Glossary » Materials » Polymers » Polymethylpentene » Filled
Filled PMP is a subcategory of Polymethylpentene. The additative is added during the manufacturing process. Its molding pressure ranges from 1 to 10 MPa.
Polymethylpentene, also known as PMP, is a thermoplastic polymer. It has a very low density and is transparent. It has excellent chemical resistance, low moisture absorption, and exceptional acoustical and electrical properties. PMP can be found in sonar covers, speaker cones, ultrasonic transducer heads, and lightweight structural parts. It is also FDA compliant for use in food processing machinery. Polymethylpentene is often used in films and coatings for gas permeable packaging.
Additional Information
Other common Polymethylpentene (PMP) include Unfilled PMP.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyaryletherketone
Glossary: Materials: Alloys: Steel: Tool Steel: AISI P20
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 30% Glass: Flame-Retardant
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C94000
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Polymers: Polyaryletherketone
Glossary: Materials: Alloys: Steel: Tool Steel: AISI P20
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 30% Glass: Flame-Retardant
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C94000
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Alloys: Steel: Carbon Steel
Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polymethylpentene, filled. Mitsui Petrochemical Industries, Ltd. 3-2-5 Kasumigaseki. Chiyoda-ku, Tokyo, Japan 100,. Phone: 03-3593-1630. FAX: 03-3593-0979 ...
eFunda Polymers: Properties of Polymethylpentene {unfilled}
eFunda Polymers: Properties of Polymethylpentene {unfilled}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 25-30 ...
... Properties of Polyamide {nylon (PA 66), 25-30% mineral filled, modified high-impact} ... Additives: 25-30% mineral filled, modified high-impact ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111. FAX: 718-972-3256. E-Mail: mail@ashleypoly.com. Web: www.ashleypoly.com ...
eFunda Polymers: Properties of Epoxy {bisphenol, low density ...
... Properties of Epoxy {bisphenol, low density, glass sphere filled, molding compounds} ... Additives: glass sphere filled. Application: molding compounds ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
eFunda: Listing of Common Polymers (Plastics) in Chronological Order. ... The first volume-produced synthesized polymer resin, PF was used in early consumer ...
In The News
Apple's Biggest PMP Competitor: "You Can't Out-iPod the iPod" · Gizmodo Jun 4 2009 2:48PM. HP shows off colour display 'skin' for gadgets ...