Glossary » Materials » Polymers » Polyamide » Unreinforced, Toughened
Unreinforced, Toughened PA is a subcategory of Polyamide. The additative is added during the manufacturing process. Its elongation at break ranges from 65 to 150 %. Its melting temperature ranges from 210 to 220 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Aluminum Alloy: Wrought
Glossary: Materials: Polymers: Fluoroplastics: THV-400
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5117
Glossary: Materials: Polymers: Polystyrene: Copolymer: Impact Modified: High Heat Resistant
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1040
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A203 Grade B
Glossary: Materials: Polymers: Liquid Crystal Polymer: 30% Mineral Filled
Glossary: Materials: Polymers: Polycarbonate: Polycarbonate / Polyester Blends, Impact Modified
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66)
Glossary: Materials: Polymers: Fluoroplastics: THV-400
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5117
Glossary: Materials: Polymers: Polystyrene: Copolymer: Impact Modified: High Heat Resistant
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1040
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A203 Grade B
Glossary: Materials: Polymers: Liquid Crystal Polymer: 30% Mineral Filled
Glossary: Materials: Polymers: Polycarbonate: Polycarbonate / Polyester Blends, Impact Modified
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66)
Related Pages
eFunda Polymers: Properties of Polyphenylene Oxide (modified ...
eFunda Polymers: Properties of Polyphenylene Oxide (modified) {alloy with nylon, unreinforced} ... Additives: alloy with nylon, unreinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-retardant grade}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter), Unit Symbol: Pa-sqrt(m)
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of Sulfone polymers {poly(phenylene ...
eFunda Polymers: Properties of Sulfone polymers {poly(phenylene-sulfone), unreinforced} ... State: poly(phenylene-sulfone). Additives: unreinforced ...
eFunda Polymers: Properties of Polyester (thermoplastic) {alloy ...
eFunda Polymers: Properties of Polyester (thermoplastic) {alloy, unreinforced, flame-retardant} ... Additives: unreinforced. Application: flame-retardant ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}