Glossary » Materials » Polymers » Polycarbonate » 20% PAN Carbon Fiber » EMI Shielding (conductive)
20% PAN Carbon Fiber EMI Shielding (conductive) PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its flexural modulus ranges from 1500 to 1800 MPa. Its tensile strength ranges from 18000 to 20000 MPa at break. Its flexural strength ranges from 27000 to 28000 MPa. Its Izod Impact strength ranges from 1.4 to 2 J/cm.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Unfilled
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C15735
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4161H
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Steel: Tool Steel: AISI O1
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 30% PAN Carbon Fiber: EMI Shielding (conductive)
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Unfilled
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C15735
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4161H
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Steel: Tool Steel: AISI O1
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 30% PAN Carbon Fiber: EMI Shielding (conductive)
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Related Pages
eFunda: Glossary: Units: Linear Mass Density: Denier
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon). Units » Linear Mass Density » Denier · Units » Linear Mass Density » Pound (mass) Per Foot ...
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, nylon (PA 6), 30% glass fiber reinforced, impact modified. 20. Polyamide, nylon (PA 6), 30% PAN carbon fiber, EMI shielding (conductive). ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber reinforced}
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester (thermoplastic), 30% carbon fiber, EMI shielding (conductive). ... Polyester (thermoplastic), poly(ethylene-terephthalate), 15-20% glass, flame-retardant. ... 30% PAN carbon fiber, EMI shielding (conductive). ...
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... 1768.4000000000001 pc = Length. Symbol, Unit Name. 5.45671×1029, Å · angstrom ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
Additives: 30% PAN carbon fiber. Application: EMI shielding (conductive) ... Elongation at break (%), 20, D638. Izod Impact (J/cm of notch) ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant grades, molding and extrusion}
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
eFunda Polymers: Properties of Polycarbonate {6% stainless steel ...
eFunda Polymers: Properties of Polycarbonate {6% stainless steel fiber, conductive}
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced}