Glossary » Materials » Polymers » Polyamide » Nylon (PA 610) » 30% Glass Fiber Reinforced » Flame-Retardant Grade
30% Glass Fiber Reinforced Flame-Retardant Grade PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 610) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5652
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 40% Aluminium Flake: EMI Shielding (conductive)
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11600
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 27 - 30% Glass Fiber and Mineral Reinforced
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C35000
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 15% Glass Reinforced V-O
Glossary: Materials: Polymers: Polyester
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5652
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 40% Aluminium Flake: EMI Shielding (conductive)
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11600
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 27 - 30% Glass Fiber and Mineral Reinforced
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C35000
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 15% Glass Reinforced V-O
Glossary: Materials: Polymers: Polyester
Related Pages
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
... Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced, flame-retardant grade} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter), Unit Symbol: Pa-sqrt(m)
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30 ...
Trade Publications. Reinforced Plastics · Design-2-Part · Chemical Processing ... Additives: 30% glass fiber reinforced. Application: flame-retardant grade ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant grades, molding and extrusion}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, also known as PA, or Nylon, has been mass-produced since 1935. ... Polyamide, nylon alloys, ceramic and glass fiber reinforced. ...