Glossary » Materials » Polymers » Polycarbonate » 20 - 30% Long Glass Fiber Reinforced » Flame-Retardant Grade
20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 1000 to 1100 MPa. Its flexural modulus ranges from 900 to 1200 MPa. Its tensile strength ranges from 14000 to 20000 MPa at break. Its flexural strength ranges from 21000 to 30000 MPa. Its compressive strength ranges from 18000 to 21000 MPa. Its Izod Impact strength ranges from 1.8 to 2 J/cm. Its elongation at break ranges from 2 to 3 %. Its hardness ranges from 77 to 85 Rockwell M. Its specific gravity ranges from 1.36 to 1.45.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2024
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4130H
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 30% Graphite Or PAN Carbon Fiber
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyvinylidene Chloride: Copolymer
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Flame-Retardant Grades, Molding and Extrusion
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2024
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4130H
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 30% Graphite Or PAN Carbon Fiber
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyvinylidene Chloride: Copolymer
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Flame-Retardant Grades, Molding and Extrusion
Related Pages
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, nylon (PA 6), 30% long glass fiber reinforced. ... Polyamide, nylon (PA 66), 20-25% glass fiber reinforced, flame-retardant grade. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30% glass fiber reinforced, flame-retardant grade}
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced}
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber ...
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber, EMI shielding (conductive)}
eFunda: Glossary: Units: Force: Ton Force (long)
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced}. eFunda: Magnetic Unit Category. eFunda: Magnetic Unit Category. ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
eFunda Polymers: Properties of Polyethersulfone {20-30% glass ...
eFunda Polymers: Properties of Polyethersulfone {20-30% glass fiber reinforced} ... Additives: 20-30% glass fiber reinforced ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 20 - 30 ...
... Properties of Polypropylene {homopolymer, 20 - 30% long glass fiber reinforced} ... State: homopolymer. Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated}
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated}
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced, flame-retardant ... Additives: 20 - 30% long glass fiber reinforced ...