Glossary » Materials » Polymers » Polyester » 50% Long Glass Fiber Reinforced
50% Long Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 10 to 20 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(butylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Polybutylene: Adhesive Resin
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Magnesium Alloy: ASTM M1A-F
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 15% Glass Fiber Reinforced
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PC
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4340H
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4718
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 7178
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1008
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Magnesium Alloy: ASTM M1A-F
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 15% Glass Fiber Reinforced
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PC
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4340H
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4718
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 7178
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1008
Related Pages
eFunda: Determination of Material Constants of a Lamina
Mechanical behaviors of a lamina and the determination of its material property constants.
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30% glass ...
State: nylon (PA 6). Additives: 30% glass fiber reinforced, impact modified ... Tensile Strength (MPa), 101, at break, 50% relative humidity, D638 ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long ...
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long glass fiber reinforced} ... Additives: 50% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyester (thermoset) {glass fiber ...
eFunda Polymers: Properties of Polyester (thermoset) {glass fiber reinforced, BMC, TMC}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Chemicals Compatibile with O-Ring Material Polyurethane, Cast
First, you can select a specific O-ring material to view its compatible chemicals. Or second, you can select a specific chemical to view all its compatible ...
eFunda: Listing of Common Polymers (Plastics)
eFunda: Listing of Common Polymers (Plastics) ... Cellulosic, Thermoplastic modified natural polymer substance. Epoxy, Thermoset polyadduct. ...
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.