Glossary » Materials » Polymers » Epoxy » Mineral and Glass Filled » Novolak Molding Compounds, Encapsulation
Mineral and Glass Filled Novolak Molding Compounds, Encapsulation Epoxy is a subcategory of Epoxy. The additative is added during the manufacturing process. Its flexural modulus ranges from 1400 to 2400 MPa. Its tensile strength ranges from 5000 to 12500 MPa at break. Its flexural strength ranges from 10000 to 21800 MPa. Its compressive strength ranges from 24000 to 48000 MPa. Its Izod Impact strength ranges from 0.3 to 0.5 J/cm. Its specific gravity ranges from 1.6 to 2.05. Its coefficient of thermal expansion ranges from 18 to 43 x 10-6/°C. Its melting temperature ranges from 145 to 155 °C. Its molding pressure ranges from 0.25 to 3 MPa.
Epoxy is a thermoset polyadduct. Common trade names include Acme, Aerolam, Basoset, Beckopx, Conapoxy, Corlar, Cycom, DER, Desmobond, Dobeckot, Dynopon, Ecco, Epikote, Epocast, Epodite, Eprosin, Eurepox, Exatron, Grilonit, Hysol, Isochembond, Lekutherm, Lopox, Nikalet, Paraplex, Quartrex, Scotchcast, and Synthane. Epoxy possesses many useful properties: air curable, highly fillable, low shrinkage, low susceptibility to stress formation, good adhesion to almost all materials, high tensile and vibrational strength, high heat resistance, high heat deformation resistance, high chemical attack resistance, good aging properties, good electrical and dielectrical properties, odorless, tasteless, and low flammability. Epoxy is commonly used in adhesives and reactive molding compounds. Epoxy is a copolymer, which means it is formed from two different chemicals, usually referred to as the "resin" and the "hardener". Epoxy-based materials can be used for coatings, adhesives, composite materials, mold making, and electrical insulators. When working with epoxy, vinegar is an effective and safe solvent for cleaning epoxy resins from tools, brushes, skin, and most surfaces.
Additional Information
Other common Epoxy include Glass Fiber Reinforced Molding Compounds Epoxy, Mineral Filled Molding Compounds Epoxy, Glass Sphere Filled Molding Compounds Epoxy, Glass Fiber Reinforced Sheet Molding Compound (SMC) Epoxy, Carbon Fiber Reinforced Sheet Molding Compound (SMC) Epoxy, Mineral and Glass Filled Novolak Molding Compounds, High Temperature Epoxy, Unfilled Casting Resins and Compounds Epoxy, Silica Filled Casting Resins and Compounds Epoxy, Aluminum Filled Casting Resins and Compounds Epoxy, Flexibilized Casting Resins and Compounds Epoxy, and Casting Resins and Compounds Epoxy.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 409
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyacetal: Homopolymer: Chemically Lubricated
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Cast: Oil Filled
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4320
Glossary: Materials: Polymers: Polycarbonate: 30% PTFE
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C54400
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade C
Glossary: Materials: Alloys: Aluminum Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyacetal: Homopolymer: Chemically Lubricated
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Cast: Oil Filled
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4320
Glossary: Materials: Polymers: Polycarbonate: 30% PTFE
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C54400
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade C
Glossary: Materials: Alloys: Aluminum Alloy: Wrought
Related Pages
Rapid Tooling, Composite Epoxy Molding
composite molding Description of the composite molding process as it applies to a toy locomotive.
eFunda Polymers: Properties of Epoxy {aluminum filled, casting ...
eFunda Polymers: Properties of Epoxy {aluminum filled, casting resins and compounds}
eFunda Polymers: Properties of Epoxy {bisphenol, low density ...
eFunda Polymers: Properties of Epoxy {bisphenol, low density, glass sphere filled, molding compounds}
eFunda Polymers: Properties of Epoxy {flexibilized, casting resins ...
eFunda Polymers: Properties of Epoxy {flexibilized, casting resins and compounds}
eFunda Polymers: Listing of Epoxy (Acme, Aerolam, Basoset, Beckopx ...
eFunda Polymers: Listing of Epoxy (Acme, Aerolam, Basoset, Beckopx, Conapoxy, Corlar, Cycom, DER, Desmobond, Dobeckot, Dynopon, Ecco, Epikote, Epocast, ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Trade Name: Acme, Aerolam, Basoset, Beckopx, Conapoxy, Corlar, Cycom, DER, Desmobond, Dobeckot, Dynopon, Ecco, Epikote, Epocast, Epodite, Eprosin, Eurepox, ...
eFunda Polymers: Properties of Epoxy {glass fiber reinforced ...
eFunda Polymers: Properties of Epoxy {glass fiber reinforced, sheet molding compound (SMC)}
eFunda Polymers: Properties of Epoxy {bisphenol, mineral filled ...
eFunda Polymers: Properties of Epoxy {bisphenol, mineral filled, molding compounds}
Screws
Other symmetrical threads are the Whitworth, and the Acme. The Acme thread form has a stronger thread which allows for use in translational applications ...
eFunda Polymers: Properties of Epoxy {mineral and glass filled ...
eFunda Polymers: Properties of Epoxy {mineral and glass filled, novolak molding compounds, high temperature}