Glossary » Materials » Polymers » Polysulfone » 20% Glass Fiber Reinforced
20% Glass Fiber Reinforced PSU is a subcategory of Polysulfone. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 825 to 1130 MPa. Its flexural modulus ranges from 750 to 980 MPa. Its tensile strength ranges from 15200 to 20000 MPa at break. Its flexural strength ranges from 23500 to 27600 MPa. Its compressive strength ranges from 19500 to 24000 MPa. Its Izod Impact strength ranges from 1.1 to 1.7 J/cm. Its elongation at break ranges from 2 to 3.5 %. Its hardness ranges from 96 to 99 Rockwell M. Its specific gravity ranges from 1.51 to 1.53. Its coefficient of thermal expansion ranges from 23 to 32 x 10-6/°C. Its melting temperature ranges from 220 to 225 °C. Its molding pressure ranges from 6 to 100 MPa.
Polysulfone, also known as PSU, is a thermoplastic polycondensate. The most common trade name is Ultrason. poly(ethersulfone) It is an expensive material. It is electroplatable and has high strength, good toughness, good dielectric strength, and dimensional stability. It is commonly used in electric connectors.
Additional Information
Other common Polysulfone (PSU) include Injection Molding, Flame-Retardant, Extrusion PSU, Mineral Filled PSU, Extrusion / Injection Molding Grade PSU, 20% Glass Fiber Reinforced PSU, 30% Carbon Fiber EMI Shielding (conductive) PSU, Injection Molding, Platable Grade PSU, PSU, Unfilled PSU, 10% Glass Fiber Reinforced PSU, 30% Carbon Fiber EMI Shielding (conductive) PSU, PSU, Unreinforced PSU, and Mineral Filled PSU.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polystyrene: Styrene / Maleic Anhydride (SMA) Copolymer: Molding and Extrusion
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type N
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): Unfilled: Medium Melting Point
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Heat Resistant
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Unfilled: Casting Resins
Glossary: Materials: Alloys: Steel: Stainless Steel
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Polymers: Polystyrene: Styrene / Maleic Anhydride (SMA) Copolymer: Molding and Extrusion
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type N
Glossary: Materials: Alloys: Steel: Alloy Steel
Glossary: Materials: Alloys: Copper Alloy: Cast
Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): Unfilled: Medium Melting Point
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Heat Resistant
Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Unfilled: Casting Resins
Related Pages
eFunda Polymers: Properties of ABS {20% long glass fiber ...
eFunda Polymers: Properties of ABS {20% long glass fiber reinforced, injection molding grade} ... Additives: 20% long glass fiber reinforced ...
eFunda: Piezo Material Data
Select specific piezoelectric material to view constitutive properties.
eFunda: Polymer (Plastic) Supplier Contact Information
Sulfone polymers, polysulfone, injection molding, platable grade. Solvay Advanced Polymers, L.L.C.. 4500 McGinnis Ferry Road. Alpharetta, GA 30005 ...
eFunda Polymers: Properties of Polystyrene and styrene copolymers ...
eFunda Polymers: Properties of Polystyrene and styrene copolymers {copolymer, 20% glass fiber reinforced, high heat resistant}
eFunda: Properties of Piezo Material Quartz
eFunda: Properties of Piezo Material Quartz. ... Piezo Data: Quartz Home | Directory | Career | News | InfoStore | Industrial · Materials Home. Piezo Basics ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone ...
... Properties of Sulfone polymers {poly(ethersulfone), 20% glass fiber reinforced} ... State: poly(ethersulfone). Additives: 20% glass fiber reinforced ...
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda Polymers: Properties of Sulfone polymers {modified ...
eFunda Polymers: Properties of Sulfone polymers {modified polysulfone, mineral filled} ... State: modified polysulfone. Additives: mineral filled ...