Glossary » Materials » Polymers » Polyphthalamide » 51% Glass / Mineral Reinforced
51% Glass / Mineral Reinforced PTA is a subcategory of Polyphthalamide. The additative is added by weight during the manufacturing process. Its flexural strength ranges from 24000 to 28400 MPa. Its elongation at break ranges from 1.9 to 2 %. Its specific gravity ranges from 1.66 to 1.68.
Polyphthalamide, also known as PTA, is a thermoplastic polycondensate.
Additional Information
Other common Polyphthalamide (PTA) include Extra Tough PTA, 45% Glass Reinforced PTA, 33% Glass Reinforced, V-0 PTA, 40% Mineral Reinforced PTA, 40% Glass / Mineral Reinforced, Heat Stablized PTA, 50% Glass / Mineral Reinforced, V-0 PTA, 15% Glass Reinforced PTA, 15% Glass Reinforced, V-0 PTA, 45% Glass Reinforced, V-0 PTA, 40% Glass / Mineral Reinforced PTA, and 40% Mineral Reinforced, Heat Stablized PTA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A570 Grade 33
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6010
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Ionomer: Molding and Extrusion
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C96700
Glossary: Materials: Alloys: Aluminum Alloy: Cast: 296.0
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 312
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5145
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6010
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Ionomer: Molding and Extrusion
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C96700
Glossary: Materials: Alloys: Aluminum Alloy: Cast: 296.0
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 312
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5145
Glossary: Materials: Polymers: Polyethersulfone: 10% Glass Fiber Reinforced
Related Pages
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, nylon (PA 66), 40% glass and mineral reinforced. ... 51. Polyamide, nylon (PA 66), 40% nickel coated carbon fiber, EMI shielding (conductive). ...
eFunda Polymers: Properties of Polyphthalamide {15% glass ...
eFunda Polymers: Properties of Polyphthalamide {15% glass reinforced, V-0}
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda Polymers: Properties of Polyphthalamide {40% glass ...
eFunda Polymers: Properties of Polyphthalamide {40% glass / mineral reinforced}
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111. FAX: 718-972-3256. E-Mail: mail@ashleypoly.com. Web: www.ashleypoly.com ...
eFunda Polymers: Properties of Polyphthalamide {45% glass ...
eFunda Polymers: Properties of Polyphthalamide {45% glass reinforced, V-0}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...