Glossary » Materials » Polymers » Polyamide » Plasticized
Plasticized PA is a subcategory of Polyamide. The additative is added during the manufacturing process. Its elastic modulus ranges from 375 to 440 MPa. Its flexural modulus ranges from 330 to 350 MPa. Its tensile strength ranges from 9700 to 10800 MPa at break. Its flexural strength ranges from 12000 to 13000 MPa. Its compressive strength ranges from 22000 to 25000 MPa. Its Izod Impact strength ranges from 0.82 to 0.91 J/cm. Its elongation at break ranges from 25 to 35 %. Its hardness ranges from 110 to 115 . Its specific gravity ranges from 1.14 to 1.16. Its melting temperature ranges from 227 to 238 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6), cast It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal)
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C86100
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5160
Glossary: Materials: Polymers: Polyaryletherketone: Poly(arylether-Ketone): 40% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal)
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C86100
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5160
Glossary: Materials: Polymers: Polyaryletherketone: Poly(arylether-Ketone): 40% Glass Fiber Reinforced
Related Pages
eFunda: Glossary: Materials: Alloys: Copper Alloy: UNS C92900
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ... eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized} ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda: Glossary: Materials: Alloys: Copper Alloy: UNS C81500
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}. Permanent Mold Casting. Typically cast iron or Meehanite (a dense cast iron) is ...
eFunda: Glossary: Materials: Alloys: Copper Alloy: UNS C99300
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}. eFunda: Listing of Coppers, High-Copper Alloys. eFunda: Listing of Coppers, ...
eFunda: Glossary: Materials: Alloys: Copper Alloy: UNS C92500
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}. eFunda: Properties of Copper Alloy UNS C15000 ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda: Glossary: Materials: Alloys: Aluminum Alloy: A357.0
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}. Die Casting. On the other hand, pure Aluminum is rarely cast due to high ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend}