Glossary » Materials » Polymers » Polycarbonate » 40% PAN Carbon Fiber » EMI Shielding (conductive)
40% PAN Carbon Fiber EMI Shielding (conductive) PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 3000 to 3100 MPa. Its flexural modulus ranges from 2800 to 2900 MPa. Its tensile strength ranges from 23000 to 24000 MPa at break. Its flexural strength ranges from 34000 to 35000 MPa. Its Izod Impact strength ranges from 1.5 to 2 J/cm. Its elongation at break ranges from 1 to 2 %. Its specific gravity ranges from 1.36 to 1.38. Its coefficient of thermal expansion ranges from 11 to 14.4 x 10-6/°C. Its molding pressure ranges from 15 to 20 MPa.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Polymers: Polystyrene: Rubber-Modified
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1330
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-3
Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 945A
Glossary: Materials: Polymers: Polyethylene: Ethylene / Vinyl Acetate, Low Density Copolymer
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 15-20% Glass: Flame-Retardant
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2124
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1330
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-3
Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 945A
Glossary: Materials: Polymers: Polyethylene: Ethylene / Vinyl Acetate, Low Density Copolymer
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 15-20% Glass: Flame-Retardant
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2124
Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
Polycarbonate, 40% PAN carbon fiber, EMI shielding (conductive). ComAlloy International Co. 481 Allied Dr. Nashville, TN 37211. Phone: 615-333-3453 ...
eFunda Polymers: Properties of Polyphenylene Sulfide {40% PAN ...
... of Polyphenylene Sulfide {40% PAN carbon fiber, EMI shielding (conductive)} ... Additives: 40% PAN carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced}
eFunda Polymers: Properties of Polyphenylene Sulfide {60 ...
... of Polyphenylene Sulfide {60% stainless steel, EMI shielding (conductive)} ... Additives: 60% stainless steel. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyetherimide {30% carbon fiber ...
... Properties of Polyetherimide {30% carbon fiber, EMI shielding (conductive)} ... Additives: 30% carbon fiber. Application: EMI shielding (conductive) ...
eFunda: Glossary: Units: Linear Mass Density: Denier
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon). Units » Linear Mass Density » Denier · Units » Linear Mass Density » Pound (mass) Per Foot ...
eFunda Polymers: Properties of ABS {20% graphite fiber, EMI ...
... Polymers: Properties of ABS {20% graphite fiber, EMI shielding (conductive)} ... Additives: 20% graphite fiber. Application: EMI shielding (conductive) ...
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... Convert pc. 95 conversions, showing those commonly used | Show all ...
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI ...
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI shielding (conductive)} ... Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of ABS {ABS / PC, injection molding ...
eFunda Polymers: Properties of ABS {ABS / PC, injection molding and extrusion}