Glossary » Materials » Polymers » Polyamide » Aromatic » Unfilled » Aramid Molded Parts
Unfilled Aramid Molded Parts PA is a subcategory of Polyamide. The additative is added during the manufacturing process.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. aromatic It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Polymers: Polyacetal: Homopolymer: 20% Glass Reinforced
Glossary: Materials: Alloys: Titanium Alloy: Wrought
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82600
Glossary: Materials: Polymers: Polyphenylene Sulfide: 40% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4028H
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C87900
Glossary: Materials: Polymers: Polyacetal: Homopolymer: 20% Glass Reinforced
Glossary: Materials: Alloys: Titanium Alloy: Wrought
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82600
Glossary: Materials: Polymers: Polyphenylene Sulfide: 40% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4028H
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C87900
Related Pages
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda Polymers: Properties of Polyimide {thermoplastic, unfilled}
eFunda Polymers: Properties of Polyimide {thermoplastic, unfilled}
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone ...
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone), unfilled} ... State: poly(ethersulfone). Additives: unfilled ...
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda Polymers: Properties of Polyimide {thermoset, unfilled}
eFunda Polymers: Properties of Polyimide {thermoset, unfilled}
eFunda Polymers: Properties of Polypropylene {copolymer, unfilled}
eFunda Polymers: Properties of Polypropylene {copolymer, unfilled}
eFunda Polymers: Properties of Phenolic {unfilled, casting resins}
eFunda Polymers: Properties of Phenolic {unfilled, casting resins}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda Polymers: Properties of Fluoroplastics {modified PE-TFE ...
eFunda Polymers: Properties of Fluoroplastics {modified PE-TFE, unfilled} ... State: modified PE-TFE. Additives: unfilled ...