Glossary » Materials » Polymers » Polyphenylene Sulfide » 50% Long Glass Fiber Reinforced
50% Long Glass Fiber Reinforced PPS is a subcategory of Polyphenylene Sulfide. The additative is added by weight during the manufacturing process. Its flexural strength ranges from 37300 to 38000 MPa. Its compressive strength ranges from 34200 to 35000 MPa. Its Izod Impact strength ranges from 5 to 5.5 J/cm. Its molding pressure ranges from 8 to 10 MPa.
Polyphenylene Sulfide, also known as PPS, is a thermoplastic polycondensate. The most common trade name is Ryton. It has high temperature resistance (230 ºC continuous), low temperature endurance, good chemical resistance, and flame retardance. PPS can be used to make high performance electrical connectors and other high stress parts.
Additional Information
Other common Polyphenylene Sulfide (PPS) include Unfilled PPS, 10-20% Glass Fiber Reinforced PPS, 30% Glass Fiber Reinforced PPS, 40% Glass Fiber Reinforced PPS, 53% Glass / Mineral Reinforced High Elongation and Impact PPS, 30% Glass Fiber, 15% PTFE PPS, 30% Long Glass Fiber Reinforced PPS, 40% Long Glass Fiber Reinforced PPS, 60% Long Glass Fiber Reinforced PPS, 65% Mineral and Glass Filled PPS, 50% Glass and Mineral Reinforced PPS, 55% Glass and Mineral Reinforced PPS, 60% Glass and Mineral Reinforced PPS, Encapsulation Grades PPS, 60% Stainless Steel EMI Shielding (conductive) PPS, 30% Carbon Fiber EMI Shielding (conductive) PPS, 40% PAN Carbon Fiber EMI Shielding (conductive) PPS, and 30% PAN Carbon Fiber, 15% PTFE EMI Shielding (conductive) PPS.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4817
Glossary: Materials: Alloys: Steel: Stainless Steel: 18-18-2
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99300
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 310S
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11500
Glossary: Materials: Polymers: Polyacrylates: Multipolymer: Molding and Extrusion Compounds
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4817
Glossary: Materials: Alloys: Steel: Stainless Steel: 18-18-2
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99300
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 310S
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11500
Glossary: Materials: Polymers: Polyacrylates: Multipolymer: Molding and Extrusion Compounds
Glossary: Materials: Alloys: Copper Alloy: Wrought
Related Pages
eFunda: Introduction to Compression Molding
Polyester · Polyimide (PI); Polyamide-imide (PAI); Polyphenylene Sulfide (PPS); Polyetheretherketone (PEEK); Fiber reinforced plastics ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
... Properties of Polyester (thermoplastic) {poly(ethylene-terephthalate), 50% long glass fiber reinforced} ... Additives: 50% long glass fiber reinforced ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Comparisons between Polymers (Plastics) and Metals and ...
CRYSTALLINE POLYMERS: e.g., PPS, PBT (Valox), Polypropylene (PP), have. -, a sharply-defined melting point,. -, high shrinkage after molding, ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Polypropylene (PP); 1950's . -, Thermoplastic, (crystalline), polymer. ... Polyphenylene Sulfide (PPS); 1973. -, Thermoplastic polycondensate. ...
eFunda Polymers: Properties of Polyphenylene Sulfide {30% glass ...
eFunda Polymers: Properties of Polyphenylene Sulfide {30% glass fiber reinforced}
eFunda: Overview of Polymers (Plastics)
Examples of crystalline plastics include acetal, polyamide (PA; nylon), polyethylene (PE), polypropylene (PP), polyester (PET, PBT), and polyphenylene ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.