Glossary » Materials » Polymers » Polycarbonate » 10-15% PTFE » Lubricated
10-15% PTFE Lubricated PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its flexural modulus ranges from 250 to 300 MPa. Its tensile strength ranges from 7500 to 10000 MPa at break. Its flexural strength ranges from 11000 to 11500 MPa. Its Izod Impact strength ranges from 2.5 to 3 J/cm. Its elongation at break ranges from 8 to 10 %. Its specific gravity ranges from 1.26 to 1.29.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C98200
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A622
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C19500
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 30% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polysulfone: Poly(phenylene-Sulfone)
Glossary: Design: Oring: Material: Polyacrylate
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A622
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C19500
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 30% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polysulfone: Poly(phenylene-Sulfone)
Glossary: Design: Oring: Material: Polyacrylate
Glossary: Materials: Alloys: Steel: Tool Steel
Related Pages
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... 1768.4000000000001 pc = Length. Symbol, Unit Name. 5.45671×1029, Å · angstrom ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polycarbonate, 10-15% PTFE, 20% fiber reinforced, lubricated. ComAlloy International Co. 481 Allied Dr. Nashville, TN 37211. Phone: 615-333-3453 ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced}
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant grades, molding and extrusion}
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... Convert pc. 95 conversions, showing those commonly used | Show all ...
eFunda Polymers: Properties of ABS {ABS / PC, injection molding ...
eFunda Polymers: Properties of ABS {ABS / PC, injection molding and extrusion}
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon)
Polycarbonate, also known as PC, has been mass-produced since 1958. ... Polycarbonate, unfilled, molding and extrusion resins, high viscosity. ...
eFunda: Glossary: Units: Length: Rod (perch, Pole)
Pace (UK), Palm (UK), Parsec (pc), Perch (rod, Pole) (rd), Petameter (Pm), Pica, Picometer (pm), Point (US Printer'S), Pole (rod, Perch) (rd), Quadrant, ...
Fluid Film Bearings
Early sliding bearings were almost certainly first made from wood after the invention of the wheel in prehistoric times, and these were lubricated with ...