Glossary » Materials » Polymers » Polyaryletherketone » Unfilled
Unfilled PAEK is a subcategory of Polyaryletherketone. The additative is added during the manufacturing process. Its elastic modulus ranges from 520 to 580 MPa. Its flexural strength ranges from 18850 to 24500 MPa. Its Izod Impact strength ranges from 1.6 to 2.7 J/cm. Its coefficient of thermal expansion ranges from 41 to 44.2 x 10-6/°C. Its melting temperature ranges from 323 to 381 °C. Its molding pressure ranges from 10 to 20 MPa.
Polyaryletherketone, also known as PAEK, is a thermoplastic polycondensate. poly(arylether-ketone) It provides high performance with excelent high-temperature properties. Its applications include airplane and automobile parts, chemical plants, oil, gas, and steam processing equipments.
Additional Information
Other common Polyaryletherketone (PAEK) include 30% Glass Fiber Reinforced PAEK, 40% Glass Fiber Reinforced PAEK, Modified, 40% Glass PAEK, 30% Carbon Fiber PAEK, Unfilled PAEK, 30% Glass Fiber Reinforced PAEK, and 30% Carbon Fiber Reinforced PAEK.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4419
Glossary: Materials: Alloys: Steel: Tool Steel: AISI W1
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A734 Type A
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304HN
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 15B41H
Glossary: Materials: Polymers: Polycarbonate: Polycarbonate / Polyester Blends, Impact Modified
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4419
Glossary: Materials: Alloys: Steel: Tool Steel: AISI W1
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A734 Type A
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304HN
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 15B41H
Glossary: Materials: Polymers: Polycarbonate: Polycarbonate / Polyester Blends, Impact Modified
Related Pages
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Polyamide {aromatic, unfilled ...
eFunda Polymers: Properties of Polyamide {aromatic, unfilled, aramid molded parts}
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Phenolic {unfilled, casting resins}
eFunda Polymers: Properties of Phenolic {unfilled, casting resins}
eFunda Polymers: Properties of Polyimide {thermoplastic, unfilled}
eFunda Polymers: Properties of Polyimide {thermoplastic, unfilled}
eFunda Polymers: Listing of Polyaryletherketone
eFunda Polymers: Listing of Polyaryletherketone. ... Polyaryletherketone, also known as PAEK, or Ketone,. ... Specific Grades of Polyaryletherketone ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda Polymers: Properties of Epoxy {unfilled, casting resins and ...
eFunda Polymers: Properties of Epoxy {unfilled, casting resins and compounds}
eFunda: Polymers (Plastics) Sorted by Thermoplastic/Thermoset
Polyaryletherketone, (PAEK), (Ketone). •, Polybutadiene, (PBD). •, Polybutylene, (PB). •, Polycarbonate, (PC). •, Polyektone, (PK). ...