Polycarbonate Copolymer High Heat PC is a subcategory of Polycarbonate. The additative is added during the manufacturing process. Its elastic modulus ranges from 320 to 340 MPa. Its flexural modulus ranges from 320 to 340 MPa. Its tensile strength ranges from 8300 to 10000 MPa at break. Its flexural strength ranges from 12000 to 14000 MPa. Its Izod Impact strength ranges from 1.5 to 12 J/cm. Its elongation at break ranges from 70 to 90 %. Its hardness ranges from 75 to 91 Rockwell M. Its specific gravity ranges from 1.14 to 1.18. Its coefficient of thermal expansion ranges from 70 to 76 x 10-6/°C. Its melting temperature ranges from 160 to 205 °C. Its molding pressure ranges from 8 to 20 MPa.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. copolymer It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 501
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): Unfilled Copolyester
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 30% Glass Reinforced V-O
Glossary: Materials: Alloys: Magnesium Alloy: ASTM HZ32A-T5
Glossary: Materials: Alloys: Steel: Stainless Steel: AM-350
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C83300
Glossary: Materials: Polymers: Fluoroplastics: PE-CTFE
Glossary: Materials: Polymers: Polyphthalamide: 45% Glass Reinforced
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): Unfilled Copolyester
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 30% Glass Reinforced V-O
Glossary: Materials: Alloys: Magnesium Alloy: ASTM HZ32A-T5
Glossary: Materials: Alloys: Steel: Stainless Steel: AM-350
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C83300
Glossary: Materials: Polymers: Fluoroplastics: PE-CTFE
Glossary: Materials: Polymers: Polyphthalamide: 45% Glass Reinforced
Related Pages
eFunda: Glossary: Units: Length: Rod (perch, Pole)
Pace (UK), Palm (UK), Parsec (pc), Perch (rod, Pole) (rd), Petameter (Pm), Pica, Picometer (pm), Point (US Printer'S), Pole (rod, Perch) (rd), Quadrant, ...
eFunda Polymers: Properties of Polystyrene and styrene copolymers ...
... and styrene copolymers {copolymer, high heat resistant, injection molding} ... State: copolymer. Application: high heat resistant, injection molding ...
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated}
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated}
Heat Treatments: Hardening: Diffusion Treatments
Low carbon (less than 0.25 %) steel cannot be heat treated by conventional means. ... Pack Carburizing: Parts are packed in a high carbon medium such as ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is susceptible to stress cracking with aromatic solvents, and is difficult to machine. -, Trade Name: Lexan, Makrolon. ...
eFunda Polymers: Properties of Polycarbonate {35% random glass mat}
eFunda Polymers: Properties of Polycarbonate {35% random glass mat}
eFunda Polymers: Properties of Polycarbonate {6% stainless steel ...
eFunda Polymers: Properties of Polycarbonate {6% stainless steel fiber, conductive}
eFunda: Glossary: Units: Linear Mass Density: Denier
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon). Units » Linear Mass Density » Denier · Units » Linear Mass Density » Pound (mass) Per Foot ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber reinforced}
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon)
Polycarbonate, also known as PC, has been mass-produced since 1958. ... Polycarbonate, unfilled, molding and extrusion resins, high viscosity. ...