Glossary » Materials » Polymers » Polyamide » Nylon (PA 66) » Molding Compound
Molding Compound PA is a subcategory of Polyamide. It is specially formulated to molding compound. Its elastic modulus ranges from 230 to 550 MPa. Its flexural modulus ranges from 410 to 470 MPa. Its flexural strength ranges from 1700 to 17900 MPa. Its compressive strength ranges from 12500 to 15000 MPa. Its Izod Impact strength ranges from 0.55 to 1 J/cm. Its elongation at break ranges from 15 to 80 %. Its specific gravity ranges from 1.13 to 1.15. Its melting temperature ranges from 255 to 265 °C. Its molding pressure ranges from 1 to 25 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Magnesium Alloy: ASTM ZK60A-T5
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Units: Pressure: Newton Per Square Meter
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 35% Glass, Super Toughened
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A414 Grade B
Glossary: Units: Pressure: Meter of Water (15.56°C)
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyphenylene Sulfide: 55% Glass and Mineral Reinforced
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Units: Pressure: Newton Per Square Meter
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 35% Glass, Super Toughened
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A414 Grade B
Glossary: Units: Pressure: Meter of Water (15.56°C)
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyphenylene Sulfide: 55% Glass and Mineral Reinforced
Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 612), molding ...
State: nylon (PA 612). Application: molding compound ... 240 - 243, extrusion. Molding Pressure (MPa), 7 - 104. Linear Mold Shrinkage (cm/cm), 0.011, D955 ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 12), molding ...
State: nylon (PA 12). Application: molding and extrusion compound ... Compression Ratio, 2.5 - 4. Linear Mold Shrinkage (cm/cm), 0.003 - 0.015, D955 ...
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter), Unit Symbol: Pa-sqrt(m)
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend}