Glossary » Materials » Polymers » Polyester » 50% Glass Fiber Reinforced
50% Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(butylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A662 Grade A
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C18900
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-35
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A515 Grade 55
Glossary: Materials: Polymers: Polyacetal
Glossary: Materials: Alloys: Steel: Tool Steel: AISI A6
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C18900
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-35
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A515 Grade 55
Glossary: Materials: Polymers: Polyacetal
Glossary: Materials: Alloys: Steel: Tool Steel: AISI A6
Glossary: Materials: Alloys: Steel: Alloy Steel
Related Pages
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(butylene-terephthalate), Unfilled}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long ...
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long glass fiber reinforced} ... Additives: 50% long glass fiber reinforced ...
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
... elastomers {silicone / polyester, psuedo-interpenetrating networks} ... State: silicone / polyester. Application: psuedo-interpenetrating networks ...
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, ... Additives: polycarbonate / polyester blends, impact modified ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30% glass ...
State: nylon (PA 6). Additives: 30% glass fiber reinforced, impact modified ... Tensile Strength (MPa), 101, at break, 50% relative humidity, D638 ...