Glossary » Materials » Polymers » Polyester » 40% Glass Fiber Reinforced
40% Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(cyclohexylene-methylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4118H
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyamide: Nylon (PA 610): Molding and Extrusion Compound
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B30H
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyester
Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Carbon Fiber
Glossary: Materials: Polymers: Polybutylene: Adhesive Resin
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyamide
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyamide: Nylon (PA 610): Molding and Extrusion Compound
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B30H
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Polymers: Polyester
Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Carbon Fiber
Glossary: Materials: Polymers: Polybutylene: Adhesive Resin
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyamide
Related Pages
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30-40 ...
Reinforced Plastics · appliance DESIGN · Test & Measurement · Business Aviation ... State: nylon (PA 610). Additives: 30-40% long glass fiber reinforced ...
eFunda: Comparisons between Polymers (Plastics) and Metals and ...
CRYSTALLINE POLYMERS: e.g., PPS, PBT (Valox), Polypropylene (PP), have. -, a sharply-defined melting point,. -, high shrinkage after molding, ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(butylene-terephthalate), Unfilled}
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester / alkyd, thermoset, alkyd, mineral filled, molding compounds, ... Polyester / alkyd, thermoset, vinyl ester, glass fiber reinforced, BMC. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 40% long ...
... Polymers: Properties of Polyamide {nylon (PA 66), 40% long glass fiber reinforced} ... State: nylon (PA 66). Additives: 40% long glass fiber reinforced ...
eFunda Polymers: Properties of Ketones {poly(arylether-ketone), 40 ...
... Properties of Ketones {poly(arylether-ketone), 40% glass fiber reinforced} ... State: poly(arylether-ketone). Additives: 40% glass fiber reinforced ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polyester ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polyester copolymer, high heat}
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...