Glossary » Materials » Polymers » Polyphenylene Sulfide » 60% Long Glass Fiber Reinforced
60% Long Glass Fiber Reinforced PPS is a subcategory of Polyphenylene Sulfide. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 8 to 10 MPa.
Polyphenylene Sulfide, also known as PPS, is a thermoplastic polycondensate. The most common trade name is Ryton. It has high temperature resistance (230 ºC continuous), low temperature endurance, good chemical resistance, and flame retardance. PPS can be used to make high performance electrical connectors and other high stress parts.
Additional Information
Other common Polyphenylene Sulfide (PPS) include Unfilled PPS, 10-20% Glass Fiber Reinforced PPS, 30% Glass Fiber Reinforced PPS, 40% Glass Fiber Reinforced PPS, 53% Glass / Mineral Reinforced High Elongation and Impact PPS, 30% Glass Fiber, 15% PTFE PPS, 30% Long Glass Fiber Reinforced PPS, 40% Long Glass Fiber Reinforced PPS, 50% Long Glass Fiber Reinforced PPS, 65% Mineral and Glass Filled PPS, 50% Glass and Mineral Reinforced PPS, 55% Glass and Mineral Reinforced PPS, 60% Glass and Mineral Reinforced PPS, Encapsulation Grades PPS, 60% Stainless Steel EMI Shielding (conductive) PPS, 30% Carbon Fiber EMI Shielding (conductive) PPS, 40% PAN Carbon Fiber EMI Shielding (conductive) PPS, and 30% PAN Carbon Fiber, 15% PTFE EMI Shielding (conductive) PPS.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyvinylchloride: Poly(vinyl-Butyral): Molding and Extrusion Compounds, Flexible
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5050
Glossary: Materials: Polymers: Polyvinylidene Chloride: Copolymer: Unplasticized: Barrier Film Resins
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ61A-F
Glossary: Materials: Polymers: Fluoroplastics: Poly(vinyl Fluoride): Unfilled: Film
Glossary: Materials: Polymers: Polyethylene: High Density Homopolymer
Glossary: Materials: Polymers: Polyphenylene Sulfide: 10-20% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720H
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type F
Glossary: Materials: Polymers: Polyvinylchloride: Poly(vinyl-Butyral): Molding and Extrusion Compounds, Flexible
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5050
Glossary: Materials: Polymers: Polyvinylidene Chloride: Copolymer: Unplasticized: Barrier Film Resins
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ61A-F
Glossary: Materials: Polymers: Fluoroplastics: Poly(vinyl Fluoride): Unfilled: Film
Glossary: Materials: Polymers: Polyethylene: High Density Homopolymer
Glossary: Materials: Polymers: Polyphenylene Sulfide: 10-20% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720H
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type F
Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% long ...
State: nylon (PA 66). Additives: 30% long glass fiber reinforced ... Hardness, 60, Rockwell E, dry (0.2% water content), D638. Izod Impact (J/cm of notch) ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 60 ...
State: partially aromatic. Additives: 60% glass fiber reinforced ... Units » Mass » Quarter (US, Long) · Materials » Alloys » Aluminum Alloy » Cast » 201.0 ...
eFunda Polymers: Properties of Polyphenylene Sulfide {65% mineral ...
eFunda Polymers: Properties of Polyphenylene Sulfide {65% mineral and glass filled}
eFunda: Properties of Piezo Material Quartz
eFunda: Properties of Piezo Material Quartz. ... Piezo Data: Quartz Home | Directory | Career | News | InfoStore | Industrial · Materials Home. Piezo Basics ...
eFunda: Polymers (Plastics) Sorted by Resin Family
Polyethersulfone, (PES). •, Polyimide, (PI). •, Polyphenylene Oxide, (PPO). •, Polyphenylene Sulfide, (PPS). •, Polyphthalamide, (PTA). ...
eFunda Polymers: Properties of Polyphenylene Sulfide {30% carbon ...
eFunda Polymers: Properties of Polyphenylene Sulfide {30% carbon fiber, EMI shielding (conductive)}
eFunda: Listing of Common Polymers (Plastics)
Polyphenylene Sulfide, (PPS), Thermoplastic polycondensate. ... Polypropylene, (PP), Thermoplastic, (crystalline), polymer. ...
eFunda Polymers: Properties of Polyphenylene Sulfide {53% glass ...
eFunda Polymers: Properties of Polyphenylene Sulfide {53% glass / mineral reinforced, high elongation and impact}
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Polypropylene (PP); 1950's . -, Thermoplastic, (crystalline), polymer. ... Polyphenylene Sulfide (PPS); 1973. -, Thermoplastic polycondensate. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30-40 ...
... Properties of Polyamide {nylon (PA 610), 30-40% long glass fiber reinforced} ... State: nylon (PA 610). Additives: 30-40% long glass fiber reinforced ...