Glossary » Materials » Polymers » Polyphenylene Oxide » Alloy With Polystyrene
Alloy With Polystyrene PPO is a subcategory of Polyphenylene Oxide. The additative is added during the manufacturing process. Its elastic modulus ranges from 310 to 380 MPa. Its flexural modulus ranges from 325 to 400 MPa. Its tensile strength ranges from 6800 to 7800 MPa at break. Its flexural strength ranges from 800 to 12800 MPa. Its compressive strength ranges from 1200 to 16400 MPa. Its Izod Impact strength ranges from 3 to 6 J/cm. Its elongation at break ranges from 48 to 50 %. Its hardness ranges from 115 to 116 Rockwell R. Its specific gravity ranges from 1.04 to 1.1. Its coefficient of thermal expansion ranges from 38 to 70 x 10-6/°C. Its melting temperature ranges from 100 to 112 °C. Its molding pressure ranges from 12 to 20 MPa.
Polyphenylene Oxide, also known as PPO, is a thermoplastic polycondensate. The most common trade name is Ashley. low glass transition temp Although it resists many chemicals, it is easily attacked by some hydrocarbons. It has excellent dimensional stability, low moisture absorption, and high mechanical and dielectric strength. PPO is processable by conventional extrusion and injection molding equipment.
Additional Information
Other common Polyphenylene Oxide (PPO) include Alloy With Polystyrene PPO, Alloy With Polystyrene, Impact Modified PPO, Alloy With Polystyrene, 15% Glass Fiber Reinforced PPO, Alloy With Polystyrene, 20% Glass Fiber Reinforced PPO, Alloy With Polystyrene, 30% Glass Fiber Reinforced PPO, Alloy With Polystyrene, Mineral Filled PPO, Alloy With Polystyrene, 30% Graphite Fiber EMI Shielding (conductive) PPO, Alloy With Polystyrene, 40% Aluminium Flake EMI Shielding (conductive) PPO, and Alloy With Nylon, Unreinforced PPO.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wire
Glossary: Materials: Polymers: Polyamide-Imide: Unfilled: Compression and Injection Molding Compound
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-6Al-2Sn-2Zr-2Mo-2Cr-0.25Si
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 20% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 15-20% Glass: Flame-Retardant
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Mineral Filled: Casting Resins
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82100
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C43000
Glossary: Materials: Polymers: Polyamide-Imide: Unfilled: Compression and Injection Molding Compound
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-6Al-2Sn-2Zr-2Mo-2Cr-0.25Si
Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 20% Glass Fiber Reinforced
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 15-20% Glass: Flame-Retardant
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Mineral Filled: Casting Resins
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82100
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C43000
Related Pages
eFunda Polymers: Properties of ABS {injection molding grade, platable}
A. Schulman, Akron, OH, 800-662-7203. American Polymers, Inc. Worcester, MA. Ashley Polymers, Brooklyn, NY. Bamberger Polymers, Inc. Jericho, NY ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111. FAX: 718-972-3256. E-Mail: mail@ashleypoly.com. Web: www.ashleypoly.com ...
eFunda: Piezo Material Data
Select specific piezoelectric material to view constitutive properties.
In The News
Alan Shearer frozen out of Newcastle managers job by Mike Ashley · Football.co.uk Jun 7 2009 10:29PM. Exhibition Sales Executive - Fashion Show ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Chemicals Compatibile with O-Ring Material Polyurethane, Cast
First, you can select a specific O-ring material to view its compatible chemicals. Or second, you can select a specific chemical to view all its compatible ...
eFunda: Properties of Piezo Material Quartz
eFunda: Properties of Piezo Material Quartz. ... Piezo Data: Quartz Home | Directory | Career | News | InfoStore | Industrial · Materials Home. Piezo Basics ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Polyphenylene Oxide (modified ...
eFunda Polymers: Properties of Polyphenylene Oxide (modified) {alloy with polystyrene, 30% graphite fiber, EMI shielding (conductive)}
eFunda: Determination of Material Constants of a Lamina
Mechanical behaviors of a lamina and the determination of its material property constants.