Glossary » Materials » Polymers » Polyester » Glass Fiber Reinforced, Premix Chopped Glass
Glass Fiber Reinforced, Premix Chopped Glass Polyester is a subcategory of Polyester. The additative is added during the manufacturing process. Its elastic modulus ranges from 1000 to 2500 MPa. Its flexural modulus ranges from 1000 to 2000 MPa. Its tensile strength ranges from 3000 to 10000 MPa at break. Its flexural strength ranges from 7000 to 20000 MPa. Its compressive strength ranges from 20000 to 30000 MPa. Its Izod Impact strength ranges from 1.5 to 16 J/cm. Its elongation at break ranges from 0.5 to 1 %. Its hardness ranges from 50 to 80 . Its specific gravity ranges from 1.65 to 2.3. Its coefficient of thermal expansion ranges from 20 to 33 x 10-6/°C. Its molding pressure ranges from 0.5 to 2 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Rigid Polyester, Flexible Polyester, Glass Fiber Reinforced High Polyester, Glass Fiber Reinforced, Unidirectional Glass Polyester, Glass Fiber Reinforced, Preformed Chopped Roving Polyester, Glass Fiber Reinforced, Woven Cloth Polyester, Glass Fiber Reinforced SMC Polyester, Glass Fiber Reinforced SMC, BMC Low Density Polyester, Glass Fiber Reinforced SMC Low Pressure Polyester, Glass Fiber Reinforced SMC Low Shrink Polyester, Glass Fiber Reinforced BMC, TMC Polyester, EMI Shielding (conductive), SMC & TMC Polyester, EMI Shielding (conductive), BMC Polyester, and 50% Glass Fiber Reinforced High Strength SMC Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Epoxy: Flexibilized
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-28
Glossary: Materials: Polymers: Polyurethane: Thermoset: Casting Resin, Liquid
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C10800
Glossary: Materials: Polymers: Polycarbonate: 20% PAN Carbon Fiber
Glossary: Materials: Polymers: Polystyrene
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Epoxy: Flexibilized
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-28
Glossary: Materials: Polymers: Polyurethane: Thermoset: Casting Resin, Liquid
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C10800
Glossary: Materials: Polymers: Polycarbonate: 20% PAN Carbon Fiber
Glossary: Materials: Polymers: Polystyrene
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel
Related Pages
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda: Polymer (Plastic) Supplier Contact Information
Polyester (thermoset), glass fiber reinforced, premix chopped glass ... Premix, Inc. Rte 20 & Harmon Rd. PO Box 281. North Kingsville, OH 44068 ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(butylene-terephthalate), Unfilled}
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester / alkyd, thermoset, alkyd, mineral filled, molding compounds, ... Polyester / alkyd, thermoset, vinyl ester, glass fiber reinforced, BMC. ...
eFunda: Listing of Common Polymers (Plastics)
eFunda: Listing of Common Polymers (Plastics) ... Cellulosic, Thermoplastic modified natural polymer substance. Epoxy, Thermoset polyadduct. ...
eFunda Polymers: Properties of Epoxy {bisphenol, glass fiber ...
eFunda Polymers: Properties of Epoxy {bisphenol, glass fiber reinforced, ... Additives: glass fiber reinforced. Application: molding compounds ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30 ...
Trade Publications. Reinforced Plastics · Design-2-Part · Chemical Processing ... Additives: 30% glass fiber reinforced. Application: flame-retardant grade ...
eFunda Polymers: Properties of Polyester (thermoset) {glass fiber ...
Additives: glass fiber reinforced, premix chopped glass ... Premix, Inc. North Kingsville, OH. Reichhold, Research Triangle Park, NC, 800-431-1920 ...
eFunda Polymers: Properties of Polyester (thermoset) {EMI ...
eFunda Polymers: Properties of Polyester (thermoset) {EMI shielding (conductive), BMC}
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...