Glossary » Materials » Polymers » Polyamide » 35% Glass Fiber Reinforced
35% Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its tensile strength ranges from 30500 to 31000 MPa at break. Its elongation at break ranges from 2.2 to 2.4 %. Its coefficient of thermal expansion ranges from 15 to 48 x 10-6/°C. Its molding pressure ranges from 5 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6), semi-aromatic semicrystalline copolymer It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Polymers: Polystyrene: Rubber-Modified: High Impact
Glossary: Materials: Polymers: Polyethylene: Ethylene / Vinyl Acetate, Low Density Copolymer
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ91C-T6
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A537
Glossary: Materials: Polymers: Polycarbonate: 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A225 Grade A
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1139
Glossary: Materials: Polymers: Polystyrene: Rubber-Modified: High Impact
Glossary: Materials: Polymers: Polyethylene: Ethylene / Vinyl Acetate, Low Density Copolymer
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ91C-T6
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A537
Glossary: Materials: Polymers: Polycarbonate: 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A225 Grade A
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1139
Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester (thermoplastic), poly(butylene-terephthalate), 35% glass fiber reinforced, flame-retardant grade. 18. Polyester (thermoplastic), 30% carbon fiber, ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend}
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda Polymers: Properties of Polyamide {partially aromatic, 35 ...
... Properties of Polyamide {partially aromatic, 35% glass fiber reinforced, impact modified} ... Additives: 35% glass fiber reinforced, impact modified ...
eFunda Polymers: Properties of Polyester (thermoplastic) {alloy ...
State: alloy. Additives: 7.0 - 30% glass fiber reinforced ... Molding Pressure (MPa), 35 - 118. Compression Ratio, 3 - 4. Linear Mold Shrinkage (cm/cm) ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}