shrinkage (cm/cm), 0.012, D955 ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Piezo Material Data
Select specific piezoelectric material to view constitutive properties.
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda: Glossary: Materials: Alloys: Aluminum Alloy: AA 5052
eFunda Polymers: Properties of Allyl {allyl diglycol carbonate . ... State: allyl diglycol carbonate. Application: cast sheet . ...
eFunda: Properties of Piezo Material Quartz
eFunda: Properties of Piezo Material Quartz. ... Piezo Data: Quartz Home | Directory | Career | News | InfoStore | Industrial · Materials Home. Piezo Basics ...
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
eFunda Polymers: Listing of Epoxy (Acme, Aerolam, Basoset, Beckopx ...
Epoxy, mineral and glass filled, novolak molding compounds, encapsulation. 7. Epoxy, mineral and glass filled, novolak molding compounds, high temperature. ...