Glossary » Materials » Polymers » Polyester » Poly(ethylene-Terephthalate) » 40% Glass » Flame-Retardant

40% Glass Flame-Retardant Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(ethylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information

Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages

Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1008
Glossary: Materials: Polymers: Thermoplastic Elastomers: Copolyester Ether
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82800
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4320
Glossary: Materials: Alloys: Copper Alloy: Wire
Glossary: Materials: Polymers: Thermoplastic Elastomers: Copolyester Ether
Glossary: Materials: Alloys: Aluminum Alloy: Cast
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82800
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4320
Glossary: Materials: Alloys: Copper Alloy: Wire
Related Pages

eFunda Polymers: Properties of ABS {flame-retardant grades ...
eFunda Polymers: Properties of ABS {flame-retardant grades, molding and extrusion}
eFunda Polymers: Properties of Acetal {40% long glass fiber ...
eFunda Polymers: Properties of Acetal {40% long glass fiber reinforced}
eFunda Polymers: Properties of Polystyrene and styrene copolymers ...
... of Polystyrene and styrene copolymers {rubber-modified, flame-retardant, UL-V0} ... Additives: rubber-modified. Application: flame-retardant, UL-V0 ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
... low resistance to strong acids and bases, is notch sensitive, and is not recommended for outdoor use or in hot water. -, Trade Name: Valox, Celanex. ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
... Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-retardant grade} ... Additives: unreinforced. Application: flame-retardant grade ...
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled ...
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled, medium melting point}
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester / alkyd, thermoset, alkyd, mineral filled, molding compounds, ... Polyester / alkyd, thermoset, vinyl ester, glass fiber reinforced, BMC. ...
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
... elastomers {silicone / polyester, psuedo-interpenetrating networks} ... State: silicone / polyester. Application: psuedo-interpenetrating networks ...