Glossary » Materials » Polymers » Polyphthalamide » 33% Glass Reinforced, V-0
33% Glass Reinforced, V-0 PTA is a subcategory of Polyphthalamide. The additative is added by weight during the manufacturing process. Its flexural modulus ranges from 1900 to 1930 MPa. Its tensile strength ranges from 26000 to 27000 MPa at break. Its flexural strength ranges from 35900 to 37300 MPa. Its Izod Impact strength ranges from 1.1 to 1.5 J/cm. Its molding pressure ranges from 5 to 15 MPa.
Polyphthalamide, also known as PTA, is a thermoplastic polycondensate.
Additional Information
Other common Polyphthalamide (PTA) include Extra Tough PTA, 45% Glass Reinforced PTA, 40% Mineral Reinforced PTA, 40% Glass / Mineral Reinforced, Heat Stablized PTA, 50% Glass / Mineral Reinforced, V-0 PTA, 51% Glass / Mineral Reinforced PTA, 15% Glass Reinforced PTA, 15% Glass Reinforced, V-0 PTA, 45% Glass Reinforced, V-0 PTA, 40% Glass / Mineral Reinforced PTA, and 40% Mineral Reinforced, Heat Stablized PTA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: 18-2FM
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C92800
Glossary: Materials: Polymers: Polyester
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ80A-T5
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ63A-T6
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 202
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1029
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C92800
Glossary: Materials: Polymers: Polyester
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ80A-T5
Glossary: Materials: Alloys: Steel: Carbon Steel
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ63A-T6
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 202
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1029
Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111. FAX: 718-972-3256. E-Mail: mail@ashleypoly.com. Web: www.ashleypoly.com ...
eFunda: Listing of Common Polymers (Plastics)
Polyphthalamide, (PTA), Thermoplastic polycondensate. Polypropylene, (PP), Thermoplastic, (crystalline), polymer. Polystyrene, (PS), Thermoplastic polymer. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced} ... State: nylon (PA 66). Additives: 30-33% glass fiber reinforced ...
efunda: Fundamental Constants
e0, 1/(m0·c2) = 8.85418781...x10-12 F/m ... m0, 4p x10-7 = 1.2566370614...x10-6 H/m. ·, natural log base. e, 2.718281828459045. ... V0, 2.24136x10-2 m3/mol ...
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester / alkyd, thermoset, vinyl ester, glass fiber reinforced, BMC. ... poly(cyclohexylene-methylene-terephthalate), 30% glass fiber reinforced. 33. ...
eFunda Polymers: Properties of Polyphthalamide {extra tough}
eFunda Polymers: Properties of Polyphthalamide {extra tough}
eFunda Polymers: Properties of Polyphthalamide {15% glass ...
eFunda Polymers: Properties of Polyphthalamide {15% glass reinforced, V-0}
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda Polymers: Properties of Polyphthalamide {15% glass reinforced}
eFunda Polymers: Properties of Polyphthalamide {15% glass reinforced}
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...