Glossary » Materials » Polymers » Polyester » 50% Long Glass Fiber Reinforced
50% Long Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 10 to 20 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(ethylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): Super-Tough
Glossary: Materials: Alloys: Steel: Tool Steel: AISI M43
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1350
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720
Glossary: Materials: Polymers: Polycarbonate: Unfilled
Glossary: Materials: Polymers: Polypropylene: Homopolymer: 10 - 40% Calcium Carbonate Filled
Glossary: Materials: Polymers: Polyester: Glass Fiber Reinforced: SMC Low Pressure
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C62400
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A619
Glossary: Materials: Alloys: Steel: Tool Steel: AISI M43
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1350
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720
Glossary: Materials: Polymers: Polycarbonate: Unfilled
Glossary: Materials: Polymers: Polypropylene: Homopolymer: 10 - 40% Calcium Carbonate Filled
Glossary: Materials: Polymers: Polyester: Glass Fiber Reinforced: SMC Low Pressure
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C62400
Glossary: Materials: Alloys: Steel: Tool Steel
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A619
Related Pages
eFunda Polymers: Properties of Polyamide {partially aromatic, 50 ...
State: partially aromatic. Additives: 50% glass fiber reinforced ... Units » Force » Ton Force (long) · Materials » Alloys » Steel » Stainless Steel » 17- ...
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda: Listing of Common Polymers (Plastics)
eFunda: Listing of Common Polymers (Plastics) ... Cellulosic, Thermoplastic modified natural polymer substance. Epoxy, Thermoset polyadduct. ...
eFunda Polymers: Properties of Polyester (thermoset) {50% glass ...
Additives: 50% glass fiber reinforced. Application: high strength SMC ... Hardness, 50 - 60, Barcol, D638. Izod Impact (J/cm of notch) ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd, mineral filled, molding compounds, granular and putty}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30% glass ...
State: nylon (PA 6). Additives: 30% glass fiber reinforced, impact modified ... Tensile Strength (MPa), 101, at break, 50% relative humidity, D638 ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled ...
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled, medium melting point}
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long ...
eFunda Polymers: Properties of Polyphenylene Sulfide {50% long glass fiber reinforced} ... Additives: 50% long glass fiber reinforced ...